Zhelezina G.F., Kulagina G.S., Kan A.Ch., Startsev V.O. Research of the climate stability of hybrid layered metal polymer materials based on aluminium and aramid organoplastics // Proceedings of VIAM. 2024. No. 7 (137). Ст. 04. URL: https://www.viam-works.ru. DOI: 10.18577/2307-6046-2024-0-7-34-44.

Research of the climate stability of hybrid layered metal polymer materials based on aluminium and aramid organoplastics

Zhelezina G.F., Kulagina G.S., Kan A.Ch., Startsev V.O.
Abstract

Climatic stability of hybrid layered metal polymer materials of the «aluminum–organoplastics» class in different climatic and laboratory conditions (warm humid climate, sea climate, salt spray chamber, etc.) is investigated. It is established that properties of materials Alor D16/41 (sheet) and Alor D16/41H (sheet) exposed in warm humid climate does not show reducing the elastic-strength properties of the samples. When exposed to narrow samples with a width of 10 mm with unprotected ends the level of preservation of tensile strength is 82–94 % from the initial value.

Keywords
layered metal polymer composite material, alloys, aramid organoplastics, climate stability, moisture absorption
Reference list
  1. Kablov E.N. Aviation materials science in the 21st century. Prospects and objectives. Aviation materials. Selected works of VIAM 1932–2002. Moscow: MISIS; VIAM, 2002, pp. 23–47.
  2. Kablov E.N., Startsev O.V. The basic and applied research in the field of corrosion and ageing of materials in natural environments (review). Aviacionnye materialy i tehnologii, 2015, no. 4 (37), pp. 38–52. DOI: 10.18577/2071-9140-2015-0-4-38-52.
  3. Mashinskaya G.P., Zhelezina G.F., Senatorova O.G. Laminated Fibrous Metal – Polymer Composites. Metal Matrix Composites. Soviet Advanced Composites Technology Series. Eds. J.N. Fridleander, I.H. Marshall. 1995, vol. 3, pp. 487–570.
  4. Kablov E.N., Antipov V.V., Girsh R.I., Serebrennikova N.Y., Konovalov A.N. Fiber Metal Laminates Based on Aluminum–Lithium Alloy Sheets in New-generation Aircraft. Russian Engineering Research, 2021, vol. 41, no. 3, pp. 215–221.
  5. Antipov V.V., Serebrennikova N.Yu., Shestov V.V., Sidelnikov V.V. Laminated hybrid materials on basis of Al–Li alloy sheets. Aviacionnye materialy i tehnologii, 2017, no. S, pp. 212–224. DOI: 10.18577/2071-9140-2017-0-S-212-224.
  6. Podzhivotov N.Y., Kablov E.N., Antipov V.V. et al. Laminated Metal-Polymeric Materials in Structural Elements of Aircraft. Inorganic Materials: Applied Research, 2017, vol. 8, no. 2, pp. 211–221.
  7. Antipov V.V., Serebrennikova N.Yu., Konovalov A.N., Nefedova Yu.N. Perspectives of application of fiber metal laminate materials based on aluminum alloys in aircraft design. Aviacionnye materialy i tehnologii, 2020, no. 1 (58), pp. 45–53. DOI: 10.18577/2071-9140-2020-0-1-45-53.
  8. Zhelezina G.F., Kolobkov A.S., Kulagina G.S., Kan A.Ch. Damping properties of hybrid layered metal-polymer materials based on aluminum, titanium alloys and organoplastics layers. Trudy VIAM, 2021, no. 2 (96), paper no. 02. Available at: http://www.viam-works.ru (accessed: November 23, 2023). DOI: 10.18577/2307-6046-2021-0-2-10-19.
  9. Yakovlev A.L., Nochovnaya N.A., Putyrskij S.V., Krohina V.A. Titanium-polymer laminated materials. Aviacionnye materialy i tehnologii, 2016, no. S2, pp. 56–62. DOI: 10.18577/2071-9140-2016-0-S2-56-62.
  10. Mashinskaya G.P., Zhelezina G.F. Alor. Great Russian Encyclopedia. Moscow: Great Russian Encyclopedia, 2015, p. 518.
  11. Startsev O.V., Krotov A.S., Senatorova O.G., Anikhovskaya L.I., Antipov V.V., Grashchenkov D.V. Sorption and diffusion of moisture in layered metal-polymer composite materials of the «SIAL» type. Materialovedenie, 2011, no. 12, pp. 38–44.
  12. Duyunova V.A., Kutyrev A.E., Serebrennikova N.Yu., Vdovin A.I., Somov A.V. Examination of the impact of aggressive environmental factors on the development of corrosion damage on samples of laminated glass-reinforced plastic of SIAL class. Aviation materials and technologies, 2021, no. 4 (65), paper no. 09. Available at: http://www.journal.viam.ru (accessed: December 08, 2023). DOI: 10.18577/2713-0193-2021-0-4-81-90.
  13. Antipov V.V., Kurs M.G., Girsh R.I., Serebrennikova N.Yu. Climatic field tests of SIAL type metal-polymer composition materials in marine climate. Aviacionnye materialy i tehnologii, 2019, no. 4 (57), pp. 56–64. DOI: 10.18577/2071-9140-2019-0-4-56-64.
  14. Voitovich V.A. Methods for preparing the surface of products made of metals and alloys. Klei. Germetiki. Tekhnologii, 2005, no. 9, pp. 19–23.
  15. Duyunova V.A., Kozlov I.A., Oglodkov M.S., Kozlova A.A. Modern trends in the anodic oxidation of aluminum-lithium and aluminum alloys (review). Trudy VIAM, 2019, no. 8 (80), paper no. 09. Available at: http://www.viam-works.ru (accessed: November 23, 2023). DOI: 10.18577/2307-6046-2019-0-8-79-89.
  16. Kablov E.N., Startsev O.V., Krotov A.S., Kirillov V.N. Climatic aging of composite materials for aviation purposes. I. Aging mechanisms. Deformatsiya i razrusheniye materialov, 2010, no. 11, pp. 19–27.
  17. Kablov E.N., Startsev O.V., Krotov A.S., Kirillov V.N. Climatic aging of composite materials for aviation purposes. III. Significant aging factors. Deformatsiya i razrusheniye materialov, 2011, no. 1. pp. 34–40.
  18. Gladkikh A.V., Kurs I.S., Kurs M.G. Analysis of the data of full-scale climatic tests combined with the application of operational factors of nonmetallic materials (review). Trudy VIAM, 2018, no. 10 (70), paper no. 09. Available at: http://www.viam-works.ru (accessed: November 21, 2023). DOI: 10.18577/2307-6046-2018-0-10-74-82.
  19. Duyunova V.A., Serebrennikova N.Yu., Nefedova Yu.N., Sidelnikov V.V., Somov A.V. Methods of forming metal-polymer composite materials (review). Aviation materials and technologies, 2022, no. 1 (66), paper no. 06. Available at: http://www.journal.viam.ru (ассеssed: September 18, 2023). DOI: 10.18577/2713-0193-2022-0-1-65-77.
  20. Antipov V.V., Chesnokov D.V., Kozlov I.A., Volkov I.A., Petrova A.P. Surface preparation aluminum alloy V-1469 before use in the composition of layered hybrid material. Trudy VIAM, 2018, no. 4 (64), paper no. 07. Available at: http://www.viam-works.ru (accessed: November 23, 2023). DOI: 10.18577/2307-6046-2018-0-4-59-65.
  21. Nefedov N.I., Semenova L.V., Kuznecova V.A., Vereninova N.P. Paint coatings for protection of metallic and polymer composite materials against aging, corrosion and biodeterioration. Aviacionnye materialy i tehnologii, 2017, no. S, pp. 393–404. DOI: 10.18577/2071-9140-2017-0-S-393-404.
  22. Kuznetsova V.A., Semenova L.V., Shapovalov G.G. Development trends in the field of anticorrosive polymeric systems for corrosion protection of fixing connections of contact couples of combined structures (review). Aviacionnye materialy i tehnologii, 2017, no. 1 (46), pp. 25–31. DOI: 10.18577/2071-9140-2017-0-1-25-31.
  23. Kablov E.N., Startsev O.V., Medvedev I.M. Review of international experience on corrosion and corrosion protection. Aviacionnye materialy i tehnologii, 2015, no. 2 (35), pp. 76–87. DOI: 10.18577/2071-9140-2015-0-2-76-87.