Medvedev P.N., Moiseeva N.S., Kochubey A.Ya., Juravleva P.L. Structural factors determining applicability of the non-destructive X-ray diffraction method for assessing residual stress. Part 2 // Proceedings of VIAM. 2025. No. 7 (149). Ст. 10. URL: https://www.viam-works.ru. DOI: 10.18577/2307-6046-2025-0-7-130-140.

Structural factors determining applicability of the non-destructive X-ray diffraction method for assessing residual stress

Part 2
Medvedev P.N., Moiseeva N.S., Kochubey A.Ya., Juravleva P.L.
Abstract

The articlecompares the X-ray diffraction and metallographic methods for determining β- phase proportion in titanium alloys. The values of the β-phase proportion determined by the metallographic method are inflated against those determined by the X-ray method. These results show the necessity to improve these methods. The study of residual stresses has shown that when applying macrodeformation, the rate of the β-phase lattice deformation growth is higher than the same of the α-phase. The paper proposes to determine the  Poisson’s ratio by the X-ray method using the accessoriez for modeling of bending or uniaxial tension tests.

Keywords
surface residual stresses, metallography, phase composition, deformation
Reference list
  1. Gorelik S.S. Recrystallization. Moscow: MISiS, 2005, 432 p.
  2. Gorelik S.S., Skakov Yu.A., Rastorguev L.N. X-ray and electron-optical analysis: textbook for universities. 4th ed., supple. and rev. Moscow: MISiS, 2002, 360 p.
  3. Umansky Ya.S., Skakov Yu.A., Ivanov A.N., Rastorguev L.N. Crystallography, X-ray and electron microscopy. Moscow: Metallurgiya, 1982, 632 p.
  4. EN 15305:2008. Non-destructive Testing. Test Method for Residual Stress analysis by X-ray Diffraction. BSI Standards Publication, 2009, 88 p.
  5. Medvedev P.N., Kashapov O.S., Reshetilo L.P. Study of surface layers of titanium alloy VT41 after mechanical treatment. Voprosy materialovedeniya, 2022, no. 3 (111), pp. 49–58.
  6. Medvedev P.N., Gulyaev A.I. Analysis of the spatial distribution of cracks in a heat-resistant nickel alloy manufactured using SLM technology. Aviacionnye materialy i tehnologii, 2020, no. 1 (58), pp. 12–18. DOI: 10.18577/2071-9140-2020-0-1-12-18.
  7. Kablov E.N., Antipov V.V. The role of new generation materials in ensuring the technological sovereignty of the Russian Federation. Vestnik Rossiyskoy akademii nauk, 2023, vol. 93, no. 10, pp. 907–916.
  8. Kablov E.N., Nochovnaya N.A., Shiryaev A.A., Davydova E.A. Investigation of structural and phase transformations in metastable β-titanium alloys and effect of cooling rate from homogenization temperature on structure and properties of VT47 alloy. Part 2. Trudy VIAM, 2020, no. 8 (90), paper no. 02. Available at: http://www.viam-works.ru (accessed: July 28, 2024). DOI: 10.18577/2307-6046-2020-0-8-11-19.
  9. Kalashnikov V.S., Reshetilo L.P., Chuchman O.V., Naprienko S.A. Strength and reliability of rods and rotor blade stamps made of heat-resistant industrial titanium alloys and modern pseudo-α-titanium alloy. Trudy VIAM, 2022, no. 2 (108), paper no. 02. Available at: http://www.viam-works.ru (accessed: July 28, 2024). DOI: 10.18577/2307-6046-2022-0-2-13-31.
  10. Oglodkov M.S., Kashapov O.S., Kalashnikov V.S., Kondratieva A.R. Comparative analysis of the characteristics of domestic alloys VT8, VT8M, VT8M-1, VT9 and Ti6242S alloy (USA) as applied to high-pressure compressor blades of aircraft gas turbine engines. Aviation materials and technologies, 2024, no. 3 (76), paper no. 04. Available at: http://www.journal.viam.ru (accessed: August 27, 2024). DOI: 10.18577/2713-0193-2024-0-3-35-50.
  11. Kashapov O.S., Pavlova T.V., Kalashnikov V.S., Zavodov A.V. Prerequisites for the development of new low-alloyed technological medium strength titanium alloy with operating temperature up to 400–450 °С, capable of strengthening. Aviation materials and technologies, 2024, no. 1 (74), paper no. 03. Available at: http://www.journal.viam.ru (accessed: August 28, 2024). DOI: 10.18577/2713-0193-2024-0-1-33-50.
  12. Kablov E.N., Putyrskiy S.V., Yakovlev A.L., Krokhina V.A., Naprienko S.A. Study of fatigue fracture resistance of stampings made of high-strength titanium alloy VT22M, manufactured with final deformation in the (α+β)- and β-regions. Titan, 2021, no. 1 (70), pp. 26–33.
  13. Peskova A.V., Sukhov D.I., Mazalov P.B. Examination of the formation of the titanium alloy VT6 structure obtained by additive manufacturing. Aviacionnye materialy i tehnologii, 2020, no. 1 (58), pp. 38–44. DOI: 10.18577/2071-9140-2020-0-1-38-44.
  14. Kolpachev B.A., Elagin V.I., Livanov V.A. Metallurgy and heat treatment of non-ferrous metals and alloys: textbook for universities. 3rd ed., suppl. and rev. Moscow: MISiS, 2001, 416 p.
  15. Volkov N.V., Skrytny V.I., Filippov V.P., Yaltsev V.N. Physical materials science: textbook for universities in 8 vols. Moscow: NRNU MEPhI, 2012, vol. 3: Methods for studying the structural and phase state of materials, 800 p.