Barannikov A.A., Veshkin E.A, Shershak P.V., Galiullin An.R. Floor panels of the cabin and baggage and cargo compartment from polymer composite materials for modern domestic aircraft. Part 1. Diversity of requirements of domestic aircraft developers for cabin and baggage and cargo compartment floor panels from polymer composite materials // Proceedings of VIAM. 2025. No. 12. Ст. 03. URL: https://www.viam-works.ru. DOI: 10.18577/2307-6046-2025-0-12-25-36.

Floor panels of the cabin and baggage and cargo compartment from polymer composite materials for modern domestic aircraft

Part 1. Diversity of requirements of domestic aircraft developers for cabin and baggage and cargo compartment floor panels from polymer composite materials
Barannikov A.A., Veshkin E.A, Shershak P.V., Galiullin An.R.
Abstract

The article examines the differences in approaches of domestic aircraft developers to the formation of requirements for the design and production of cabin floor panels and baggage and cargo compartment made of polymer composite materials. The article examines the analysis of requirements for floor panels and baggage and cargo compartment of modern domestic aircraft: MS-21-300, SSJ-NEW, Il-114-300, Tu-214 and other models, taking into account world experience. The problems of unification of technical requirements and the possibility of using domestic developments in the design of various types of aircraft are considered.

Keywords
aircraft, polymer composite materials, carbon plastic, floor panels, cabin, baggage and cargo compartment
Reference list
  1. Samoilov I.A., Lesnichy I.V., Samoilov V.I., Kipcharsky D.A. Status and Development Prospects of the Russian Civil Aviation Fleet. Nauchnyy vestnik GosNII GA, 2014, no. 4 (315), pp. 9–16.
  2. Order of the Government of the Russian Federation of July 25, 2022 No. 1693-r «Comprehensive Program for the Development of the Air Transport Industry of the Russian Federation until 2030». Available at: http://government.ru/docs/all/141773/ (accessed: August 12, 2025).
  3. Veshkin E.A., Satdinov R.A., Barannikov A.A. Modern materials for the aircraft cabin. Trudy VIAM, 2021, no. 9 (103), pp. 33–42. Available at: http://www.viam-works.ru (accessed: August 26, 2025). DOI: 10.18577/2307-6046-2021-0-9-33-42.
  4. Shokin G.I., Shershak P.V., Andryunina M.A. Experience in the Development and Implementation of Production of Aircraft Honeycomb Floor Panels from Domestic Materials. Aviatsionnaya promyshlennost, 2017, no. 1, pp. 32–39.
  5. Barannikov A.A., Veshkin E.A., Postnov V.I., Strelnikov S.V. On the Production of PCM Floor Panels for Aircraft (review article). Izvestiya Samarskogo nauchnogo tsentra RAN, 2017, vol. 19, no. 4 (2), pp. 198–213.
  6. Feigenbaum Yu.M., Butushin S.V., Bozhevalov D.G., Sokolov Yu.S. Composite Materials and the History of Their Implementation in Aircraft Structures. Nauchnyy vestnik GosNII GA, 2015, no. 7 (318), pp. 24–37.
  7. Barbotko S.L., Kirillov V.N., Shurkova E.N. Fire safety evolution for polymer composites of aeronautical application. Aviacionnye materialy i tehnologii, 2012, no. 3, pp. 56–63.
  8. Dushin M.I., Ermolaev A.M., Katyrev I.Ya. et al. Carbon fiber-reinforced plastics in floor panels of three-layer construction. Aviatsionnaya promyshlennost, 1978, no. 6, pp. 8–12.
  9. Strelnikov S.V., Petukhov V.I., Postnov V.I., Shvets N.I. New solutions in the technology of manufacturing prepregs for interior panels. Izvestiya Samarskogo nauchnogo tsentra RAN, 2011, vol. 13, no. 4 (2), pp. 498–507.
  10. Komarov V.A., Kutsevich K.E., Pavlova S.A., Tyumeneva T.Yu. Optimization of Three-Layer Honeycomb Floor Panels Made of Low-Combustibility Polymer Composite Materials Based on High-Strength Carbon and Glass Fibers and an Adhesive Binder. Vestnik Samarskogo universiteta. Aerokosmicheskaya tekhnika, tekhnologii i mashinostroenie, 2020, no. 3, pp. 51–72.
  11. Komarov V.A., Pavlova S.A. Consideration of Stiffness Requirements in the Design of Three-Layer Aircraft Floor Panel Structures Made of High-Strength Composite Materials. Vestnik Samarskogo universiteta. Aerokosmicheskaya tekhnika, tekhnologii i mashinostroyenie, 2021, no. 2. pp. 45–52.
  12. Kablov E.N. Innovative developments of FSUE «VIAM» SSC of RF on realization of «Strategic directions of the development of materials and technologies of their processing for the period until 2030». Aviacionnye materialy i tehnologii, 2015, no. 1 (34), pp. 3–33. DOI: 10.18577/2071-9140-2015-0-1-3-33.
  13. Kan A.Ch., Zhelezina G.F., Kulagina G.S., Ayupov T.R. Fire safety of structural organic plastics reinforced with aramid fabrics. Aviation materials and technologies, 2022, no. 4 (69), pp. 51–60. Available at: http://www.journal.viam.ru (accessed: October 16, 2025). DOI: 10.18577/2713-0193-2022-0-4-51-60.
  14. Flitelam UNS2 Technical Data. Available at: https://www.yumpu.com/pt/document/view/52337885/aim-composites-ltd-flitelam-uns2-technical-data-lindberg-lund-as (accessed: September 04, 2025).
  15. Ilyushenkov S.F., Batizat D.V., Sereduta P.I. Development of three-layer honeycomb floor panels for passenger aircraft made of polymer composites. Polimernye materialy, 2025, no. 3 (310), pp. 14–21.
  16. Starkov A.I., Kutsevich K.E., Tyumeneva T.Yu., Petrova A.P. Low-combustibility adhesive prepregs designed for the manufacture of integral and three-layer honeycomb structures aircraft technology. Trudy VIAM, 2022, no. 5 (111), paper no. 04. Available at: http://www.viam-works.ru (accessed: October 16, 2025). DOI: 10.18577/2307-6046-2022-0-5-41-52.
  17. Sarychev I.A., Serkova E.A., Khmelnitsky V.V., Zastrogin O.B. Thermosetting binders for aircraft floor panel materials (review). Trudy VIAM, 2019, no. 7 (79), paper no. 03. Available at: http://www.viam-works.ru (accessed: September 04, 2025). DOI: 10.18577/2307-6046-2019-0-7-26-33.
  18. Product Data Sheets. Available at: https://www.thegillcorp.com/product/ (accessed: September 04, 2025).
  19. Order of the Government of the Russian Federation dated July 4, 2023 No. 1789-r «Comprehensive scientific and technical program for the full innovation cycle «New composite materials: design and production technologies». Available at: http://government.ru/docs/all/148638/ (accessed: October 16, 2025).
  20. Startsev V.O., Antipov V.V., Slavin A.V., Gorbovets M.A. Modern domestic polymer composite materials for aviation industry (review). Aviation materials and technologies, 2023, no. 2 (71), pp. 122–144. Available at: http://www.journal.viam.ru (accessed: October 16, 2025). DOI: 10.18577/2713-0193-2023-0-2-122-144.