Guseva M.A. Practical use of the rheological method in determining the conditions of production control and curing modes in the development of polymer binders // Proceedings of VIAM. 2025. No. 12. Ст. 01. URL: https://www.viam-works.ru. DOI: 10.18577/2307-6046-2025-0-12-3-11.
Practical use of the rheological method in determining the conditions of production control and curing modes in the development of polymer binders
Abstract
At the development stage, the composition of a polymer binder from the rheological point of view is based on the choice of viscosity at different temperatures and the duration of exposure to temperature. The main methods to determine the viscosity value of a polymer binder are rheological testing methods, implemented using rheological equipment of various brands, and measuring systems of different configurations. The study shows practical use of rheological equipment of various brands in control analysis, possibilities of rotational and oscillatory rheometry for determining binder curing modes in prepregs.
Keywords
rheology, production control, curing, development, binding, polymeric composite materials
Reference list
- Mukhametov R.R., Petrova A.P. Thermosetting binders for polymer composite materials: textbook. Manual. Ed. E.N. Kablov. Moscow: NRC «Kurchatov Institute» – VIAM, 2021, 528 p.
- Severs E.T. Rheology of polymers. Moscow: Khimiya, 1966, 200 p.
- Schramm G. Fundamentals of practical rheology and rheometry. Moscow: KolosS, 2003, 312 p.
- Guseva M.A., Petrova A.P. Possibilities of rheology in the study of binders for PCM. Vse materialy. Entsiklopedicheskiy spravochnik, 2021, no. 7, pp. 38–45.
- Kablov E.N., Antipov V.V. The Role of New Generation Materials in Ensuring the Technological Sovereignty of the Russian Federation. Vestnik Rossiyskoy akademii nauk, 2023, vol. 93, no. 10, pp. 907–916.
- Kablov E.N., Laptev A.B., Prokopenko A.N., Gulyaev A.I. Relaxation of polymeric composite materials under the prolonged action of static load and climate (review). Part 1. Binders. Aviation materials and technologies, 2021, no. 4 (65), paper no. 08. Available at: http://www.journal.viam.ru (accessed: March 28, 2025). DOI: 10.18577/2713-0193-2021-0-4-70-80.
- Guseva M.A., Prokopova L.A., Khaskov M.A. Determination of melting temperatures of solid polymers by the rheological method. Zavodskaya laboratoriya. Diagnostika materialov, 2021, vol. 87, no. 7, pp. 38–43.
- Tkachyk A.I., Kyznecova P.A., Donetskiy K.I., Karavaev R.Yu. Some technological features of manufacturing polymer composite materials by non-autoclave molding of prepregs. Trudy VIAM, 2024, no. 12 (142), paper no. 04. Available at: http://www.viam-works.ru (accessed: March 28, 2025). DOI: 10.18577/2307-6046-2024-0-12-44-55.
- Galygin V.E., Baronin G.S., Tarov V.P., Zavrazhin D.O. Modern technologies for the production and processing of polymer and composite materials: textbook. Tambov: Publ. House of TSTU, 2012, 180 p.
- Kablov E.N., Kondrashov S.V., Melnikov A.A., Pavlenko S.A., Guseva M.A., Pykhtin A.A., Larionov S.A. Investigation of the influence of the thermal regime of FDM printing on the structuring and warping of polyethylene samples. Trudy VIAM, 2021, no. 7 (101), paper no. 06. Available at: http://www.viam-works.ru (accessed: March 28, 2025). DOI: 10.18577/2307-6046-2021-0-7-48-58.
- Morozova V.S., Ivanov М.S., Shestakov A.M., Pavlukovich N.G. The influence of the melt flow of polyetheretherketone on the characteristics of carbon fiber plastic based on it. Trudy VIAM, 2024, no. 1 (131), paper no. 05. Available at: http://www.viam-works.ru (accessed: March 28, 2025). DOI: 10.18577/2307-6046-2024-0-1-44-51.
- Kuznetcova P.A., Tkachuk A.I., Lyubimova A.S., Eldjaeva G.B. Characteristics of the molten epoxy resin system VSE-62, processed by the injection methods, for the manufacture of highly loaded structural polymer composite materials. Trudy VIAM, 2023, no. 5 (123), paper no. 04. Available at: http://www.viam-works.ru (accessed: March 28, 2025). DOI: 10.18577/2307-6046-2023-0-5-43-53.
- Guseva M.A., Ibragimov Z.D. Selection of curing system when developing epoxy compositions with energy-efficient curing mode. Trudy VIAM, 2024, no. 3 (133), paper no. 05. URL: http://www.viam-works.ru (accessed: March 28, 2025). DOI: 10.18577/2307-6046-2024-0-3-52-62.
- Guseva M.A. Application of Rheological Methods in the Development of Polymer Binders and Industrial Control. Reports of the XXXI Symposium on Rheology. Moscow: TIPS RAS, 2024, p. 87.
- Guseva M.A. Rheological Approach to the Development of Polymer Binders for Polymeric Composites. Reports of the VIII All-Rus. Sci. and Tech. Conf. «Polymer Composite Materials and New Generation Production Technologies». Moscow: NRC «Kurchatov Institute» – VIAM, 2024, p. 173.