Shiryaev A.A., Krokhinа V.A., Putyrskiy S.V., Anisimova A.Yu. The influence of heat treatment parameters on mechanical properties and structure of semi-finished products made of high-strength titanium alloy VT23M // Proceedings of VIAM. 2025. No. 8 (150). Ст. 06. URL: https://www.viam-works.ru. DOI: 10.18577/2307-6046-2025-0-8-67-75.
The influence of heat treatment parameters on mechanical properties and structure of semi-finished products made of high-strength titanium alloy VT23M
Abstract
The article presents the results of the structure study, as well as physical and mechanical properties of forgings made of titanium (α + β) alloy VT23M after heat treatment. The choice of the heat treatment type (double annealing) is has been reasoned. The influence of process parameters on the microstructure features and the level of strength and ductile characteristics, impact toughness, are studied. Based on the analysis, the temperatures of the first and the second stages of double annealing of forgings made of VT23M alloy are selected, providing the balanced set of mechanical properties and the favorable microstructure.
Keywords
titanium alloys, alloy VT23M, forgings, heat treatment, microstructure, mechanical properties
Reference list
- Kablov E.N., Antipov V.V. The Role of New Generation Materials in Ensuring the Technological Sovereignty of the Russian Federation. Vestnik Rossiyskoy akademii nauk, 2023, vol. 10, no. 93, pp. 907–916.
- Kablov E.N., Belov E.V., Trapeznikov A.V., Leonov A.A., Zaitsev D.V. Strengthening features and aging kinetics of high-strength cast aluminum alloy AL4MS based on Al–Si–Cu–Mg system. Aviation materials and technologies, 2021, no. 2 (63), paper no. 03. Available at: http://www.journal.viam.ru (accessed: June 04, 2025). DOI: 10.18577/2713-0193-2021-0-2-24-34.
- Krokhina V.A., Arislanov А.A., Putyrskiy S.V., Anisimova A.Yu. Investigation of the regularities of the formation of the structure of rods made of titanium alloy VT6 depending on various technological schemes of manufacture. Aviation materials and technologies, 2023, no. 4 (73), paper no. 04. Available at: http://www.journal.viam.ru (accessed: June 09, 2025). DOI: 10.18577/2713-0193-2023-0-4-36-44.
- Kapustin V.I., Zakharchenko K.V., Cherepanova V.K., Shayapov V.R. Investigation of dissipative processes of VT6 alloy under fatigue. Aviation materials and technologies, 2022, no. 4 (69), paper no. 09. Available at: http://www.journal.viam.ru (accessed: June 09, 2025). DOI: 10.18577/2713-0193-2022-0-4-96-111.
- Duyunova V.A., Pavlova T.V., Kashapov O.S., Chuchman O.V. Fatigue strength of forgings from VT6 alloy for parts of gas turbine engines and aircrafts. Aviation materials and technologies, 2023, no. 2 (71), paper no. 02. Available at: http://www.journal.viam.ru (accessed: June 09, 2025). DOI: 10.18577/2713-0193-2023-0-2-23-35.
- Titanium and titanium alloys. Fundamentals and applications. Eds. C. Leyens, M. Peters. Wiley–VCH, 2003, 513 p.
- Putyrsky S.V., Arislanov A.A., Yakovlev A.L., Nochovna N.A. Studing of mechanical properties of deformed semi-finished products of VT23M and VT43 alloys, assessment of their climatic stability in the Arctic climate. Trudy VIAM, 2018, no. 4 (64), paper no. 12. Available at: http://www.viam-works.ru (accessed: May 26, 2025). DOI: 10.18577/2307-6046-2018-0-4-101-110.
- Lyasotskaya V.S. Heat treatment of welded joints of titanium alloys. Moscow: Ekomet, 2003, 352 p.
- Glazunov S.G., Moiseev V.N. Titanium alloys. Structural titanium alloys. Moscow: Metallurgiya, 1974, 368 p.
- Ilyin A.A., Kolachev B.A., Polkin I.S. Titanium alloys. Composition, structure, properties. Moscow: VILS-MATI, 2009, 520 p.
- Shvetsov O.V., Kondratiev S.Yu. Effect of hardening and aging modes on the operational properties of VT23 alloy. Nauchno-tekhnicheskiye vedomosti SPbPU. Yestestvennyye i inzhenernye nauki, 2018, vol. 24, no. 2, pp. 119–133. DOI: 10.18721/JEST.240210.
- Gladkovsky S.V., Veselova V.E., Dubinsky S.V. et al. Effect of heat treatment modes on crack resistance characteristics and fracture mechanisms of metastable titanium alloy VT23. Vestnik PNIPU. Mashinostroyenie. Materialovedenie, 2023, vol. 25, no. 1, pp. 16–26. DOI: 10.15593/2224-9877/2023.1.02.
- Dzunovich D.A., Panin P.V., Lukina E.A., Shiryaev A.A. Heat treatment effect on structure and properties of welded large-dimensioned semi-finished products from VT23 titanium alloy. Trudy VIAM, 2018, no. 1 (61), paper no. 07. Available at: http://www.viam-works.ru (accessed: May 29, 2025). DOI: 10.18577/2307-6046-2018-0-1-7-7.
- Gunawarman G., Niinomi M., Eylon D. et al. Effect of β Phase Stability at Room Temperature on Mechanical Properties in β-Rich α+β Type Ti–4,5Al–3V–2Mo–2Fe Alloy. ISIJ International, 2002, vol. 42, no. 2, pp. 191–199.
- Gunawarman G., Niinomi M., Fukunaga K. et al. Effect of Cooling Rate on Microstructure and Fracture Characteristics of β-Rich α+β Type Ti–4,5Al–3V–2Mo–2Fe Alloy. Materials Transactions, 2001, vol. 42, no. 7, pp. 1339–1348.
- Kablov E.N., Kirillov V.N., Zhirnov A.D., Startsev O.V., Vapirov Yu.M. Centers for climatic testing of aviation PCM. Aviatsionnaya promyshlennost, 2009, no. 4, pp. 36–46.
- Veselova V.E., Gladkovsky S.V., Kovalev N.I. Influence of heat treatment modes on the structure and mechanical properties of metastable titanium alloy VT23. Vestnik Permskogo natsional'nogo issledovatelskogo politekhnicheskogo universiteta. Ser.: Mashinostroyeniye, materialovedeniye, 2021, vol. 23, no. 4, pp. 31–39. DOI: 10.15593/2224-9877/2021.4.04.
- Ilyin A.A., Skvortsova S.V., Popova Yu.A., Kudelina I.M. Influence of heat treatment on the formation of the structure and properties of large-sized semi-finished products made of VT23 alloy. Titan, 2010, no. 4, pp. 48–53.
- Fukai H., Minakawa K.-N., Ouchi C. Strength–Ductility Relationship in Solution Treated and Aged α+β Type Ti–4.5%Al–3%V–2%Fe–2%Mo Titanium Alloy. ISIJ International, 2004, vol. 44, no. 11, pp. 1911–1917.
- Xu J., Zeng W., Zhao Y. et al. Effect of globularization behavior of the lamellar alpha on tensile properties of Ti-17 alloy. Journal of Alloys and Compounds, 2016, vol. 673, pp. 86–92.