Antipov V.V., Salimov I.E., Bespalov A.S., Babashov V.G. Study of the influence of the composition of the binder on the density, physica-mechanical and hydrophobic properties of heat-sound insulation material // Proceedings of VIAM. 2024. No. 9 (139). Ст. 03. URL: https://www.viam-works.ru. DOI: 10.18577/2307-6046-2024-0-9-25-32.

Study of the influence of the composition of the binder on the density, physica-mechanical and hydrophobic properties of heat-sound insulation material

Antipov V.V., Salimov I.E., Bespalov A.S., Babashov V.G.
Abstract

The influence of the composition of the binder component on the physica-mechanical properties of a flexible low-density heat-sound insulation fibrous material has been studied. The density, flexibility, elasticity, tensile strength, moisture, sorption moisture of experimental samples of flexible low-density heat-sound insulation fibrous materials has been studied. It is determined that experimental samples of flexible, low-density heat-sound insulation fibrous materials are not inferior in terms of properties to native and foreign analogues.

Keywords
fibrous heat-sound insulation material, density, elasticity, flexibility, moisture absorption, hydrophobicity
Reference list
  1. Kablov E.N. Innovative developments of FSUE «VIAM» SSC of RF on realization of «Strategic directions of the development of materials and technologies of their processing for the period until 2030». Aviacionnye materialy i tehnologii, 2015, no. 1 (34), pp. 3–33. DOI: 10.18577/2071-9140-2015-0-1-3-33.
  2. Kablov E.N., Grashchenkov D.V., Isaeva N.V., Solntsev S.S., Sevastyanov V.G. Glass and Ceramics Based High-Temperature Composite Materials for use in Aviation Technology. Glass and Ceramics, 2012, vol. 69, no. 3–4, pp. 109–112.
  3. Kablov E.N., Shuldeshov E.M., Petrova A.P., Lapteva M.A., Sorokin A.E. Dependence of complex of sound-proof VZMK type material properties on concentration of hydrophobizing composition on the basis of organosilicon sealant. Aviacionnye materialy i tehnologii, 2020, no. 2 (59), pp. 41–49. DOI: 10.18577/2071-9140-2020-0-2-41-49.
  4. Barinov D.Ya., Marakhovskij P.S., Zuev A.V. Mathematical modeling of destruction of fiberglass-based thermal-protection material. Aviacionnye materialy i tehnologii, 2020, no. 4 (61), pp. 71–78. DOI: 10.18577/2071-9140-2020-0-4-71-78.
  5. Zuev A.V., Zarichnyak Yu.P., Barinov D.Ya., Krasnov L.L. Measurement of thermophysical properties of flexible thermal insulation. Aviation materials and technology, 2021, no. 1 (62), paper no. 11. Available at: http://www.journal.viam.ru (accessed: July 22, 2024). DOI: 10.18577/2713-0193-2021-0-1-119-126.
  6. Osnos S.P. Application of materials based on basalt fibers in the aerospace industry. Kompozitnyj mir, 2015, no. 4 (61), pp. 72–79.
  7. Babashov V.G., Bespalov A.S., Istomin A.V., Varrik N.M. Heat and sound insulating material made using plant raw materials. Novye ogneupory, 2017, no. 3, pp. 173–178.
  8. Kablov E.N. Materials for «Buran» spaceship – innovative solutions of formation of the sixth technological mode. Aviacionnye materialy i tehnologii, 2013, no. S1, pp. 3–9.
  9. Boynovich L.B., Domantovsky A.G., Emelyanenko A.M. et al. Anti-icing properties of superhydrophobic coatings on aluminum and stainless steel. Izvestiya Akademii nauk. Ser.: Khimicheskaya, 2013, no. 2, pp. 383–390.
  10. Kondrashov E.K., Nefedov N.I., Vereninova N.P. et al. Modification of fluorocopolymer coatings by telomers to improve their hydrophobicity. Polymer Science. Ser.: D, 2016, vol. 9, no. 2, pp. 212–218.
  11. Nefedov N.I., Haskov M.A., Petrova A.P., Buznik V.M. Study of the thermal properties of fluorinated paraffins and hydrophobic coatings on their base. Trudy VIAM, 2017, no. 2 (50), paper no. 11. Available at: http:// www.viam-works.ru (accessed: July 23, 2024). DOI: 10.18577/2307-6046-2017-0-2-11-11.
  12. Orlov A.V., Chursova L.V., Grebeneva T.A., Panina N.N. Flame retardants for creating flame retardant and fireproof polymer composite materials. Klei. Germetiki. Tekhnologii, 2022, no. 1, pp. 23–30. DOI: 10.31044/1813-7008-2022-0-1-23-30.
  13. Kan A.Ch., Zhelezina G.F., Kulagina G.S., Ayupov T.R. Fire safety of structural organic plastics reinforced with aramid fabrics. Aviation materials and technologies, 2022, no. 4 (69), paper no. 05. Available at: http://www.journal.viam.ru (accessed: July 23, 2024). DOI: 10.18577/2713-0193-2022-0-4-51-60.
  14. Istomin A.V. Technology of obtaining flexible thermal insulation materials. Steklo i keramika, 2023, vol. 96, no. 3 (1143), pp. 48–56. DOI: 10.14489/glc.2023.03.pp.048-056.
  15. Salimov I.E., Bespalov A.S., Babashov V.G., Maksimov V.G. Investigation of the influence of the chemical composition of Fenotam N210, Fenotam N210M, KMF-S, SFZh-3024 resins on their physico-chemical properties. Trudy VIAM, 2024, no. 2 (132), paper no. 09. Available at: http://www.viam-works.ru (accessed: July 23, 2024). DOI: 10.18577/2307-6046-2024-0-2-84-91.