Khrulkov A.V., Donetskiy K.I., Melnikov D.A., Klimenko O.N., Slavin A.V. Prepreg tack as a function of various parameters during laying out blanks of parts and samples from polymer composite materials // Proceedings of VIAM. 2025. No. 3 (145). Ст. 04. URL: https://www.viam-works.ru. DOI: 10.18577/2307-6046-2025-0-3-33-46.

Prepreg tack as a function of various parameters during laying out blanks of parts and samples from polymer composite materials

Khrulkov A.V., Donetskiy K.I., Melnikov D.A., Klimenko O.N., Slavin A.V.
Abstract

Polymer composite materials are gradually replacing metals, including in such important structures as an aircraft wing or a fuselage. One of the technological stages in the manufacture of blanks for future parts is the process of laying out the prepreg on the tooling. When laying out, the stickiness of the prepreg plays an important role. The stickiness of the prepreg to the substrate should be such that it does not separate from it during transportation and is easily separated when moving onto the tooling. An analysis of the stickiness level depending on temperature, compaction force, and the speed of separation from the substrate is given in this article.

Keywords
tack, cohesion, temperature, tooling
Reference list
  1. Kablov E.N. New generation materials and digital technologies for their processing. Vestnik Rossiyskoy akademii nauk, 2020, vol. 90, no. 4, pp. 331–334.
  2. Slavin A.V., Donetskiy K.I., Khrulkov A.V. Prospects for the use of polymer composite materials in aircraft structures in 2025–2035 (review). Trudy VIAM, 2022, no. 11 (117), paper no. 08. Available at: http://www.viam-works.ru (accessed: September 05, 2024). DOI: 10.18577/2307-6046-2022-0-11-81-92.
  3. Kablov E.N. The role of fundamental research in the creation of new generation materials. Reports of the XXI Mendeleev Congress on General and Applied Chemistry: in 6 vols. St. Petersburg, 2019, vol. 4, p. 24.
  4. Onishchenko G.G., Kablov E.N., Ivanov V.V. Scientific and technological development of Russia in the context of achieving national goals: problems and solutions. Innovatsii, 2020, no. 6 (260), pp. 3–16.
  5. Tkachuk A.I., Donetsky K.I., Terekhov I.V., Karavaev R.Yu. The use of thermosetting matrices for the manufacture of polymer composite materials by the non-autoclave molding methods. Aviation materials and technology, 2021, no. 1 (62), paper no. 03. Available at: https://www.journal.viam.ru (accessed: August 02, 2024). DOI: 10.18577/2713-0193-2021-0-1-22-33.
  6. Bolshakov V.A., Antyufeeva N.V. Evaluation of the curing process model of the adhesive binder in prepreg. Aviation materials and technologies, 2023, no. 4 (73), paper no. 07. Available at: http://www.journal.viam.ru (accessed: August 02, 2024). DOI: 10.18577/2713-0193-2023-0-4-66-77.
  7. Startsev V.O., Antipov V.V., Slavin A.V., Gorbovets M.A. Modern domestic polymer composite materials for aviation industry (review). Aviation materials and technologies, 2023, no. 2 (71), paper no. 10. Available at: http://www.journal.viam.ru (accessed: August 02, 2024). DOI: 10.18577/2713-0193-2023-0-2-122-144.
  8. Mukhametov R.R., Petrova A.P. Thermosetting binders for polymer composite materials: textbook. Ed. E.N. Kablov. Moscow: NRC «Kurchatov Institute» – VIAM, 2021, p. 363.
  9. Tkachuk A.I., Lyubimova A.S., Kuznetcova P.A. Opportunities of the development of plant-based epoxy resins (review). Trudy VIAM, 2022, no. 8 (114), paper no. 04. Available at: http://www.viam-works.ru (accessed: November 08, 2023). DOI: 10.18577/2307-6046-2022-0-8-49-64.
  10. Kogan D.I., Chursova L.V., Panina N.N. et al. Promising polymeric materials for structural composite products with energy-efficient molding mode. Plasticheskie massy, 2020, no. 3–4, pp. 52–54.
  11. Veshkin E.A. Technologies for non-autoclave molding of low-porosity polymer composite materials and large-sized structures made of them: thesis, Cand. Sc. (Tech.). Moscow, 2016, 146 p.
  12. Erasov V.S., Sibayev I.G. Scheme for the development and evaluation of properties of structural aviation composite materials. Aviation materials and technologies, 2023, no. 1 (70), paper no. 05. Available at: http://www.journal.viam.ru (accessed: December 04, 2023). DOI: 10.18577/2713-0193-2023-0-1-61-81.
  13. Postnov V.I., Veshkin E.A., Makrushin K.V., Sudin Yu.I. Technological features of manufacturing polymer composite materials of main rotor blades for a light helicopter. Aviation materials and technologies, 2023, no. 1 (70), paper no. 06. Available at: http://www.journal.viam.ru (accessed: December 04, 2023). DOI: 10.18577/2713-0193-2023-0-1-82-92.
  14. Raskutin A.E. Russian polymer composite materials of new generation, their exploitation and implementation in advanced developed constructions. Aviacionnye materialy i tehnologii, 2017, no. S, pp. 349–367. DOI: 10.18577/2071-9140-2017-0-S-349-367.
  15. Budelmann D., Schmidt C., Meiners D. Adhesion-cohesion balance of prepreg tack in thermoset automated fiber placement. Part 1: Adhesion and surface wetting. Composites Part C, 2023, no. 12, art. 100396.
  16. Budelmann D., Schmidt C., Meiners D. Prepreg tack: A review of mechanisms, measurement, and manufacturing implication. Polymer Composites, 2020, no. 41, pp. 3440–3458. DOI: 10.1002/pc.25642.
  17. Budelmann D. Tack of epoxy resin films for aerospace-grade prepregs: Influence of resin formulation, B-staging and toughening. Polymer Testing, 2022, no. 114, art. 107709.
  18. Gerasimov S.B. Development of polymer composite materials for the manufacture of large-sized complex-profile products using the automated laying method: thesis, Cand. Sc. (Techn.). Moscow, 2000, p. 24.
  19. Budelmann D., Schmidt C., Steuernagel L., Meiners D. Adhesion-cohesion balance of prepreg tack in thermoset automated fiber placement. Part 2: Ply-ply cohesion through contact formation and autohesion. Composites Part C, 2023, no. 12, art. 100396.
  20. Postnov V.I., Nikitin K.E., Petukhov V.I., Burkhan O.L., Orzaev V.G. Method and device for determining the tack of prepregs. Aviacionnye materialy i tehnologii, 2009, no. 3, pp. 29–33.
  21. Strelnikov S.V., Petukhov V.I., Postnov V.I., Shvets N.I. New solutions in the technology of manufacturing prepregs for interior panels. Izvestiya Samarskogo nauchnogo tsentra RAN, 2011, vol. 13, no. 4 (2), pp. 498–507.
  22. Measuring techniques for prepreg tackiness: A COMPARATIVE STUDY SAMPE Europe Conference 2023 Madrid – Spain. Available at: https://www.researchgate.net/publication/374949895_Measuring_techniques_for_ prepreg_tackiness_A_comparative_study (available at: September 17, 2024).
  23. Crossley R.J., Schubel P.J., Warrior N.A. The experimental determination of prepreg tack and dynamic stiffness. Composite Part A: Applied Science Manufacture, 2012, no. 43, pp. 423–434.
  24. Heinecke F., Willberg C. Manufacturing-induced imperfections in composite parts manufactured via automated fiber placement. Experimental Mechanics, 2010, no. 50, pp. 599–606.
  25. Experimental analysis of prepreg tack. Available at: https://inria.hal.science/hal-01131583/ (available at: September 17, 2024).
  26. Tackiness characterization of thermoset prepreg materials. Available at: https://spectrum.library.concordia.ca/id/eprint/987702/1/Dodongeh_MASc_S2021.pdf (available at: September 17, 2024).
  27. Mishkin S.I., Klimenko O.N., Kutcevich K.E. Determination of stickiness of prepregs on the basis of carbon fillers the sounding method. Trudy VIAM, 2018, no. 3 (109), paper no. 04. Available at: http://www.viam-works.ru (accessed: August 05, 2024). DOI: 10.18577/2307-6046-2022-0-3-35-43.