Krasnov I.S., M.A. Dalin, Zarodova A.A., Yakovleva S.I., Verhodanova A.A. A automated ultrasonic inspection of titanium alloy gas turbine disc forgings using conical acoustic mirror // Proceedings of VIAM. 2024. No. 5 (135). Ст. 04. URL: https://www.viam-works.ru. DOI: 10.18577/2307-6046-2024-0-5-37-49.

A automated ultrasonic inspection of titanium alloy gas turbine disc forgings using conical acoustic mirror

Krasnov I.S., M.A. Dalin, Zarodova A.A., Yakovleva S.I., Verhodanova A.A.
Abstract

Acoustic conical mirror for high sensitivity ultrasonic inspection of titanium alloy complex shape forging was offered and developed. Its geometrical parameters were calculated using mathematical modelling. The correction coefficients which are needed for compensation of the curved input surface influence were calculated. The high accuracy of the calculation was confirmed. The use of an acoustic mirror allowed increasing the sensitivity of inspection by more than 12 dB (4 times).

Keywords
acoustic mirror, sensitivity, ultrasonic inspection, curved surface, titanium alloy, forgings
Reference list
  1. Kablov E.N. VIAM: new generation materials for PD-14. Krylya Rodiny, 2019, no. 7–8, pp. 54–58.
  2. Kablov E.N. VIAM materials and technologies for Aviadvigatel. Permskiye aviatsionnyye dvigateli, 2014, no. 31, pp. 43–47.
  3. Kablov E.N. New generation materials – the basis of innovation, technological leadership and national security of Russia. Intellekt i tekhnologii, 2016, no. 2 (14), pp. 16–21.
  4. Antipov V.V. Prospects for development of aluminium, magnesium and titanium alloys for aerospace engineering. Aviacionnye materialy i tehnologii, 2017, no. S, pp. 186–194. DOI: 10.18577/2107-9140-2017-0-S-186-194.
  5. Duyunova V.A., Pavlova T.V., Kashapov O.S., Chuchman O.V. Fatigue strength of forgings from VT6 alloy for parts of gas turbine engines and aircrafts. Aviation materials and technologies, 2023, no. 2 (71), paper no. 02. Available at: http://www.journal.viam.ru (accessed: November 13, 2023). DOI: 10.18577/2713-0193-2023-0-2-23-35.
  6. Gorbovets M.A., Hodinev I.A., Karashaev M.M., Ryzhkov P.V. Low cycle dwell fatigue testing of heat resistant metallic materials (review). Trudy VIAM, 2022, no. 5 (111), paper no. 11. Available at: http://www.viam-works.ru (accessed: November 13, 2023). DOI: 10.18577/2307-6046-2022-0-5-123-137.
  7. Airworthiness standards for aircraft engines: AP-33: approved by Resolution of the 32nd session of the Council on Aviation and Airspace Use on 17.02.2012. 3rd ed. with amendments 33-1 and 33-2. Moscow: Aviaizdat, 2012, pp. 7–11.
  8. Gorbovets M.A., Slavin A.V. Proof of material compliance with the requirements to part No. 33 of JARs. Aviaсionnye materialy i tehnologii, 2018, no. 3, pp. 89–94. DOI: 10.18577/2071-9140-2018-0-3-89-94.
  9. Krasnov I.S., Lozhkova D.S., Dalin M.A. Evaluation of deficiency of titanium alloy forgings for probabilistic calculation of gas turbine engine disks fracture risk. Aviation materials and technologies, 2021, no. 2 (63), paper no. 12. Available at: https://www.journal.viam.ru (accessed: November 13, 2023). DOI: 10.18577/2713-0193-2021-0-2-115-122.
  10. AC 33.14-1 - Damage Tolerance for High Energy Turbine Engine Rotors. Washington, DC: Department of Transportation, Federal Aviation Administration, 2001, 128 р.
  11. Nikolaev E.V., Slavin A.V., Startsev V.O., Laptev A.B. Modern approaches to assessing the impact of external factors on materials and complex technical systems (to the 120th anniversary of G.V. Akimov). Trudy VIAM, 2021, no. 9 (103), paper no. 12. Available at: http://www.viam-works.ru (accessed: November 13, 2023). DOI: 10.18577/2307-6046-2021-0-9-117-130.
  12. Kablov E.N. Innovative developments of FSUE «VIAM» SSC of RF on realization of «Strategic directions of the development of materials and technologies of their processing for the period until 2030». Aviacionnye materialy i tehnologii, 2015, no. 1 (34), pp. 3–33. DOI: 10.18577/2071-9140-2015-0-1-3-33.
  13. AMS2628. Ultrasonic Immersion Inspection Titanium and Titanium alloy Billet Premium Grade. New York, NY: SAE, 2019, 26 р.
  14. DOT/FAA/AR-05/29. Inspection Development for Nickel Billet–Engine Titanium Consortium Phase II. Washington, DC: Department of Transportation Federal Aviation Administration, 2005, рр. 3–21.
  15. Karpelson A. Bi-curved Ultrasonic Transducers. The e-Journal of Nondestructive Testing, 2006, vol. 11, no. 5. Available at: https://www.ndt.net/article/v11n05/karpelson/karpelson.htm (accessed: November 13, 2023).
  16. AMS2636 Rev. A. Ultrasonic Immersion Inspection Titanium and Titanium Alloy Forgings Premium Grade. New York, NY: SAE, 2016, 16 р.