Ivankov R.R., Klimenko O.N., Gulyaev I.N., Osiyanenko N.V. The influence of different cutting methods on the texture and stress-related properties of carbon fiber samples // Proceedings of VIAM. 2025. No. 6 (148). Ст. 04. URL: https://www.viam-works.ru. DOI: 10.18577/2307-6046-2025-0-6-46-63.

The influence of different cutting methods on the texture and stress-related properties of carbon fiber samples

Ivankov R.R., Klimenko O.N., Gulyaev I.N., Osiyanenko N.V.
Abstract

The article treats the five most commonly used methods for cutting products and structures made of polymer composite materials and provides the main advantages and disadvantages of each of them. This article also outlines the design features and principles of operation of each type of tool, with which the manufacture of standard test samples is carried out. The strength parameters and structure of carbon fiber plastics, which were made by different cutting methods, are given. Using the method of X-ray computed tomography, the analysis of the defective zone of the polymer composite material was carried out.

Keywords
carbon fiber reinforced plastics, cutting of carbon fiber polymer composite material, strength properties of carbon fiber polymer composite material, adhesion, polymer binder, X-ray computed tomography
Reference list
  1. Kablov E.N. New generation materials. Zashchita i bezopasnost, 2014, no. 4 (71), pp. 28–29.
  2. Rudskoy A.I. Technological heredity in the production and operation of structural materials. Tekhnologiya metallov, 2019, no. 2, pp. 2–10.
  3. Davydova I.F., Kablov E.N., Kavun N.S. Heat-resistant non-flammable polyimide glass-fiber laminates for products of aviation and rocket technology. Vse materialy. Entsiklopedicheskiy spravochnik, 2009, no. 7, pp. 2–11.
  4. Kablov E.N., Sagomonova V.A., Sorokin A.E., Tselikin V.V., Gulyaev A.I. Study of the structure and properties of a polymer composite material with an integrated vibration-absorbing layer. Vse materialy. Entsiklopedicheskiy spravochnik, 2020, no. 3, pp. 2–9.
  5. Kudritsky V.G. Composite materials for friction units for space applications. Polimernye materialy i tekhnologii, 2022, vol. 8, no. 3, pp. 82–88.
  6. Mikhailin Yu.A. Fibrous polymer composite materials in engineering. St. Petersburg: Nauchnye osnovy i tekhnologii, 2013, 720 p.
  7. Lurye S.A., Mironov Yu.M., Nelyub V.A. et al. Modeling the dependencies of physical and mechanical characteristics on the parameters of the micro- and nanostructure of polymer composite materials. Nauka i obrazovanie, 2012, no. 6, p. 4. DOI: 10.7463/0612.0431339.
  8. Petrova A.P., Malysheva G.V. Adhesives, adhesive binders and adhesive prepregs. Moscow: VIAM, 2017, 472 p.
  9. Sleptsov V.V. Methods of mechanical processing of machine parts made of polymer composite materials (review). Novye materialy i tekhnologii v mashinostroyenii, 2021, no. 34, pp. 80–83.
  10. Malysheva G.V., Guzeva, T.A., Fedorov B.B. Features of waterjet processing of fiberglass. Sovremennye naukoyemkie tekhnologii, 2018, no. 9, pp. 66–70.
  11. Yudina E.V. Modern technologies for improving the efficiency and quality of mechanical processing of polymer composite materials used in rocket and space technology. Innovatsii. Nauka. Obrazovaniye, 2020, no. 22, pp. 323–332.
  12. Golovanov D.S. Study of the influence of waterjet machining on parts made of polymer-composite materials. Vestnik RGATA im. P.A. Solovyeva, 2023, no. 1 (64), pp. 92–98.
  13. Golovanov D.S., Mitin R.A., Tolkachev A.V. Influence of form-generating waterjet machining on combined materials: polymer-composite material – titanium alloy. Vestnik RGATA im. P.A. Solovyeva, 2023, no. 4 (67), pp. 45–48.
  14. Bolotnikov I.S., Kosenko E.A. Methods and technological features of cutting polymer composite materials (review). Energy and resource-saving technologies and equipment in the road and construction industries: proc. Int. scientific-practical. conf. (September 23–25, 2021, Belgorod). Belgorod: BSTU named after V.G. Shukhov, 2021, рp. 19–25.
  15. Verchenko A.V., Kurskaya I.A., Chigrinets E.G. Optimization of the process of waterjet cutting of workpieces from aviation materials. Vestnik Moskovskogo aviatsionnogo instituta, 2019, vol. 26, no. 1, рp. 212–229.
  16. Golubeva K.R., Noskov A.I. Technologies for processing materials based on fiberglass. Naukoyemkie tekhnologii v mashinostroenii, 2021, no. 6 (120), pp. 24–28. DOI: 10.30987/2223-4608-2021-6-24-28.
  17. Raskutin A.E., Khrulkov A.V., Girsh R.I. Technological features of machining of composite materials when manufacturing details of designs (review). Trudy VIAM, 2016, no. 9, paper no. 12. Available at: http://www.viam-works.ru (accessed: July 18, 2024). DOI: 10.18577/2307-6046-2016-0-9-12-12.
  18. Pripisnov Ya.A., Grishina O.I. Modern methods of mechanical processing of composite materials (review). Trudy VIAM, 2018, no. 10 (70), paper no. 07. Available at: http://www.viam-works.ru (accessed: July 18, 2024). DOI: 10.18577/2307-6046-2018-0-10-53-61.
  19. Dyshenko V.S., Donetskiy K.I., Minibaev M.I., Ablyaz T.R., Shlykov E.S., Shiryaev V.V. Methods of mechanical and electrical discharge machining of polymer composite materials (review). Trudy VIAM, 2018, no. 3 (109), paper no. 10. Available at: http://www.viam-works.ru (accessed: July 18, 2024). DOI: 10.18577/2307-6046-2022-0-3-102-120.
  20. Khrulkov I.A., Gulyaev I.N., Mishkin S.I. Features of cutting polymer composite materials with diamond wheels (review). Trudy VIAM, 2022, no. 4 (110), paper no. 02. Available at: http://www.viam-works.ru (accessed: July 18, 2024). DOI: 10.18577/2307-6046-2022-0-4-22-31.
  21. Grishchenko T.A., Melyukhov N.I., Lyubushkin V.O. Application of waterjet cutting in processing parts made of polymer composite materials. Vestnik Inzhenernoy shkoly Dalnevostochnogo federalnogo universiteta, 2017, no. 2 (31), pp. 49–55. DOI: 10.5281/zenodo.808901.
  22. Makarov V.F., Meshkas A.E. Modern methods of mechanical processing of parts made of high-strength composite materials for aviation and rocket and space technology. Modern trends in metalworking technologies and designs of metalworking machines and components: interuniv. sci. coll. Ufa: Ufa State Aviation Tech. Univ., 2015, pp. 14–20.
  23. Titov S.A., Ryzhova T.B., Vermel V.D. et al. Assessment of PCM damage during mechanical processing (milling, drilling) using acoustic microscopy. Proceedings of the V industry conf. on measuring equipment and metrology for aircraft research «KIMILA–2023» (October 17–18, 2023, Zhukovsky). Zhukovsky: TsAGI named after prof. N.E. Zhukovsky, 2023, рp. 292–299.
  24. Kozhevnikov S.I., Makarov V.F. Theoretical studies of the influence of the milling trajectory of form-forming surfaces on the wear resistance of tooling. Avtomatizirovannoe proyektirovanie v mashinostroyenii, 2018, no. 6, pp. 117–120.
  25. Dudarev A.S., Aleksutin A.S. Problems of modeling the milling process of polymer composite materials. Science, theory, practice of the aviation-industrial cluster of modern Russia: Reports V Int. Sci.-prod. conf., dedicated to the Day of Russian Science (February 06–07, 2020, Ulyanovsk). Ulyanovsk: USTU, 2020, pp. 48–56.
  26. Polovnev D.I., Baurova N.I. Selection of methods of mechanical processing of polymer composite materials used in the production and repair of machines. Novye materialy i tekhnologii v mashinostroyenii, 2019, no. 29, pp. 77–80.
  27. Sleptsov V.V. Assessment of the influence of processing technology on the quality of holes in machine parts made of polymer composite materials. Novye materialy i tekhnologii v mashinostroyenii, 2022, no. 36, pp. 113–116.
  28. Geraskina M.E., Kazakova T.Yu., Nepomnyashchiy Yu.G. et al. Methods of cutting a curved surface of a reflector manufactured using RTM technology. Reshetnev readings: materials of the XXVI Int. scientific and practical. conf., dedicated to the memory of the general designer of rocket and space systems, academician M.F. Reshetnev (November 9–11, 2022, Krasnoyarsk). Krasnoyarsk: SSU of Science and Technology named after academician M.F. Reshetnev, 2022, part 1, pp. 20–23.
  29. Lobanov D.V., Danilov P.G., Vladimirova N.A., Grigoriev A.N. Development of an experimental stand for studying the process of processing non-metallic composite materials. Aktualnye problemy v mashinostroenii, 2021, vol. 8, no. 3-4, pp. 87–98.
  30. Dudarev A.S., Nechaeva E.V. Calculation of thermal stress in the process of cutting polymer composite materials with a carbide tool. Uchenye zapiski Krymskogo inzhenerno-pedagogicheskogo universiteta, 2022, no. 3 (77), pp. 152–156. DOI: 10.34771/UZCEPU.2022.77.3.029.
  31. Dudarev A.S., Gumarov E.Kh. Study of thermophysics during diamond drilling of fibreglass and carbon fibre-reinforced polymer composites. Proceedings of Irkutsk State Technical University, 2021, vol. 25, no. 3, pp. 290–299. DOI: 10.21285/1814-3520-2021-3-290-299.
  32. Usacheva A.O., Gopantsov D.N., Vakulin M.S., Kazakov I.S. Influence of geometric parameters of end mills on surface quality during high-speed processing of carbon fiber reinforced plastics. Technologies and equipment: ways of innovative development: Reports Int. scientific and technical conf. (June 9, 2023, Voronezh). Voronezh: VSTU, 2023, pp. 517–520.
  33. Minibaev M.I., Usacheva M.N., Dyshenko V.S., Goncharov V.A. A device and tool for making sample from polymer composite materials on a CNC machine (review). Trudy VIAM, 2021, no. 4 (98), paper no. 08. Available at: http://www.viam-works.ru (accessed: July 22, 2024). DOI: 10.18577/2307-6046-2021-0-4-100-109.
  34. Minibaev M.I., Raskutin A.E., Goncharov V.A. Peculiarities of technology production specimens of PCM on CNC machines (review). Trudy VIAM, 2019, no. 1 (73), paper no. 11. Available at: http://www.viam-works.ru (accessed: July 22, 2024). DOI: 10.18577/2307-6046-2019-0-1-105-114.
  35. Noskov A.I., Gilmutdinov A.Kh., Asadullina A.R. Features of laser cutting of carbon polymer composite materials. Uspekhi prikladnoy fiziki, 2019, vol. 7, no. 2, pp. 155–164.
  36. Yaresko S.I., Balakirov S.N. Modeling of a composite material for laser dimensional processing. Izvestiya Volgogradskogo gosudarstvennogo tekhnicheskogo universiteta, 2021, no. 3 (250), pp. 46–50. DOI: 10.35211/1990-5297-2021-3-250-46-50.
  37. Eltawahni H.A., Olabi A.G., Basmage O.M., Benyounis K.Y. CO2 Laser Cutting of Glass Fiber-Reinforced Plastics. Encyclopedia of Renewable and Sustainable Materials, 2020, vol. 1, pp. 145–159.
  38. Ablyaz T.R. Improving the efficiency of electrical discharge machining of special-purpose products with composite electrode tools. Materials, 2021, vol. 14, no. 20. DOI: 10.3390/ma14206105.
  39. Ablyaz T.R., Shlykov E.S., Muratov K.R., Sidhu S.S. Analysis of wire-cut electro discharge machining of polymer composite materials. Micromachines, 2021, vol. 12, no. 5. DOI: 10.3390/mi12050571.
  40. Hsissou R., Benkhaya S., Elharfi A. et al. New epoxy composite polymers as a potential anticorrosive coatings for carbon steel in 3.5% NaCl solution: Experimental and computational approaches. Chemical Data Collections, 2021, vol. 31, p. 100619. DOI: 10.1016/j.cdc.2020.100619.
  41. Hsissou R., Bekhta A., Rafik M. et al. Rheological properties of composite polymers and hybrid nanocomposites. Heliyon, 2020, vol. 6, no. 6, p. e187. DOI: 10.1016/j.heliyon.2020.e04187.
  42. Thomason J. A review of the analysis and characterisation of polymeric glass fibre sizings. Polymer Testing, 2020, vol. 85, p. 106421. DOI: 10.1016/j.polymertesting.2020.106421.
  43. Kablov E.N., Laptev A.B., Prokopenko A.N., Gulyaev A.I. Relaxation of polymeric composite materials under the prolonged action of static load and climate (review). Part 1. Binders. Aviation materials and technologies, 2021, no. 4 (65), paper no. 08. Available at: http://www.journal.viam.ru (accessed: July 18, 2024). DOI: 10.18577/2713-0193-2021-0-4-70-80.
  44. Kablov E.N. Innovative developments of FSUE «VIAM» SSC of RF on realization of «Strategic directions of the development of materials and technologies of their processing for the period until 2030». Aviacionnye materialy i tehnologii, 2015, no. 1 (34), pp. 3–33. DOI: 10.18577/2071-9140-2015-0-1-3-33.