Bondarenko Yu.A., Narskiy A.R., Kolodiazniy M.Yu. Experimental and computational methods for studying the thermal conditions of the process of directional crystallization of nickel superalloys // Proceedings of VIAM. 2024. No. 4 (134). Ст. 01. URL: https://www.viam-works.ru. DOI: 10.18577/2307-6046-2024-0-4-3-17.

Experimental and computational methods for studying the thermal conditions of the process of directional crystallization of nickel superalloys

Bondarenko Yu.A., Narskiy A.R., Kolodiazniy M.Yu.
Abstract

The paper presents the results of the application of experimental and computational methods for studying the thermal conditions of the process of directed crystallization of heatresistant alloys, which have found wide application in the production of blades for modern aviation
gas turbine engines made of heat-resistant alloys. Methods for estimating the values of the temperature gradient, the crystallization rate, the size of the liquid-solid zone at the crystallization front, and their effect on the structure and properties of superalloys are proposed and implemented

Keywords
directional crystallization, superalloys, temperature gradient, crystallization front, structure, properties
Reference list
  1. Kablov E.N. Cast blades of gas turbine engines. Alloys, technologies, coatings. 2nd ed. Moscow: Nauka, 2006, 632 p.
  2. Kablov E.N. Specialty: metal for aviation. On the occasion of the 100th anniversary of the birth of Academician S.T. Kishkina. Vestnik Rossiyskoy akademii nauk, 2006, vol. 76, no. 6, pp. 553–558.
  3. Kablov E.N., Svetlov I.L., Petrushin N.V. Nickel heat-resistant alloys for casting blades with directional and monocrystalline structure (part I). Materialovedenie, 1997, no. 4. pp. 32–39.
  4. Bazyleva O.A., Arginbayeva E.G., Lutskaya S.A., Dmitriev N.S. Foundry intermetallic alloy based on Ni3Al compound for turbine blades gas turbine engines. Aviation materials and technologies, 2022, no. 2 (67), paper no. 01. Available at: http://www.journal.viam.ru (accessed: January 09, 2024). DOI: 10.18577/2713-0193-2022-0-2-5-17.
  5. Svetlov I.L., Petrushin N.V., Epishin A.I., Karashaew M.M., Elyutin E.S. Single crystals of nickel-based superalloys alloyed with rhenium and ruthenium (review). Part 1. Aviation materials and technologies, 2023, no. 1 (70), paper no. 03. Available at: http://www.journal.viam.ru (accessed: January 09, 2024). DOI: 10.18577/2713-0193-2023-0-1-30-50.
  6. Svetlov I.L., Petrushin N.V., Epishin A.I., Karashaew M.M., Elyutin E.S. Single crystals of nickel-based superalloys alloyed with rhenium and ruthenium (review). Part 2. Aviation materials and technologies, 2023, no. 2 (71), paper no. 01. Available at: http://www.journal.viam.ru (accessed: January 09, 2024). DOI: 10.18577/2071-9140-2023-0-2-3-22.
  7. Kablov E.N. Innovative developments of FSUE «VIAM» SSC of RF on realization of «Strategic directions of the development of materials and technologies of their processing for the period until 2030». Aviacionnye materialy i tehnologii, 2015, no. 1 (34), pp. 3–33. DOI: 10.18577/2071-9140-2015-0-1-3-33.
  8. Matuszewski K., Müller A., Ritter N., Retting R., Kurzydłowski K.J., Singer R.F. On the thermodynamics and kinetics of TCP phase precipitation in Re- and Ru-containing Ni-base superalloys. Advanced Engineering Materials, 2015, vol. 17, no. 8, pp. 1127–1133.
  9. Matuszewski K., Retting R., Singer R.F. The effect of Ru on precipitation of two topologically close packed phases in Re-containing Ni base superalloys: quantitative FIB-SEM investigation and 3D image modeling. MATEC Web of Conferences, 2014, vol. 14, art. 09001. DOI: 10.1051/matecconf/20141409001.
  10. Kablov E.N., Petrushin N.V., Svetlov I.L. Computer-aided design of a heat-resistant nickel alloy of the fourth generation for single-crystal gas turbine blades. Foundry heat-resistant alloys. Effect of S.T. Kishkin. Moscow: Nauka, 2006, pp. 98–115.
  11. Min P.G., Vadeev V.E. The development and introduction into serial production of the new superalloy VZhL125 for the advanced aviation engines vanes. Aviation materials and technologies, 2023, no. 1 (70), paper no. 01. Available at: http://www.journal.viam.ru (accessed: January 09, 2024). DOI: 10.18577/2713-0193-2023-0-3-3-14.
  12. Bridgman P.W. Certain physical properties of single crystals of tungsten, antimony, bismuth, tellurium, cadmium, zinc, and tin. Proceedings of the American Academy of Arts and Sciences, 1925, vol. 60, рp. 305–383.
  13. Stockbarger D.C. The production of large single crystals of lithium fluoride. Review of Scientific Instruments, 1936, vol. 7, pp. 133–136.
  14. Giamei A.F., Tschinkel J.G. Liquid Metal Cooling: A New Solidification Technique. Metallurgical Transactions A, 1976, vol. 7A, pp. 1427–1434.
  15. Bondarenko Yu.A., Echin A.B., Surova V.A., Narsky A.R. Development of technologies and equipment for producing blades of the hot path of gas turbine engines from superalloys with directional and single-crystal structure. Trudy VIAM, 2023, no. 7 (125), paper no. 01. Available at: http://www.viam-works.ru (accessed: January 11, 2024). DOI: 10.18577/2307-6046-2023-0-7-3-14.
  16. Bondarenko Yu.A., Echin A.B., Surova V.A., Narsky A.R. On the directional crystallization of heat-resistant alloys using a cooler. Liteynoe proizvodstvo, 2011, no. 5, pp. 36–39.
  17. Gerasimov V.V., Morozova G.I., Tarasova I.M. On the chemical nature of «boils» in the production of single-crystalline blades from heat-resistant nickel alloys. Tekhnologiya metallov, 2000, no. 7, pp. 7–8.
  18. Kolyadov E.V., Visik E.M., Shurygin V.D. Equipment for cleaning crystallizers of directional crystallization plants. Liteynoe proizvodstvo, 2023, no. 1, pp. 33–36.
  19. Bondarenko Yu.A., Echin A.B., Bazhenov V.E., Koltygin A.V. Computer modeling of temperature distribution on the surface of the mold and inside the casting during high-gradient directional crystallization. Izvestiya vuzov. Tsvetnaya metallurgiya, 2017, no.4, pp. 53–61.
  20. Pikunov M.V. Melting of metals. Crystallization of alloys. Hardening of castings. Moscow: MISIS, 2005, 414 p.
  21. Echin A.B. The influence of temperature gradient and crystallization rate on the structure and properties of monocrystalline Re and Ru containing heat-resistant alloys in relation to high-gradient technology for casting gas turbine engine blades: thesis, Cand. Sc. (Tech). Moscow: VIAM, 2016, 135 p.