Prokopova L.A., Golovina E.Yu., Ponomarenko S.A. Methods for determining the mass fraction of hexamine in the catalyst FU // Proceedings of VIAM. 2024. No. 5 (135). Ст. 08. URL: https://www.viam-works.ru. DOI: 10.18577/2307-6046-2024-0-5-83-90.

Methods for determining the mass fraction of hexamine in the catalyst FU

Prokopova L.A., Golovina E.Yu., Ponomarenko S.A.
Abstract

The paper presents a comparative study of methods for determining the mass fraction of hexamine in samples of the «catalyst FU» using manual and instrumental approaches. The work describes the principles and stages of each method and analyzes their advantages and disadvantages. Statistics of the results of determining the composition of the product by three methods are presented. Based on the results obtained, a method for determining the mass fraction of urotropin has been proposed, which makes it possible to increase the accuracy and efficiency of the analysis.

Keywords
analytical chemistry, quantitative analysis, determination of nitrogen content, Kjeldahl method, elemental analysis, elemental analyzer, high pressure liquid chromatography
Reference list
  1. Kablov E.N., Semenova L.V., Petrova G.N., Larionov S.A., Perfilova D.N. Polymer composite materials on a thermoplastic matrix. Izvestiya vuzov. Khimiya i khimicheskaya tekhnologiya, 2016, vol. 59, is. 10, pp. 61–71.
  2. Kablov E.N. The role of chemistry in the creation of new generation materials for complex technical systems. Report XX Mendeleev Congress on General and Applied Chemistry. Ekaterinburg: Ural Branch of the Russian Academy of Sciences, 2016, pp. 25–26.
  3. Kablov E.N., Chursova L.V., Babin A.N., Mukhametov R.R., Panina N.N. Developments of FSUE «VIAM» in the field of melt binders for polymer composite materials. Polimernye materialy i tekhnologii, 2016, vol. 2, no. 2, pp. 37−42.
  4. Chernin I.Z., Smekhov F.M., Zherdev Yu.V. Epoxy polymers and compositions. Moscow: Khimiya, 1982, 232 p.
  5. Khorova E.A., Myshlyavtsev A.V., Strizhak E.A., Tretyakova N.A. Examination of hydrogenated butadiene-nitrile rubbers by methods of differential scanning calorimetry and dynamic mechanical analysis. Aviacionnye materialy i tehnologii, 2019, no. 1 (54), pp. 11–16. DOI: 10.18577/2071-9140-2019-0-1-11-16.
  6. Кhorova E.A., Tretyakova N.A., Vakulov N.V. Research of resistance of rubbers to the exposure of mold fungi. Aviation materials and technologies, 2021, no. 3 (64), paper no. 12. Available at: http://www.journal.viam.ru (accessed: December 12, 2023). DOI: 10.18577/2713-0193-2021-0-3-128-132.
  7. Kuznetsova V.А. Influence of the elastomeric modifier on mechanical and viscoelastic properties of epoxy and rubber compositions for erosion resistant coatings. Aviacionnye materialy i tehnologii, 2020, no. 2 (59), pp. 56–62. DOI: 10.18577/2071-9140-2020-0-2-56-62.
  8. Mukhametov R.R., Petrova A.P. Thermosetting binders for polymer composites (review). Aviacionnye materialy i tehnologii, 2019, no. 3 (56), pp. 48–58. DOI: 10.18577/2071-9140-2019-0-3-48-58.
  9. Andrianov R.A., Ponomarev Yu.E. Foams based on phenol-formaldehyde polymers. Rostov: Publ. house Rostov State Univ., 1987, 80 p.
  10. Vorobyov V.A. Polymer technology. Moscow: Vysshaya shkola, 1980, 303 p.
  11. Guben-Weil. Methods of organic chemistry: in 2 vols. Moscow: Khimiya, 1967, vol. 2: Methods of analysis, 1032 p.
  12. Siggia S., Hannah J.G. Quantitative organic analysis by functional groups. Moscow: Khimiya, 1983, 672 p.
  13. Sauer E.A., Ershov A.B. Modern analyzers for determining nitrogen using the Kjeldahl method. Analitika i kontrol, 2019, no. 2, pp. 168–192. DOI: 10.15826/analitika.2019.23.2.002.
  14. Isakova N.A., Fikhtengolts V.S., Belova G.A., Pankratova E.D. Technical analysis and control of synthetic rubber production. Leningrad: Khimiya, 1976, 168 p.
  15. State Standard 32979–2014. Solid mineral fuel. Instrumental method for the determination of carbon, hydrogen and nitrogen. Moscow: Standartinform, 2015, 11 p.
  16. Fundamentals of analytical chemistry: in 2 vols. Ed. Yu.A. Zolotov. Moscow: Vysshaya shkola, 1996, vol. 1: General questions. Separation methods, 383 p.
  17. Ponomarenko S.A., Shimkin A.A. Chromatographic methods of analysis: possibilities of application in the aviation industry (review). Zavodskaya laboratoriya. Diagnostika materialov, 2017, vol. 83, no. 4, pp. 5–13.