Potapov M.V., Valeev R.A., Morgunov R.B., Piskorsky V.P. Properties of sintered magnets (Pr, Nd, Ce, Dy)(Fe, Co)B obtained from unrefined rare earth metals // Proceedings of VIAM. 2025. No. 2 (144). Ст. 05. URL: https://www.viam-works.ru. DOI: 10.18577/2307-6046-2025-0-2-65-74.
Properties of sintered magnets (Pr, Nd, Ce, Dy)(Fe, Co)B obtained from unrefined rare earth metals
Abstract
Sintered materials of the following composition (NdWPrpDyzCex)–(Fe1-yCoy)–B (w ≤ 0,44; p ≤ 0,45; x ≤ 0,13; z ≤ 0,41; y ≤ 0,26) were studied. Hysteresis curves of demagnetization by induction and magnetization are given. It was found that the admixture of neodymium and cerium in the studied quantities does not adversely affect the magnetic characteristics of sintered materials. Thus, suitable sintered materials can be made from insufficiently purified rare earth metals, although the value of the temperature coefficient of induction of materials of such composition is insufficient for use in navigation devices.
Keywords
permanent magnets, rare-earth magnets, saturation magnetization, residual induction, coercive force, temperature coefficient of induction
Reference list
- Production of rare and rare earth metals. Moscow: NTD Bureau, 2014, pp. 84–116
- Hirosawa S., Matsuura Yu., Yamamoto H. et al. Magnetization and magnetic anisotropy of R2Fe14B measured on single crystals. Journal of Applied Physics, 1986, vol. 59, pp. 873–879.
- Buschow K.H.J., de Mooij D.B., Sinnema S. et al. Magnetic and crystallographic properties of ternary rare earth compounds of the type R2Co14B. Journal of Magnetism and Magnetic Materials, 1985, vol. 51, pp. 211–217.
- Boltich E.B., Oswald E., Huang M.Q. et al. Magnetic characteristics of R2Fe14B systems prepared with high purity rare earths (R = Ce, Pr, Dy and Er). Journal of Applied Physics, 1985, vol. 57, pp. 4106–4108.
- Matusevich V.A., Getya A.N., Sharaban Yu.V. Application of high-coercivity permanent magnets in aircraft units. Elektrotekhnika i Elektromekhanika, 2006, no. 1, pр. 33–35.
- Sinnema S., Franse J.J.M., Radwanski R.J. et al. Magnetic measurements on R2Fe14B and R2Co14B compounds in high field. Journal de Physique, 1985, vol. 46, pp. C6-301‒C6-304.
- Abache C., Oesterreicher H. Magnetic properties of compounds R2Fe14B. Journal of Applied Physics, 1985, vol. 57, pp. 4112–4114.
- Korolev D.V., Piskorskii V.P., Valeev R.A., Bakradze M.M., Dvoretskaya E.V., Koplak O.V., Morgunov R.B. Rare-earth RE–TM–B micromagnets engineering (review). Aviation materials and technology, 2021, no. 1 (62), paper no. 05. Available at: http://www.journal.viam.ru (accessed: July 29, 2024). DOI: 10.18577/2713-0193-2021-0-1-44-60.
- Faria R.N., Davies B.E., Brown D.N. et al. Microstructural and magnetic studies of cast and annealed Nd and PrFeCoBZr alloys and HDDR materials. Journal of Alloys and Compounds, 2000, vol. 296, pp. 223–228.
- Cherednichenko I.V., Bavina M.A., Bondarenko Yu.A., Shurygin V.D., Ovchinnikov A.D., Galimullin S.A. Influence of directed crystallization parameters on structure and properties of Alnico 5-7 alloy permanent magnets. Trudy VIAM, 2023, no. 11 (129), paper no. 08. Available at: http://www.viam-works.ru (accessed: June 27, 2024). DOI: 10.18577/2307-6046-2023-0-11-77-89.
- Kablov E.N. Innovative developments of FSUE «VIAM» SSC of RF on realization of «Strategic directions of the development of materials and technologies of their processing for the period until 2030». Aviacionnye materialy i tehnologii, 2015, no. 1 (34), pp. 3–33. DOI: 10.18577/2071-9140-2015-0-1-3-33.
- Kablov E.N., Ospennikova O.G., Vershkov A.V. Rare metals and rare earth elements – materials of modern and future high technologies. Trudy VIAM, 2013, no. 2, paper no. 01. Available at: http://www.viam-works.ru (accessed: June 27, 2024).
- Lapteva K.A., Tolmachev I.I. Calculation of the demagnetizing factor during longitudinal magnetization in magnetic particle testing. Izvestiya Tomskogo politekhnicheskogo universiteta, 2012, vol. 321, no. 2, pp. 140–144.
- Sato M., Ishii Y. Simple and approximate expressions of demagnetizing factors of uniformly magnetized rectangular rod and cylinder. Journal of Applied Physics, 1989, vol. 66, no. 2, pp. 983–985.
- Chen D., Brug J.A., Goldfarb R.B. Demagnetizing factor for cylinder. IEEE Transactions on Magnetics, 1991, vol. 27, no. 4, pp. 3601–3619.
- Valeev R.A., Korolev D.V., Morgunov R.B., Piskorsky V.P. The effect of high concentrations of cobalt on the properties of magnets Pr–Dy–Fe–Co–B and Nd–Dy–Fe–Co–B. Trudy VIAM, 2022, no. 10 (116), paper no. 06. Available at: http://www.viam-works.ru (accessed: June 27, 2024). DOI: 10.18577/2307-6046-2022-0-10-66-75.
- Perigo E.A., Takiishi H., Motta C.C. et al. On the squareness factors behavior of RE‒FeB (RE=Nd or Pr) magnets above room temperature. IEEE Transactions on Magnetics, 2000, vol. 45, no. 10, pp. 4431‒4434.
- Yujing Z., Tranyu M., Mi Y. et al. Squareness factors of demagnetization curves for multi-main-phase Nd‒Ce‒Fe-B magnets with different Ce contents. Journal of Magnetism and Magnetic Materials, 2019, vol. 487. DOI: 10/1016/j.jmmm.2019.165355.
- Valeev R.A., Korolev D.V., Morgunov R.B., Piskorsky V.P. The contribution of phases to the magnetization of sintered materials Nd–Dy–Fe-Co–B. Trudy VIAM, 2022, no. 11 (117), paper no. 06. Available at: http://www.viam-works.ru (accessed: June 27, 2024). DOI: 10.18577/2307-6046-2022-0-11-60-68.
- Kablov E.N., Petrakov A.F., Piskorsky V.P., Valeev R.A., Nazarova N.V. Influence of dysprosium and cobalt on the temperature dependence of magnetization and phase composition of materials of the Nd‒Dy‒Fe‒Co‒B system. Metallovedenie i termicheskaya obrabotka metallov, 2007, no. 4, pp. 3–10.
- Corfield M.R., Williams A.J., Harris I.R. The effect on long annealing at 1000°C for 24 h on the microstructure and magnetic properties of Pr‒Fe‒B/Nd‒Fe‒B magnets based on Nd16Fe76B8 and Pr16Fe76B8. Journal of Alloys and Compounds, 2000, vol. 296, pp. 138–147.
- Faria R.N., Davies B.E., Brown D.N. et al. Microstructural and magnetic studies of cast and annealed Nd and Pr‒Fe‒Co‒B‒Zr alloys and HDDR materials. Journal Alloys and Compounds, 2000, vol. 296, pp. 223–228.
- Urusov V.S. Theoretical crystal chemistry. Moscow: Moscow State Univ. Press, 1987, 275 p.
- Cook B.A., Harringa J.L., Laabs F.C. et al. Diffusion of Fe, Co, Nd and Dy in R2(Fe1‒xCox)14B where R=Nd or Dy. Journal of Magnetism and Magnetic Materials, 2001, vol. 233, pp. L136‒L141.
- Smirnov B.M., Son E.E., Tereshonok D.V. Diffusion and mobility of atomic particles in liquid. Zhurnal eksperimentalnoy i teoreticheskoy fiziki, 2017, vol. 152, is. 5, pp. 1065–1072.
- Kryukov Ya.V., Samsonov N.Yu., Yatsenko V.A. Russian rare earth industry: should we adopt China’s experience? EKO, 2018, no. 10 (532), pp. 138–152. DOI: 10.30680/ЭСО0131-7652-2018-10-138-152.