Sorokin I.A., Solovyanchik L.V., Mekalina I.V., Tsapenko A.N. Optically transparent polymer films with anti-reflective coating // Proceedings of VIAM. 2025. No. 2 (144). Ст. 07. URL: https://www.viam-works.ru. DOI: 10.18577/2307-6046-2025-0-2-89-99.

Optically transparent polymer films with anti-reflective coating

Sorokin I.A., Solovyanchik L.V., Mekalina I.V., Tsapenko A.N.
Abstract

At present, the most appropriate way to prevent mechanical damage to the screens of indicating devices is to use protective glasses on a polymer base, which can be integrated into the finished design. To improve the quality of displayed information, it is necessary to reduce the intensity of glare, as well as to ensure maximum light transmission of these products, which can be achieved by applying optical coatings. This paper presents the results of research on obtaining a four-layer anti-reflective coating based upon TiО2 and SiО2 on a polymer film with and without an adhesive layer, and presents their characteristics.

Keywords
anti-reflective film, anti-glare coating, anti-reflective coating, reactive magnetron sputtering
Reference list
  1. Rudnev V.P., Mekalina I.V. Properties of organic glasses after natural aging under load in humid subtropics. Aviation materials and technologies, 2022, no. 4 (69), paper no. 08. Available at: http://www.journal.viam.ru (accessed: September 02, 2024). DOI: 10.18577/2713-0193-2022-0-4-84-95.
  2. Chizhov P.N., Petrachkov D.N., Shatalin V.A. et al. Influence of the polycarbonate sheet molding method on the optical characteristics of aircraft glazing products. Aviation materials and technologies, 2023, no. 2 (71), paper no. 05. Available at: http://www.journal.viam.ru (accessed: September 02, 2024). DOI: 10.18577/2713-0193-2023-0-2-63-76.
  3. Smirnova O.V., Erofeeva S.B. Polycarbonates. Moscow: Khimiya, 1975, 288 p.
  4. Sivukhin D.V. General course of physics: in 5 vols. 3rd ed. Moscow: FIZMATLIT, 2005, vol. 4: Optics, 792 p.
  5. Ilyina E., Lukin P. Effect of protective screen on light distribution of luminaire. Poluprovodnikovaya svetotekhnika, 2012, vol. 4, no. 18, pp. 44–47.
  6. Optical interference coatings. Eds. N. Kaiser, H.K. Pulker. Berlin: Springer-Verlag, 2003, 503 р. DOI: 10.1007/978-3-540-36386-6.
  7. Koglin J.E., Christensen F.E., Craig W.W. et al. NuSTAR hard X-ray optics. Proceedings of SPIE. San Diego, 2005, р. 5900. DOI: 10.1117/12.618601.
  8. Harry G.M., Armandula H., Black E. et al. Thermal noise from optical coatings in gravitational wave detectors. Applied Optics, 2006, vol. 45, no. 7, p. 1569–1574. DOI: 10.1364/ao.45.001569.
  9. Shanmugam N., Pugazhendhi R., Elavarasan R.M. et al. Anti-reflective coating materials: A holistic review from PV perspective. Energies, 2020, vol. 13, no. 10, p. 2631. DOI: 10.3390/en13102631.
  10. Lequime M., Nadji S., Stojcevski D. et al. Determination of the optical constants of a dielectric layer by processing in situ spectral transmittance measurements along the time dimension. Applied Optics, 2017, vol. 56, p. 181. DOI: 10.1364/ao.56.00c181.
  11. Nadji S.L., Lequime M., Begou T. et al. Use of a broadband monitoring system for the determination of the optical constants of a dielectric bilayer. Applied Optics, 2018, vol. 57, p. 877. DOI: 10.1364/ao.57.000877.
  12. Dvoretskaya E.V., Korolev D.V., Piskorskii V.P., Valeev R.A., Koplak O.V., Morgunov R.B. Magnetron sputtering of the iron shell and microinclusions in microwires PrDyFeCoB. Aviation materials and technologies, 2022, no. 2 (67), paper no. 08. Available at: http://www.journal.viam.ru (accessed: September 02, 2024). DOI: 10.18577/2713-0193-2022-0-2-85-96.
  13. Bogatov V.A., Krynin A.G., Shchur P.A. Influence of the leakage value in the vacuum chamber on the parameters of reactive magnetron discharge and properties of titanium oxide coatings. Aviacionnye materialy i tehnologii, 2019, no. 1 (54), pp. 17–22. DOI: 10.18577/2071-9140-2019-0-1-17-22.
  14. Konstantinova Yu.A. Anti-reflective coatings for solar batteries. Nauchnye issledovaniya: ot teorii k praktike, 2015, no. 3, pp. 198–200.
  15. Tsekhanovskaya M.S., Sheinberger A.A., Kutsenko K.V., Ivanichko S.P. Anti-reflective coatings for semiconductor electro-optical devices based on InP. XIX Int. scientific-practical. conf. Tomsk: Tomsk State Univ. of control systems and radioelectronics, 2023, pp. 177–179.
  16. Troitsky B.B., Lokteva A.A., Lopatin M.A. et al. Production of antireflective coatings from mesoporous silicon dioxide on silicate glass at low gel firing temperatures. Fizika i khimiya stekla, 2013, vol. 39, no. 5, pp. 715–722.
  17. Melnikov A.A., Shchur P.A. Transparent conductive antireflective coatings based on ITO, SiO2, TiO2. Trudy VIAM, 2019, No. 8 (80), paper no. 07. Available at: http://www.viam-works.ru (accessed: September 03, 2024). DOI: 10.18577/2307-6046-2019-0-8-56-66.
  18. Kleinhempel R., Wahl A., Thielsch R. Large area AR coating on plastic substrate using roll to roll methods. Surface and Coatings Technology, 2011, vol. 205, рр. S502 S505. DOI: 10.1016/j.surfcoat.2010.10.064.
  19. Kablov E.N. Innovative developments of FSUE «VIAM» SSC of RF on realization of «Strategic directions of the development of materials and technologies of their processing for the period until 2030». Aviacionnye materialy i tehnologii, 2015, no. 1 (34), pp. 3–33. DOI: 10.18577/2071-9140-2015-0-1-3-33.
  20. Kablov E.N. New Generation Materials – the Basis for Innovation, Technological Leadership, and National Security of Russia. Intellekt i tekhnologii, 2016, no. 2 (14), pp. 16–21.
  21. Kablov E.N. Chemistry in aviation materials science. Rossiyskiy khimicheskiy zhurnal, 2010, vol. LIV, no. 1, pp. 3–4.
  22. Kablov E.N. What is the innovations. Nauka i zhizn, 2011, no. 5, рр. 2–6.
  23. Laptev A.B., Pavlov M.R., Zeleneva T.O. Light sources for simulating the aging of polymer materials under the influence of solar radiation. Trudy VIAM, 2024, no. 5 (135), paper no. 07. Available at: http://www.viam-works.ru (accessed: September 10, 2024). DOI: 10.18577/2307-6046-2024-0-5-71-82.
  24. Kuzmichev A.I. Magnetronnye spraying systems. Kyiv: Avers, 2008, book 1: Introduction in physics and equipment of magnetron sputtering, 244 р.