Starkov A.I., Kutsevich K.E., Isaev A.Yu., Vakhrusheva Ja.A., Putilina P.M. Investigation of the properties of high-strength standard modulus carbon fiber produced in China // Proceedings of VIAM. 2025. No. 12. Ст. 10. URL: https://www.viam-works.ru. DOI: 10.18577/2307-6046-2025-0-12-115-125.

Investigation of the properties of high-strength standard modulus carbon fiber produced in China

Starkov A.I., Kutsevich K.E., Isaev A.Yu., Vakhrusheva Ja.A., Putilina P.M.
Abstract

The article presents the results of investigation of the following properties of fiber: geometric cross-sectional characteristics, crystal structure, mass fraction of the dressing, linear density and fiber density, geometric cross-sectional characteristics of microplastics, tensile strength, modulus of elasticity and elongation at break of the microplastics. For carbon fiber reinforced plastic (CFRP) the following properties were determined: ultimate strength and modulus of elasticity under tension and bending, compressive strength, in-plane and interlaminar shear strength, curved beam strength, transversal strength, residual compressive strength after impact, specific interlaminar fracture toughness under Mode I and Mode II loading conditions. At the same time the microstructures of carbon fiber plastics were studied.

Keywords
carbon fiber, carbon fiber reinforced plastic (CFRP), adhesive prepreg, characteristics of carbon fibers, characteristics of carbon
Reference list
  1. Malakhovsky S.S., Panafidnikova A.N., Kostromina N.V., Osipchik V.S. Carbon fiber reinforced plastics in the modern world: their properties and applications. Uspekhi v khimii i khimicheskoy tekhnologii, 2019, vol. XXXIII, no. 6, pp. 62–64.
  2. Petrova A.P., Malysheva G.V. Adhesives, adhesive binders, and adhesive prepregs: a textbook. Ed. by E.N. Kablov. Moscow: VIAM, 2017, 472 p.
  3. Isaev A.Yu., Rubtsova E.V., Kotova E.V., Sutyagin M.N. Research of properties of glues and glue binding, made with use of modern domestic component base. Trudy VIAM, 2021, no. 3 (97), paper no. 05. Available at: http://www.viam-works.ru (accessed: May 18, 2025). DOI: 10.18577/2307-6046-2021-0-3-58-67.
  4. Bolshakov V.A., Antyufeeva N.V. Evaluation of the curing process model of the adhesive binder in prepreg. Aviation materials and technologies, 2023, no. 4 (73), paper no. 07. Available at: http://www.journal.viam.ru (accessed: May 20, 2025). DOI: 10.18577/2713-0193-2023-0-4-66-77.
  5. Perov N.S. Design of polymeric materials on the molecular principles. II. The molecular mobility in the cross-linked complex systems. Aviacionnye materialy i tehnologii, 2017, no. 4 (49), pp. 30–36. DOI: 10.18577/2071-9140-2017-0-4-30-36.
  6. Starkov A.I., Kutsevich K.E., Tyumeneva T.Yu., Petrova A.P. Low-combustibility adhesive prepregs designed for the manufacture of integral and three-layer honeycomb structures aircraft technology. Trudy VIAM, 2022, no. 5 (111), paper no. 04. Available at: http://www.viam-works.ru (accessed: May 18, 2025). DOI: 10.18577/2307-6046-2022-0-5-41-52.
  7. Malysheva G.V., Grashchenkov D.V., Guzeva T.A. Evaluation of technological use efficiency of adhesives and glue prepregs in the manufacture of three-layer panels. Aviacionnye materialy i tehnologii, 2018, no. 4 (53), pp. 26–30. DOI: 10.18577/2071-9140-2018-0-4-26-30.
  8. Mishkin S.I. Application of carbon fiber plastics in constructions of pilotless devices (review). Trudy VIAM, 2022, no. 5 (111), paper no. 08. Available at: http://www.viam-works.ru (accessed: May 20, 2025). DOI: 10.18577/2307-6046-2022-0-5-87-95.
  9. Method for producing film adhesives and adhesive prepregs with a thermosetting polymer binder and a device for implementing it: pat. 2254172С1 Rus. Federation; appl. 31.05.04; publ. 20.06.05.
  10. Garcia F.G., Soares B.G., Pita V.J.R.R. et al. Mechanical properties of epoxy networks based on DGEBA and aliphatic amines. Journal of Applied Polymer Science, 2007, no. 3, pp. 2047–2055. DOI: 10.1002/app.24895.
  11. Brostow W., Goodman S.H., Wahrmund J. Handbook of Thermoset Plastics. 3rd ed. Plastics Design Library, 2014, pp. 191–252. DOI: 10.1016/978-1455731077.
  12. Zhao X., Huang Z., Song P. et al. Curing kinetics and mechanical properties of fast curing epoxy resins with isophorone diamine and N-(3 aminopropyl)-imidazole. Journal of Applied Polymer Science, 2019, vol. 136, pp. 1–10. DOI: 10.1002/APP.47950.
  13. Zhao X., Huang Z., Song P. et al. Curing kinetics and mechanical properties of epoxy resin /1-benzyl-2-methylimidazole / isophorone diamine system. Thermochimica Acta, 2020, vol. 690, p. 178657. DOI: 10.1016/j.tca.2020.178657.
  14. Aufray M. Physico-chemical characterization of epoxy-amine / metal interphases, characterization of their constituents: Dissertation PhD. L’Institut National das Sciences Appliques de Lyon, 2005, 186 p. Available at: https://www.researchgate.net/publication/281600273 (accessed: May 18, 2025).
  15. Sidorina A.I., Safronov A.M. Study of the resistance of carbon fibers to oxidation. Trudy VIAM, 2022, no. 7 (113), paper no. 06. Available at: http://www.viam-works.ru (accessed: May 20, 2025). DOI: 10.18577/2307-6046-2022-0-7-63-73.
  16. Varshavsky V.Ya. Carbon Fibers. Moscow: Varshavsky V.Ya., 2005, 496 p.
  17. Carbon Fibers and Carbon Composites. Ed. E. Fitzer. Moscow: Mir, 1988, 338 p.
  18. Tagawa M., Ohmae N., Umeno M. et al. Surface Characterization of Carbon Fibers Exposed to 5 eV Energetic Atomic Oxygen Beam Studied by Wetting Force Measurements. Japanese Journal of Applied Physics, 1991, vol. 30, pp. 2134–2138.