Lukina N.F., Isaev A.Yu., Smirnov O.I., Salando R.P. Properties of VK-106 adhesive for fastening of heat-shrinkable tubes in the design of electric plaits // Proceedings of VIAM. 2024. No. 8 (138). Ст. 03. URL: https://www.viam-works.ru. DOI: 10.18577/2307-6046-2024-0-8-28-37.
Properties of VK-106 adhesive for fastening of heat-shrinkable tubes in the design of electric plaits
Abstract
Results of research of the properties of VK-106 epoxy thixotropic adhesive intended for connection of products from heat-shrinkable materials with the shells of electric plaits and the bodies of electric connectors at melting point temperature with the subsequent curing of adhesive joint at room temperature are presented. The data on keeping of strength characteristics of the adhesive joints executed with use of VK-106 adhesive, after influence of external factors in comparison with the initial characteristics are provided.
Keywords
epoxy adhesive of cold curing, thixotropy, heat-shrinkable tubes, electric plaits, adhesive joints, shear strength, maintainability
Reference list
- TE Connectivity. Available at: https://www.te.com/usa-en/product-657863-000html (accessed: March 21, 2024).
- Kablov E.N. Main directions of development of materials for aerospace engineering of the 21st century. Perspektivnye materialy, 2000, no. 3, pp. 27–36.
- Kablov E.N. New generation materials and digital technologies for their processing. Vestnik Rossiyskoy akademii nauk, 2020, vol. 90, no. 4, pp. 331–334.
- Kablov E.N. The role of fundamental research in creating new generation materials. Reports of the XXI Mendeleev Congress on General and Applied Chemistry: in 6 vols. St. Petersburg, 2019, vol. 4, p. 24.
- Kablov E.N., Laptev A.B., Prokopenko A.N., Gulyaev A.I. Relaxation of polymeric composite materials under the prolonged action of static load and climate (review). Part 1. Binders. Aviation materials and technologies, 2021, no. 4 (65), paper no. 08. Available at: http://www.journal.viam.ru (accessed: March 21, 2024). DOI: 10.18577/2713-0193-2021-0-4-70-80.
- Grashhenkov D.V., Chursova L.V. Strategy of development of composite and functional materials. Aviacionnye materialy i tehnologii, 2012, no. S, pp. 231–242.
- Antipov V.V., Serebrennikova N.Yu., Konovalov A.N., Nefedova Yu.N. Perspectives of application of fiber metal laminate materials based on aluminum alloys in aircraft design. Aviacionnye materialy i tehnologii, 2020, no. 1 (58), pp. 45–53. DOI: 10.18577/2071-9140-2020-0-1-45-53.
- Aviation materials: a reference book in 13 vols. Ed. E.N. Kablov. 7th ed., add. and rev. Moscow: VIAM, 2019, vol. 10: Adhesives, sealants, rubbers, hydraulic fluids, part 1: Adhesives, adhesive prepregs, 276 p.
- Petrova A.P., Malysheva G.V. Adhesives, adhesive binders and adhesive prepregs: a textbook. Ed. E.N. Kablov. Moscow: VIAM, 2017, 472 p.
- Petrova A.P., Donskoy A.A. Adhesives. Sealants. St. Petersburg: Professional, 2008, 589 p.
- Muhametov R.R., Ahmadieva K.R., Chursova L.V., Kogan D.I. New polymeric binding for perspective methods of manufacturing of constructional fibrous PCM. Aviacionnye materialy i tekhnologii, 2011, no. 2, pp. 38–42.
- Petrova A.P. Foaming adhesives and their application in aircraft manufacturing. Klei. Germetiki. Tekhnologii, 2015, no. 1, pp. 2–5
- Isaev A.Yu., Pavlyuk B.Ph., Petrova A.P., Lukina N.Ph., Balabanova O.S. Effect of modification of cold cured epoxy adhesives with elastomers on the resource strength of adhesive joint. Trudy VIAM, 2020, no. 9 (91), paper no. 03. Available at: http://www.viam-works.ru (accessed: March 21, 2024). DOI: 10.18577/2307-6046-2020-0-9-27-34.
- Malysheva G.V., Grashchenkov D.V., Guzeva T.A. Evaluation of technological use efficiency of adhesives and glue prepregs in the manufacture of three-layer panels. Aviacionnye materialy i tehnologii, 2018, no. 4 (53), pp. 26–30. DOI: 10.18577/2071-9140-2018-0-4-26-30.
- Kablov E.N., Minakov V.T., Anikhovskaya L.I. Adhesives and materials based on them for repair of aircraft structures. Aviatsionnye materialy i tekhnologii, 2002, no. 1, pp. 61–65.
- Shershak P.V., Yakovlev N.O., Shokin G.I., Kutsevich K.E., Popkova E.A. Evaluation method and factors influencing the bonding quality between face and honey-comb cores in floor and interior aircraft panels. Aviacionnye materialy i tehnologii, 2020, no. 2 (59), pp. 81–88. DOI: 10.18577/2071-9140-2020-0-2-81-88.
- Dementyeva L.A., Tyumeneva T.Yu., Sharova I.A. Low-flammability adhesives for aviation equipment. VI Int. Conf. «Low-flammability polymeric materials». Vologda, 2011, pp. 102–104.
- Zastrogina O.B., Shvets N.I., Serkova U.A., Veshkin E.A. Fire-safe materials based on phenol-formaldehyde binders. Klei. Germetiki. Tekhnologii, 2017, no. 7, pp. 22–27.
- Akhmadieva K.R., Petrova А.P., Shosheva A.L., Bokov V.V. Heat-resistant polyimide adhesive of constructive purposes. Trudy VIAM, 2023, no. 6 (124), paper no. 02. Available at: http://www.viam-works.ru (accessed: February 21, 2024). DOI: 10.18577/2307-6046-2023-0-6-15-24.
- Kutsevich K.E., Tyumeneva T.Yu., Petrova A.P. Influence of fillers on properties of adhesive prepregs and PCM on their basis. Aviacionnye materialy i tehnologii, 2017, no. 4 (49), pp. 51–55.
- Zastrogina O.B., Serkova E.А., Sarychev I.A., Vavilova M.I. Influence of Russian and Chinese vinyflex on the properties of the VFT binder and fiberglass based on it. Aviacionnye materialy i tehnologii, 2020, no. 3 (60), pp. 3–9. DOI: 10.18577/2071-9140-2020-0-3-3-9.
- Anikhovskaya L.I., Minakov V.T. Adhesives and adhesive prepregs for advanced aerospace products. Aviation materials. Selected works of VIAM 1932–2002. Moscow: MISIS; VIAM, 2002, pp. 315–325.
- Donskoy A.A., Baritko N.V. Low-density self-extinguishing sealants. Klei. Germetiki. Tekhnologii, 2006, no. 9, pp. 10–12.
- Batizat V.P., Anikhovskaya L.I., Dementyeva L.A. Adhesives for bonding metal and composite structures. Aviatsionnaya promyshlennost, 1983, no. 11, pp. 15–17.
- Batizat V.P., Anikhovskaya L.I., Vlasova V.I. et al. Features of the application of high-strength structural adhesives. Aviation materials. Moscow: VIAM, 1982, pp. 207–211.
- Sytyj Yu.V., Sagomonova V.A., Kislyakova V.I., Bolshakov V.A. New vibro absorbing materials. Aviacionnye materialy i tehnologii, 2012, no. 2, pp. 51–54.
- Petrova A.P. Main stages of gluing technology. Klei. Germetiki. Tekhnologii, 2014, no. 2, pp. 24–30.
- Fridlyander I.N., Anikhovskaya L.I., Senatorova O.G., Sidelnikov V.V., Dementyeva L.A. Composite adhesive and layered metal-polymer composites. Mechanical Engineering: Encyclopedia in 40 vols. Moscow: Mashinostroenie, 2001, vol: II-3: Non-ferrous metals and alloys. Сomposite metallic materials. Eds. I.N. Fridlyander, E.N. Kablov, pp. 814–831.
- Karimova S.A., Pavlovskaya T.G., Petrova A.P. Surface preparation of aluminum alloys using anodic oxidation. Klei. Germetiki. Tekhnologii, 2014, no. 1, pp. 34–38.
- Kochergin Yu.S., Grigorenko T.I., Kulik T.A. Properties of epoxy adhesives modified with oligosulfones. Klei. Germetiki. Tekhnologii, 2005, no. 11, pp. 3–7.
- Kurshubadze I.V., Petrova A.P. Performance of adhesive joints in marine subtropical conditions. Klei. Germetiki. Tekhnologii, 2005, no. 12, pp. 14–17.
- Petrova A.P., Dementyeva L.A., Kutsevich K.E., Buznik V.M. On the possibility of using materials based on adhesive prepregs in Arctic conditions. Klei. Germetiki. Tekhnologii, 2015, no. 2, pp. 12–16.
- Shvedkova A.K., Petrova A.P., Buznik V.M. Climatic resistance of composite materials based on adhesive prepregs in continental arctic conditions. Klei. Germetiki. Tekhnologii, 2016, no. 1, pp. 19–25.
- Petrova A.P., Lukina N.F., Isaev A.Yu., Smirnov O.I. The effect of the adhesive primer EP-0234 on the properties of adhesive compounds obtained using adhesive VK-36. Trudy VIAM, 2022, no. 6 (112), paper no. 04. Available at: http://www.viam-works.ru (accessed: June 28, 2024). DOI: 10.18577/2307-6046-2022-0-6-39-48.