Barbotko S.L. About combustion of titanium alloys and methods of assessment of their fire hazard // Proceedings of VIAM. 2025. No. 6 (148). Ст. 09. URL: https://www.viam-works.ru. DOI: 10.18577/2307-6046-2025-0-6-110-120.

About combustion of titanium alloys and methods of assessment of their fire hazard

Barbotko S.L.
Abstract

Titanium has high melting point, low density and high mechanical properties, therefor it finds broad application in space engineering. The fire hazard characteristics of titanium, relevance of performed works and experimental methods of assessment are analyzed. It is established that there are no standardized test methods on fire hazard for samples of titanium alloys, as a result the obtained results are incomparable. The main requirements to which there has to correspond the test stand intended for assessment of fire hazard of samples made of titanium alloys are analyzed.

Keywords
titanium, titanium alloys, fire hazard, combustion, test methods, test equipment
Reference list
  1. Kablov E.N. Innovative developments of FSUE «VIAM» SSC of RF on realization of «Strategic directions of the development of materials and technologies of their processing for the period until 2030». Aviacionnye materialy i tehnologii, 2015, no. 1 (34), pp. 3–33. DOI: 10.18577/2071-9140-2015-0-1-3-33.
  2. Kablov E.N. Materials for Aerospace Engineering. Vse materialy. Entsiklopedicheskiy spravochnik, 2007, no. 5, pp. 7–27.
  3. Kablov E.N. Quality Control of Materials – a Guarantee of Safe Operation of Aviation Equipment. Aviatsionnye materialy i tekhnologii, 2001, no. 1, pp. 3–8.
  4. Perelman V.I. Brief Handbook of a Chemist. Moscow: State Sci. Publ. House of Chemical Literature, 1951. 676 p.
  5. Aviation Materials and Technologies. Ed. by E.N. Kablov. Moscow: VIAM, 2007, is.: Combustion and Fire Safety of Titanium Alloys, 80 p.
  6. Nochovnaya N.A., Alekseev E.B., Izotova A.Yu., Novak A.V. Fire-safe titanium alloys and features of their application. Titan, 2012, no. 4 (38), pp. 42–46.
  7. Bai A.S., Lainer D.I., Slesareva E.N., Tsypin M.I. Oxidation of titanium and its alloys. Moscow: Metallurgiya, 1970, 320 p.
  8. Pokhil P.F., Belyaev A.F., Frolov Yu.V., Logachev V.S., Korotkov A.I. Combustion of powdered metals in active environments. Moscow: Nauka, 1972, 294 p.
  9. Fox D.G. Investigation of Titanium Combustion Characteristics and Suppression Techniques: Report AFAPL-TR-75-73 Air Force Aero-Propulsion Laboratory, 1976, 66 p. Available at: https://www.fire.tc.faa.gov/pdf/fsr-0350.pdf (accessed: December 02, 2024).
  10. Sarkos С.P. Titanium Fuselage Environmental Conditions in Post-Crash Fires: Technical Report FAA-RD-71-3 (FAA-NA-71-2). FAA, US, 1971, 74 p. Available at: https://www.fire.tc.faa.gov/pdf/rd71-3.pdf (accessed: December 02, 2024).
  11. Sarkos С.P. Small-scale fire tests of high-temperature cabin pressure sealant and insulating materials: Report FAA-RD-71-67. Federal Aviation Administration. National Aviation Facilities Experimental Center, 1971. 35 p. Available at: https://www.fire.tc.faa.gov/pdf/rd71-67.pdf (accessed: December 02, 2024).
  12. Certification Specifications and Acceptable Means of Compliance for Large Aeroplanes. CS 25. Amendment 28. 1515 p. Available at: https://www.easa.europa.eu/en/document-library/certification-specifications/group/cs-25-large-aeroplanes#cs-25-large-aeroplanes (accessed: December 02, 2024).
  13. Titanium fire: Rosaviatsia named the reasons for the Tu-204 engine failure in flight. Available at: http://www.vesti.ru/doc.html?id=3052737 (accessed: December 02, 2024).
  14. Barbotko S.L., Volny O.S., Kiriyenko O.A., Shurkova E.N. Analysis of the main areas of research carried out by foreign organizations involved in fire safety of aviation equipment and aerospace materials (review). Problemy bezopasnosti poletov, 2018, no. 2, pp. 3–35.
  15. Uihlein T., Schlegel H. Titanium Fire In Jet Engines. Available at: http://www.fire.tc.faa.gov/pdf/fsr-0457.pdf (accessed: December 02, 2024).
  16. Antipov V.V. Prospects for development of aluminium, magnesium and titanium alloys for aerospace engineering. Aviacionnye materialy i tehnologii, 2017, no. S, pp. 186–194. DOI: 10.18577/2071-9140-2017-S-186-194.
  17. Arislanov A.A., Goncharova L.J., Nochovnaya N.А., Goncharov V.A. Prospects for the use of titanium alloys in laminated composite materials. Trudy VIAM, 2015, no. 10, paper no. 04. Available at: http://www.viam-works.ru (accessed: December 02, 2024) DOI: 10.18577/2307-6046-2015-0-10-4-4.
  18. Doronin O.N., Gorlov D.S., Azarovsky E.N., Kochetkov A.S. Study of the structure and properties of a heat-resistant coating at high-temperature deformation of samples from titanium intermetallic alloy. Aviation materials and technology, 2021, no. 1 (62), paper no. 06. Available at: http://www.journal.viam.ru (accessed: December 16, 2024). DOI: 10.18577/2013-0193-2021-0-1-61-70.
  19. Nochovnaya N.A., Panin P.V., Kochetkov A.S., Bokov K.A. VIAM experience in the field of development and research of economically alloyed titanium alloys of new generation. Trudy VIAM, 2016, no. 9, paper no. 05. Available at: http://www.viam-works.ru (accessed: December 02, 2024). DOI: 10.18577/2307-6046-2016-0-9-5-5.
  20. Kashapov O.S., Pavlova T.V., Kalashnikov V.S., Zavodov A.V. Prerequisites for the development of new low-alloyed technological medium strength titanium alloy with operating temperature up to 400–450 °С, capable of strengthening. Aviation materials and technologies, 2024, no. 1 (74), paper no. 03. Available at: http://www.journal.viam.ru (accessed: December 16, 2024). DOI: 10.18577/2713-0193-2024-0-1-33-50.
  21. Putyrskiy S.V., Plokhikh А.I., Arislanov А.A., Naprienko S.A., Anisimova A.Yu. Study of structure and mechanical properties of the laminar structure material based on titanium alloys VT1-0 and VT47. Aviation materials and technologies, 2023, no. 2 (71), paper no. 03. Available at: http://www.journal.viam.ru (accessed: December 16, 2024). DOI: 10.18577/2713-0193-2023-0-2-36-50.
  22. Barbotko S.L., Volny O.S., Kiriyenko O.A., Shurkova E.N. Fire safety assessment of polymeric materials for aviation purposes: analysis of the state, test methods, development prospects, methodological features. Ed. E.N. Kablov. Moscow: VIAM, 2018, 424 p.
  23. Barbotko S.L., Kiriyenko O.A., Volny O.S., Lutsenko A.N. Fire hazard analysis of aircraft engine nacelles and other fire hazardous areas; fire testing methods used for materials and structural elements for compliance with aviation standards. Problemy bezopasnosti poletov, 2017, no. 5, pp. 3–24.
  24. Barbotko S.L., Volny O.S., Veshkin E.A., Goncharov V.A. Assessment of fire resistance of materials and structural elements for aviation equipment. Aviatsionnaya promyshlennost, 2018, no. 2, pp. 63–67.
  25. Stobridge Th.R., Moulder J.C., Clark A.F. Titanium Combustion in turbine Engines: Report FAA-RD-79-51. NBSIR 79-1616, NBS, 1979, 137 p. Available at: https://nvlpubs.nist.gov/nistpubs/Legacy/IR/nbsir79-1616.pdf (accessed: December 02, 2024).
  26. Chernenko E.V., Griva V.A., Rozenband V.I. Study of the flammability patterns of titanium powders. Fizika goreniya i vzryva, 1982, vol. 18, no. 5, pp. 20–26.
  27. Bakhman N.N., Kuznetsov G.P., Puchkov V.M. Combustion of titanium plates. Fizika goreniya i vzryva, 2000, vol. 36, no. 4, pp. 60–65.
  28. Bolobov V.I. Mechanism of Self-Ignition of Titanium Alloys in Oxygen. Combustion, Explosion, and Shock Waves, 2002, vol. 38, no. 6, pp. 639–645.
  29. Belousova N.S., Glotov O.G., Guskov A.V. Study of titanium particle combustion. Aktualnye problemy aviatsii i kosmonavtiki, 2017, vol. 1, pp. 276–278.
  30. Glotov O.G. Ignition and combustion of titanium particles. Experimental research methods and results. Uspekhi fizicheskikh nauk, 2019, vol. 189, no. 2, pp. 135–171. DOI: 10.3367/UFNr.2018.04.038349.
  31. Kablov E.N., Kashapov O.S., Medvedev P.N., Pavlova T.V. Study of a α+β-titanium alloy based on a system of Ti–Al–Sn–Zr–Si–β-stabilizing alloying elements. Aviacionnye materialy i tehnologii, 2020, no. 1 (58), pp. 30–37. DOI: 10.18577/2071-9140-2020-0-1-30-37.
  32. Nochovnaya N.A., Nikitin Ya.Yu., Grigorenko V.B., Kozlov I.A. Changes in the surface properties of titanium alloy VT20 in the chemical removal of operational carbon pollution. Trudy VIAM, 2017, no. 10 (58), paper no. 05. Available at: http://www.viam-works.ru (accessed: December 02, 2024). DOI: 10.18577/2307-6046-2017-0-10-5-5.