Donetskiy K.I., Ablyaz T.R., Shlykov E.S., Osinnikov I.V., Blokhin V.B., Muratov K.R. Study of the influence of the electrical discharge machining process on the structure of polymer composite material VKU-29 // Proceedings of VIAM. 2024. No. 6 (136). Ст. 05. URL: https://www.viam-works.ru. DOI: 10.18577/2307-6046-2024-0-6-51-60.

Study of the influence of the electrical discharge machining process on the structure of polymer composite material VKU-29

Donetskiy K.I., Ablyaz T.R., Shlykov E.S., Osinnikov I.V., Blokhin V.B., Muratov K.R.
Abstract

Processing of polymer composite materials with minimal defect formation is an important prerequisite for their long-term operation. Materials produced by the technology of copy-piercing electrical discharge machining (EDM) under consideration are also characterized by characteristic defects. The influence of the EDM modes, the applied conductive layer and  the electrode-tool material on the structure of the surface layer of structural carbon fiber reinforced plastic VKU-29 was studied. Technological parameters of EDM were obtained, ensuring the quality and efficiency of polymer composite materials, taking into account the minimal number of structural defects.

Keywords
carbon fiber polymer, copy-piercing electrical discharge machining, electrode-tool, processing modes, structural defects
Reference list
  1. Sarde B., Patil Y.D. Recent Research Status on Polymer Composite Used in Concrete-An Overview. Materials Today: Proceedings, 2019, vol. 18, pp. 3780–3790.
  2. Kablov E.N. New Generation Materials and Technologies for Their Digital Processing. Herald of the Russian Academy of Sciences, 2020, vol. 90, no. 2, pp. 225–228.
  3. Onishchenko G.G., Kablov E.N., Ivanov V.V. Scientific and technological development of Russia in the context of achieving national goals: problems and solutions. Innovatsii, 2020, no. 6 (260), pp. 3–16.
  4. Kablov E.N. The role of fundamental research in the creation of materials of the new generation. XXI Mendeleevsky Congress for General and Applied Chemistry: in 6 vols. St. Petersburg, 2019, vol. 4, p. 24.
  5. Kondrashov S.V., Shashkeev K.A., Petrova G.N., Mekalina I.V. Constructional polymer composites with functional properties. Aviacionnye materialy i tehnologii, 2017, no. S, pp. 405–419. DOI: 10.18577/2071-9140-2017-0-S-405-419.
  6. Bataev A.A., Bataev V.A. Compositional materials: structure, receipt, application: textbook. Novosibirsk: NSTU, 2002, 384 p.
  7. Kerber M.L., Vinogradov V.M., Golovkin G.S. et al. Polymer composite materials: structure, properties, technology: textbook. St. Petersburg: Profession, 2008, 560 p.
  8. Ablyaz T.R., Donetskiy K.I., Shlykov E.S., Muratov K.R., Dyushenko V.S., Minibaev M.I. A comprehensive analysis of the methods of processing polymer composite materials. STIN, 2022, no. 6, рр. 5–8.
  9. Tkachuk A.I., Donetsky K.I., Terekhov I.V., Karavaev R.Yu. The use of thermosetting matrices for the manufacture of polymer composite materials by the non-autoclave molding methods. Aviation materials and technology, 2021, no. 1 (62), paper no. 03. Available at: https:// www.journal.viam.ru (accessed: April 02, 2024). DOI: 10.18577/2713-0193-2021-0-1-22-33.
  10. Sidorina A.I. Multiaxial carbon fabrics in the products of aviation technology (review). Aviation materials and technologies, 2021, no. 3 (64), paper no. 10. Available at: http://www.journal.viam.ru (accessed: April 02, 2024). DOI: 10.18577/2713-0193-2021-0-3-105-116.
  11. Mukhametov R.R., Petrova A.P. Thermosetting binders for polymer composites (review). Aviacionnye materialy i tehnologii, 2019, no. 3 (56), pp. 48–58. DOI: 10.18577/2071-9140-2019-0-3-48-58.
  12. Startsev V.O., Antipov V.V., Slavin A.V., Gorbovets M.A. Modern domestic polymer composite materials for aviation industry (review). Aviation materials and technologies, 2023, no. 2 (71), paper no. 10. Available at: http://www.journal.viam.ru (accessed: March 08, 2024). DOI: 10.18577/2713-0193-2023-0-2-122-144.
  13. Baurova N.I., Zorin V.A. The use of polymer composite materials in the production and repair of machines: textbook. Moscow: MADI, 2016, 264 p.
  14. Raskutin A.E. Development strategy of polymer composite materials. Aviacionnye materialy i tehnologii, 2017, no. S, pp. 344–348. DOI: 10.18577/2071-9140-2017-0-S-344-348.
  15. Dyshenko V.S., Donetskiy K.I., Minibaev M.I., Ablyaz T.R., Shlykov E.S., Shiryaev V.V. Methods of mechanical and electrical discharge machining of polymer composite materials (review). Trudy VIAM, 2018, no. 3 (109), paper no. 10. Available at: http://www.viam-works.ru (accessed: March 05, 2024). DOI: 10.18577/2307-6046-2022-0-3-102-120.
  16. Film B.P. Mechanical processing of plastic: reference. Moscow: Mashinostroyenie, 1987, 152 p.
  17. Fukuzawa Y., Katougi H., Mohri N. et al. Machining properties of ceramics with an electric discharge machine. Proceedings of the XII ISEM. Dusseldorf: VDI Verlag, 1998, pp. 445–454.
  18. Mohri N., Fukuzawa Y., Tani T. et al. Assisting electrode method for machining insulating ceramics. Annals CIRP, 1996, no. 45 (1), pp. 201–204.
  19. Mohri N., Fukusima Y., Fukuzawa Y. et al. Layer generation process on work-piece in electrical discharge machining. Annals CIRP, 2003, no. 52 (1), pp. 161–164.
  20. Gunyaeva A.G., Sidorina A.I., Kurnosov A.O., Klimenko O.N. Polymeric composite materials of new generation on the basis of binder VSE-1212 and the filling agents alternative to ones of Porcher Ind. and Toho Tenax. Aviacionnye materialy i tehnologii, 2018, no. 3 (52), pp. 18–26. DOI: 10.18577/2071-9140-2018-0-3-18-26.