Sevalnev G.S., Oblivantsev K.D., Dulnev K.V., Sevalneva T.G. Structure and properties of electrospark coating based on high-nitrogen structural steel // Proceedings of VIAM. 2025. No. 2 (144). Ст. 01. URL: https://www.viam-works.ru. DOI: 10.18577/2307-6046-2025-0-2-3-13.

Structure and properties of electrospark coating based on high-nitrogen structural steel

Sevalnev G.S., Oblivantsev K.D., Dulnev K.V., Sevalneva T.G.
Abstract

The structure, hardness and tribological characteristics of the electrospark coating based on high nitrogen structural steel of the Fe–C–Cr–Mn–Mo–Ni–V alloying system were studied. It was found that the maximum thickness of the coating based on steel is 34,5 μm. Samples with a single-layer coating of 18 μm thick have the best wear resistance. Application of the coating helps to increase the wear resistance of 30KhGSN2A steel by more than 3 times.

Keywords
high nitrogen steels, electrospark alloying, coating, hardness, microstructure, wear resistance
Reference list
  1. Kablov E.N. New generation materials and digital technologies for their processing. Vestnik Rossiyskoy akademii nauk, 2020, vol. 90, no. 4, pp. 331–334.
  2. Sevalnev G.S. Beryllium-containing steels – perspective material with a high level of physical and mechanical properties. Aviation materials and technologies, 2023, no. 3 (72), paper no. 02. Available at: http://www.journal.viam.ru (accessed: January 24, 2024). DOI: 10.18577/2713-0193-2023-0-3-15-29.
  3. Bogachev I.A., Sulyanova E.A., Sukhov D.I., Mazalov P.B. Microstructure and properties investigations of Fe–Cr–Ni stainless steel obtained by selective laser melting. Trudy VIAM, 2019, no. 3 (75), paper no. 01. Available at: http://www.viam-works.ru (accessed: July 31, 2024). DOI: 10.18577/2307-6046-2019-0-3-3-13.
  4. Voznesenskaya N.M., Tonysheva O.A., Eliseev E.A. Modern structural steels of cryogenic purpose and influence of some alloying elements on their properties (review). Trudy VIAM, 2020, no. 1, paper no. 01. Available at: http://www.viam-works.ru (accessed: July 31, 2024). DOI: 10.18577/2307-6046-2020-0-1-3-14.
  5. Bannykh I.O., Ashmarin A.A., Betzofen S.Ya. et al. Optimization of chemical composition and parameters of thermomechanical processing of TRIP steels based on new methods of X-ray tensiometry, texture and phase analysis. Metally, 2022, no. 6, pp. 66–72.
  6. Kaplanskii Yu.Yu., Mazalov P.B. World trends in the development of refractory high-entropy alloys for heat-loaded units of aerospace technics (review). Aviation materials and technologies, 2022, no. 2 (67), paper no. 03. Available at: http://www.journal.viam.ru (accessed: July 25, 2024). DOI: 10.18577/2713-0193-2022-0-2-30-42.
  7. Yeh J.-W., Chen Y.-L., Lin S.-J., Chen S.-K. High-entropy alloys – a new era of exploitation. Materials Science Forum, 2007, vol. 560, pp. 1–9. DOI: 10.4028/www.scientifi c.net/MSF.560.1.
  8. Cantor B., Chang I.T.H., Knight P., Vincent A.J.B. Microstructural development in equiatomic multicomponent alloys. Materials Science and Engineering: A, 2004, vol. 375–377, pp. 213–218. DOI: 10.1016/j.msea.2003.10.257.
  9. Cantor B. Multicomponent and high entropy alloys. Entropy, 2014, vol. 16, no. 9, pp. 4749–4768.
  10. Zakirova L.I., Laptev A.B. Properties of protective electroplating coatings for replacement of cadmium on steel fixing parts (review). Part 1. Morphology and corrosion resistance. Aviaсionnye materialy i tehnologii, 2020, no. 3 (60), pp. 37–46. DOI: 10.18577/2071-9140-2020-0-3-37-46.
  11. Laptev A.B., Zakirova L.I., Degovets M.L. Properties of protective galvanic coatings for replacement of cadmium on steel fixing parts (review). Part 2. Hydrogen embrittlement and frictional characteristics. Aviacionnye materialy i tehnologii, 2020, no. 4 (61), pp. 35–40. DOI: 10.18577/2071-9140-2020-0-4-35-40.
  12. Filonnikov A.L., Rinchinova S.V. Borating as a method of strengthening the working surfaces of technological equipment. Simvol nauki, 2019, no. 1, pp. 33–35.
  13. Baptista A., Silva F., Porteiro J. et al. Sputtering physical vapour deposition (PVD) coatings: A critical review on process improvement and market trend demands. Coatings. 2018, vol. 8, no. 11, p. 402.
  14. Holleck H., Schier V. Multilayer PVD coatings for wear protection. Surface and Coatings Technology, 1995, vol. 76, pp. 328–336.
  15. Rashev Ts.V. High-nitrogen became. Metallurgy under pressure. Sofia: Prof. Marin Drinov, 1995, 272 p.
  16. Sevalnev G.S., Gromov V.I., Dulnev K.V., Sevalneva T.G. Contact endurance of nitrogenous austenitic-martensitic steels with different hardening mechanism. Aviation materials and technologies, 2024, no. 2 (75), paper no. 01. Available at: http://www.journal.viam.ru (accessed: July 31, 2024). DOI: 10.18577/2713-0193-2024-0-2-3-14.
  17. Sevalnev G.S., Antsyferova M.V., Dulnev K.V., Sevalneva T.G., Vlasov I.I. Influence of nitrogen concentration on the structure and properties of sparingly alloyed structural steel. Aviacionnye materialy i tehnologii, 2020, no. 2 (59), pp. 10–16. DOI: 10.18577/2071-9140-2020-0-2-10-16.
  18. Antsyferova M.V., Bannykh I.O., Lukin E.I. et al. Structure and properties of high-strength low-alloy martensitic steels with super-equilibrium nitrogen content. Electrometallurgiya, 2023, no. 5, pp. 2–11. DOI: 10.31044/1684-5781-2023-0-5-2-11.
  19. Bakradze M.M., Voznesenskaya N.M., Leonov A.V. et al. Development and study of high-strength corrosion-resistant steel for bearing parts. Metallurg, 2019, no. 11, pp. 39–44.
  20. Leonov A.V., Voznesenskaya N.M., Tonysheva O.A. Influence of heat treatment parameters on the properties and microstructure of high-strength corrosion-resistant steel with super-equilibrium nitrogen content. Stal, 2022, no. 11, pp. 35–39.
  21. Gadalov V.N., Filonovich A.V., Shkatov V.V. et al. Description of the electric spark alloying process (generalized model). Izvestiya Yugo-Zapadnogo gosudarstvennogo universiteta, 2016, no. 4 (21), pp. 58–66.
  22. Verkhoturov A.D., Ivanov V.I., Dorokhov A.S., Konevtsov L.A. Influence of the nature of electrode materials on the erosion and properties of the alloyed layer. Criteria for assessing the effectiveness of electric spark alloying. Inzhenernye tekhnologii i sistemy, 2018, vol. 28, no. 3, pp. 302–320.
  23. Alymov M.I., Stolin A.M., Bazhin P.M. Study of the structure and properties of protective coatings obtained by the method of electric spark alloying with SHS electrodes (review). Zavodskaya laboratoriya. Diagnostika materialov, 2022, vol. 88, no. 2, pp. 40–48.