Kablov E.N., Nerush S.V., Chubov D.G., Sukhov D.I., Filonova E.V., Pahomkin S.I. Structural instability of heat-resistant nickel-based superalloys with high content of the gamma prime phase obtained by selective laser melting method // Proceedings of VIAM. 2025. No. 8 (150). Ст. 01. URL: https://www.viam-works.ru. DOI: 10.18577/2307-6046-2025-0-8-3-13.

Structural instability of heat-resistant nickel-based superalloys with high content of the gamma prime phase obtained by selective laser melting method

Kablov E.N., Nerush S.V., Chubov D.G., Sukhov D.I., Filonova E.V., Pahomkin S.I.
Abstract

The study is devoted to the analysis of structural instability of heat-resistant nickel-based superalloys with a high content of γ′-phase (about 50 % and higher) obtained by selective laser melting (SLM). Two new alloy compositions differing only in Re and C content were used for the experiments. The results show that both alloys are crack-free after SLM, while exhibiting a pronounced cellular microstructure. In alloy 1, columnar grains with uniform distribution of  γ′-particles (150–250 nm) prevail, which provides structural stability, the proportion of γ′-phase in it is 48±2 %. Alloy 2, despite maintaining a high proportion of γ′-phase (55±3 %) after heat treatment, is prone to the formation of topologically closed packed phases due to segregation of Re and residual stresses. The different amount of γ′-phase in the alloys is explained by the difference in their chemical composition. Calculations of the lattice parameters revealed the dependence of the misfit of γ/γ′-phases on the composition: in sample 2 with lower misfit (0,29 %) the particles have morphology close to cubic, while in sample 1 (misfit 0,37 %) the particles are close to spherical. The morphology and misfit are related to the influence of Re. The anisotropy of the γ′-particle shape in the longitudinal section of sample 2 is related to the directional heat flux during SLM.

Keywords
nickel-based superalloys, additive manufacturing, selective laser melting, built directional
Reference list
  1. Reed R.C. The Superalloys: Fundamentals and Applications. Cambridge: Cambridge University Press, 2006, 372 p. DOI: 10.1017/CBO9780511541285.
  2. Pollock T.M., Tin S. Nickel-Based Superalloys for Advanced Turbine Engines: Chemistry, Microstructure and Properties. Journal of Propulsion and Power, 2006, vol. 22 (2), pp. 361–374. DOI: 10.2514/1.18239.
  3. Logunov A.V. Heat-resistant nickel alloys for blades and disks of gas turbines. Moscow: Moskovskie uchebniki, 2018, 592 p.
  4. Kablov E.N., Evgenov A.G., Petrushin N.V., Bazyleva O.A., Mazalov I.S., Dynin N.V. New generation materials and digital additive technologies for the production of resource parts of FSUE VIAM. Part 3. Adaptation and creation of materials. Elektrometallurgiya, 2022, no. 4, pp. 15–25.
  5. Evgenov A.G., Shurtakov S.V., Prager S.M., Malinin R.Yu. On the development of a universal calculation method for assessing the degradation of recycled metal powder materials, depending on the cyclicity of use in the selective laser melting process. Aviacionnye materialy i tehnologii, 2020, no. 4 (61), pp. 3–11. DOI: 10.18557/2071-9140-2020-0-4-3-11.
  6. Ospennikova O.G., Naprienko S.A., Medvedev P.N., Zaitsev D.V., Rogalev A.M. Features of the formation of the structural-phase state of the EP648 alloy during selective lase manufacture. Trudy VIAM, 2021, no. 8 (102), paper no. 01. Available at: http://www.viam-works.ru (accessed: December 13, 2024). DOI: 10.18557/2307-6046-2021-0-8-3-11.
  7. Sukhov D.I., Nerush S.V., Efimochkin I.Yu., Karachevchev F.N., Bogachev I.A. Production of MMC based on VZh159 alloy by selective laser melting. Aviation materials and technologies, 2021, no. 2 (63), paper no. 07. Available at: http://www.journal.viam.ru (accessed: December 13, 2024). DOI: 10.18577/2713-0193-2021-0-2-62-72.
  8. Movenko D.A., Shurtakov S.V. Microcrack formation and controlling in nickel superalloys processed by selective laser melting (review). Aviation materials and technologies, 2022, no. 2 (67), paper no. 04. Available at: http://www.journal.viam.ru (accessed: December 13, 2024). DOI: 10.18577/2713-0193-2022-0-2-43-51.
  9. Min P.G., Vadeev V.E., Sukhov D.I., Raevskikh A.N. Structure and mechanical properties of corrosion-resistant heat-resistant nickel alloy obtained by selective laser melting. Materialovedenie, 2021, no. 12, pp. 3–10. DOI: 10.31044/1684-579Х-2021-0-12-3-10.
  10. Vogel F., Cheng J., Liang S.B. et al. Formation and evolution of hierarchical microstructures in a Ni-based superalloy investigated by in situ high-temperature synchrotron X-ray diffraction. Journal of Alloys and Compounds, 2022, vol. 919, art. 165845. DOI: 10.1016/j.jallcom.2022.165845.
  11. Wang X., Carter L.N., Pang B. et al. Microstructure and yield strength of SLM-fabricated CM247LC Ni-Superalloy. Acta Materialia, 2017, vol. 128, pp. 87–95. DOI: 10.1016/j.actamat.2017.02.007.
  12. Won K.-U., Kim J.-Y., Yun J.-Y. et al. Fabrication of the CM247LC Ni-based superalloy using metal-material extrusion additive manufacturing and its microstructure and mechanical properties. Powder Metallurgy, 2025, vol. 68 (3), pp. 238–251. DOI: 10.1177/00325899251339695.
  13. Radavich J., Furrer D., Carneiro T., Lemsky J. The Microstructure and Mechanical Properties of EP741NP Powder Metallurgy Disc Material. Proceedings of the International Symposium on Superalloys. Pittsurg: TSM (The Minerals, Metals and Materials Society), 2008, pp. 63–72. DOI: 10.7449/2008/Superalloys_2008_63_72.
  14. Ioannidou C., König H.-H., Semjatov N. et al. In-situ synchrotron X-ray analysis of metal Additive Manufacturing: Current state, opportunities and challenges. Materials & Design, 2022, vol. 219, art. 110790. DOI: 10.1016/j.matdes.2022.110790.
  15. Carter L.N., Martin C., Withers P.J., Attallah M.M. The influence of the laser scan strategy on grain structure and cracking behaviour in SLM powder-bed fabricated nickel superalloy. Journal of Alloys and Compounds, 2014, vol. 615, pp. 338–347. DOI: 10.1016/j.jallcom.2014.06.172.
  16. Zhao Y., Li K., Gargani M., Xiong W. A comparative analysis of Inconel 718 made by additive manufacturing and suction casting: Microstructure evolution in homogenization. Additive Manufacturing, 2020, vol. 36, art. 101404. DOI: 10.1016/j.addma.2020.101404.
  17. Zhao Y., Zhao X., Qi X. et al. The origin of the straight propagation of the σ phase in a Ni-based single crystal superalloy at elevated temperature. Acta Materialia, 2024, vol. 275, art. 120056. DOI: 10.1016/j.actamat.2024.120056.
  18. Chou K.-C., Sridhar S., Pal U.B. Activities and ternary phase diagrams. Calphad, 1997, vol. 21, no. 4, pp. 483–495. DOI: 10.1016/S0364-5916(98)00006-6.
  19. Kalentics N., Ortega M. de Seijas V., Griffiths S. et al. 3D laser shock peening – A new method for improving fatigue properties of selective laser melted parts. Additive Manufacturing, 2020, vol. 33, art. 101112. DOI: 10.1016/j.addma.2020.101112.
  20. Wang B., Castellana J., Melkote S.N. A hybrid post-processing method for improving the surface quality of additively manufactured metal parts. CIRP Annals, 2021, vol. 70, no. 1, pp. 175–178. DOI: 10.1016/j.cirp.2021.03.010.
  21. Fertig R.S., Baker S.P. Dislocation dynamics simulations of dislocation interactions and stresses in thin films. Acta Materialia, 2010, vol. 58, no. 15, pp. 5206–5218. DOI: 10.1016/j.actamat.2010.06.001.
  22. Ramsperger M., Singer R.F., Körner C. Microstructure of the Nickel-Base Superalloy CMSX-4 Fabricated by Selective Electron Beam Melting. Metallurgical and Materials Transactions: A. Physical metallurgy and materials science, 2016, vol. 47, pp. 1469–1480. DOI: 10.1007/s11661-015-3300-y.
  23. Kenel C., De Luca A., Joglekar S.S. et al. Evolution of Y2O3 dispersoids during laser powder bed fusion of oxide dispersion strengthened Ni–Cr–Al–Ti γ/γʹ superalloy. Additive Manufacturing, 2021, vol. 47, p. 102224. DOI: 10.1016/j.addma.2021.102224.
  24. Xinxu L., Chonglin J., Yong Z. et al. Segregation and homogenization for a new nickel-based superalloy. Vacuum, 2020, vol. 177, art. 109379. DOI: 10.1016/j.vacuum.2020.109379.
  25. Smith T.M., Esser B.D., Antolin N. et al. Segregation and η phase formation along stacking faults during creep at intermediate temperatures in a Ni-based superalloy. Acta Materialia, 2015, vol. 100, pp. 19–31. DOI: 10.1016/j.actamat.2015.08.053.
  26. Zhao Y., Chang Y., Li X. et al. P phase precipitation and strengthening behavior of a novel polycrystalline Ni3Al-based intermetallic alloy at 1100 °C. Acta Materialia, 2024, vol. 265, art. 119601. DOI: 10.1016/j.actamat.2023.119601.
  27. Rettig R., Heckl A., Singer R.F. Modeling of Precipitation Kinetics of TCP-Phases in Single Crystal Nickel-Base Superalloys. Advanced Material Research, 2011, vol. 278, pp. 180–185. DOI: 10.4028/www.scientific.net/amr.278.180.
  28. DebRoy T., Wei H.L., Zuback J.S. et al. Additive manufacturing of metallic components – Process, structure and properties. Progress in Materials Science, 2018, vol. 92, pp. 112–224. DOI: 10.1016/j.pmatsci.2017.10.001.