Shosheva A.L., Kopnov A.Yu., Lavrin M.A., Mitroshina A.A. Synthesis and properties of thermosetting polyimide materials // Proceedings of VIAM. 2025. No. 10 (152). Ст. 06. URL: https://www.viam-works.ru. DOI: 10.18577/2307-6046-2025-0-10-68-83.

Synthesis and properties of thermosetting polyimide materials

Shosheva A.L., Kopnov A.Yu., Lavrin M.A., Mitroshina A.A.
Abstract

The paper presents a review of scientific and technical information on LaRC-series polyimide materials. The most significant physical and thermomechanical properties of heat-resistant polyimide polymer matrices are outlined, including thermal stability, mechanical strength, and resistance to aggressive environments. The main advantages of these polyimides are highlighted. The chemical compositions of LaRC-series polyimide materials and their structural formulas are described. Promising application areas for polyimide materials in the aerospace industry are discussed.

Keywords
PMR-15, thermosetting polyimide, polyimide resins, thermo-oxidative stability, polyimide films, polyimide foams
Reference list
  1. Davydova I.F., Kablov E.N., Kavun N.S. Heat-resistant non-flammable polyimide glass-fiber laminates for aviation and rocket technology products. Vse materialy. Entsiklopedicheskiy spravochnik, 2009, no. 7, pр. 2–11.
  2. Scola D. Polyimide Resins. ASM Handbook. ASM International, 2001, vol. 21: Composites, pp. 105–119.
  3. Mikhailin Yu.A. Technological and operational characteristics of polyimide binders, prepregs and imidoplastics of the PMR type (review). Plasticheskie massy, 1984, no. 3, pp. 17–23.
  4. Akhmadieva K.R., Petrova А.P., Shosheva A.L., Bokov V.V. Heat-resistant polyimide adhesive of constructive purposes. Trudy VIAM, 2023, no. 6 (124), paper no. 02. Available at: http://www.viam-works.ru (accessed: January 15, 2025). DOI: 10.18577/2307-6046-2023-0-6-15-24.
  5. Zharinov M.A., Shimkin A.A., Akhmadiyeva K.R., Zelenina I.V. Features and properties of solvent-free PMR-type polyimide resin. Trudy VIAM, 2018, no. 12 (72), paper no. 05. Available at: http://www.viam-works.ru (accessed: January 14, 2025). DOI: 10.18577/2307-6046-2018-0-12-46-53.
  6. Valueva M.I., Zelenina I.V., Nacharkina A.V., Sidorina A.I., Slavin A.V. High-temperature carbon fiber reinforced plastics based on polyimide binders. Trudy VIAM, 2024, no. 11 (141), paper no. 06. Available at: http://www.viam-works.ru (accessed: January 13, 2025). DOI: 10.18577/2307-6046-2024-0-11-71-88.
  7. Zelenina I.V., Valueva M.I., Nacharkina A.V., Kurshev E.V. Structure and properties of high-temperature carbon fiber reinforced plastic based on polyimide binder. Trudy VIAM, 2023, no. 3 (121), paper no. 02. Available at: http://www.viam-works.ru (accessed: January 17, 2025). DOI: 10.18577/2307-6046-2023-0-3-13-28.
  8. Pater R.H., Curto P.A. Advanced materials for space applications. Acta Astronautica, 2007, vol. 61, no. 11–12, pp. 1121–1129.
  9. Process for preparing a tough, soluble, aromatic, thermoplastic copolyimide: pat. US5639850A; appl. 18.05.95; publ. 17.06.97.
  10. Whitley K.S. Mechanical Properties of LaRC TM SI Polymer for a Range of Molecular Weights. NASA technical memorandum. Hampton, 2000, pp. 5–32.
  11. Tough, soluble, aromatic, thermoplastic copolyimides: pat. US5741883A; appl. 16.12.94; publ. 21.04.98.
  12. Holloway N.M., Barnes K.N., Draughon G.K., Scott L.A. Fabrication of adhesiveless lightweight flexible circuits using Langley Research Center soluble-imide «LaRC-SI» polyimide film. SPIE. San Diego, 2002, pp. 293–303.
  13. Sang Q. Preparation and etching of LaRC-SI polyimide film. Louisville: University of Louisville, 1999, p. 1073.
  14. Bryant R.G. Moving Technology from Test Tube to Commercial Product: А Case Study of Three Inventions. Recent Progress in Space Technology, 2014, vol. 4, no. 1, p. 38.
  15. Low Toxicity High Temperature PMR Polyimides: pat. US5171822A; appl. 05.02.91; publ. 15.12.92.
  16. Hou T.H., Wilkinson S.P., Johnston N.J. et al. Processing and properties of IM7/LARC-RP46 polyimde composites. 39th International SAMPE Symposium and Exhibition. Anaheim, California, 1994, pp. 1–14.
  17. Hutapea P., Yuan F. The effect of thermal aging on the Mode-I interlaminar fracture behavior of a high-temperature IM7/LaRC-RP46 composite. Composites science and technology, 1999, vol. 59, no. 8, pp. 1271–1286.
  18. Simone C.D., Xiao Y., Sun X., Scola D. Some aspects of the cure of RP-46, a nadic end-capped polyimide, and phenyl nadimide and bis-nadic-3,4'-ODA model compounds. High Performance Polymers, 2005, vol. 17, no. 1, pp. 51–72.
  19. Pater R.H. Polyimide Resins Resist Extreme Temperatures. Spinoff NASA Contribution. Virginia, 2009, p. 57.
  20. Heat, moisture, and chemical resistant polyimide compositions and methods for making and using them: pat. US6777525B2; appl. 01.04.02; publ. 17.08.04.
  21. Hawkins B.P., Hinkley J.A., Pater R.H., Moore J. Stretch-orientation of LaRC™ RP50 polyimide film. High Performance Polymers, 2006, vol. 18, no. 4, pp. 469–478.
  22. Imide oligomers endcapped with phenylethynyl phthalic anhydrides and polymers therefrom: pat. US5567800A; appl. 28.10.94; publ. 22.10.96.
  23. Phenylethynyl terminated imide oligomers: pat. US5412066A; appl. 03.04.94; publ. 02.05.95.
  24. Fang X., Scola D.A. Investigation of microwave energy to cure carbon fiber reinforced phenylethynyl‐terminated polyimide composites, PETI-5/IM7. Journal of Polymer Science. Part A: Polymer Chemistry, 1999, vol. 37, no. 24, pp. 4616–4628.
  25. Thompson C., Connell J., Hergenrother P. Adhesive and composite properties of a new phenylethynyl terminated imide. 47th International SAMPE Symposium and Exhibition. Hampton, 2002, pp. 1–13.
  26. Ghose S., Watson K.A., Cano R.J. et al. High temperature VARTM of phenylethynyl terminated imides. High Performance Polymers, 2009, vol. 21, no. 5, pp. 653–672.
  27. Cho D., Drzal L.T. Characterization, properties, and processing of LaRC PETI‐5 as a high‐temperature sizing material. II. Thermal characterization. Journal of Applied Polymer Science, 2000, vol. 75, no. 10, pp. 190–199.
  28. Gavrish A.V., Akhmadieva K.R., Shosheva A.L., Lavrin M.A. Thermosetting oligoimides with phenylethynyl reactive groups. Trudy VIAM, 2023, no. 9 (127), paper no. 04. Available at: http://www.viam-works.ru (accessed: January 22, 2025). DOI: 10.18577/2307-6046-2023-0-9-41-56.
  29. Cho D., Choi Y., Drzal L.T. Characterization, properties, and processing of LaRC PETI-5® as a high-temperature sizing material: III. Adhesion enhancement of carbon/BMI composites. The Journal of Adhesion, 2003, vol. 79, no. 1, pp. 1–22.
  30. Tenney D.R., Davis J.G., Pipes R.B., Johnston N. NASA Composite Materials Development: Lessons Learned and Future Challenges. Materials Science and Engineering: А, 2009, no. 1, pp. 25–26.
  31. Composition of and method for making high performance resins for infusion and transfer molding processes: pat. US6359107B1; appl. 18.05.00; publ. 19.03.02.
  32. Cano R.J., Ghose S., Watson K.A. et al. Processing and Properties of Vacuum Assisted Resin Transfer Molded Phenylethynyl Terminated Imide Composites. SAMPE. Baltimore, 2002, art. NF1676L-13433.
  33. Ghose S., Cano R.J., Britton S.M. et al. Phenylethynyl Terminated Imide (PETI) Composites Made by High Temperature VARTM. The 14th European conference on composite materials. Budapest, 2010, pp. 1–10.
  34. Williams M.K., Melendez O., Palou J. et al. Characterization of polyimide foams after exposure to extreme weathering conditions. Journal of adhesion science and technology, 2004, vol. 18, no. 5, pp. 561–573.
  35. Williams M.K., Nelson G.L., Brenner J.R. et al. High performance polyimide foams. ACS Symposium Series. Washington, DC: American Chemical Society, 2001, pp. 49–62.
  36. Aromatic polyimide foam: pat. US6133330A; appl. 21.05.99; publ. 17.10.00.
  37. Hou T.-H., Weiser E.S., Siochi E.J., St. Clair T.L. Processing characteristics of TEEK polyimide foam. High Performance Polymers, 2004, vol. 16, no. 4, pp. 487–504.
  38. Kuwabara A., Ozasa M., Shimokawa T. et al. Basic mechanical properties of balloon-type TEEK-L polyimide-foam and TEEK-L filled aramid-honeycomb core materials for sandwich structures. Advanced composite materials, 2005, vol. 14, no. 4, pp. 343–363.
  39. Williams M.K., Weiser E.S., Fesmire J.E. et al. Effects of cell structure and density on the properties of high performance polyimide foams. Polymers for Advanced Technologies, 2005, vol. 16, no. 2–3, pp. 167–174.
  40. Weiser E.S., Johnson T.F., St. Clair T.L. et al. Polyimide foams for aerospace vehicles. High Performance Polymers, 2000, vol. 12, no. 1, pp. 1–12.
  41. Kablov E.N., Bejder E.Ya., Petrova G.N., Stolyankov Yu.V., Rumyanceva T.V. Foamed polyimides. Trudy VIAM, 2015, no. 4, paper no. 09. Available at: http://www.viam-works.ru (accessed: January 22, 2025). DOI: 10.18577/2307-6046-2015-0-4-9-9.
  42. Structures from low dielectric polyimides: pat. US5338826A; appl. 28.09.92; publ. 16.08.94.
  43. Process for preparing essentially colorless polyimide film containing phenoxy-linked diamines: pat. US4595548A; appl. 23.08.84; publ. 17.06.86.
  44. Thompson C.M., Herring H.M., Gates T.S., Connell J.W. Preparation and characterization of metal oxide/polyimide nanocomposites. Composites science and technology, 2003, vol. 63, no. 11, pp. 1591–1598.
  45. Wooldridge E.M., Powers C.E. Evaluation of thin films for the Next-Generation Space Telescope (NGST) sunshield. Space Telescopes and Instruments. Kona, Hawaii, 1998, pp. 134–140.
  46. Woo B., Ertmer K.M., Coverstone V.L. et al. Deployment experiment for ultralarge solar sail system (ultrasail). Journal of Spacecraft and Rockets, 2011, vol. 48, no. 5, pp. 874–880.
  47. Reed K., Willenberg H.J. Early commercial demonstration of space solar power using ultra-lightweight arrays. Acta Astronautica, 2009, vol. 65, no. 9–10, pp. 1250–1260.
  48. Nazarenko V., St. Clair A., Klouda R. et al. Chemically imidized polyimide as an alignment material for liquid crystal displays. SID Symposium Digest of Technical Papers. Wiley, 1998, pp. 135–138.
  49. Dingemans T.J., van der Zwaag S., Knijnenberg A. et al. Novel liquid crystal thermoset resins for cryogenic fuel tank applications. The 24th International Congress of the Aeronautical Sciences. Yokohama, 2004, pp. 1–4.
  50. Pavlick M., Johnson W., Jensen B., Weiser E. Evaluation of mechanical properties of advanced polymers for composite cryotank applications. Composites. Part A: Applied Science and Manufacturing, 2009, vol. 40, no. 4, pp. 359–367.