Selection of curing system when developing epoxy compositions with energy-efficient curing mode

Guseva M.A., Ibragimov Z.D.
Abstract

Polymer binders with an energy-efficient curing mode are compositions containing hardeners and curing accelerators that are capable of curing the polymer system at low temperatures (120–150 °C), with minimal time, while maintaining the increased strength and thermomechanical characteristics of PCM, derived from it. This paper presents a technology for the development of a polymer binder with selection of a curing system to obtain an epoxy composition with an energy-efficient curing mode as part of import substitution issues.

Keywords
development of polymer binders, epoxy compositions, energy efficiency, curing mode, catalytic system, hardener
Reference list
  1. Panina N.N., Kim M.A., Gurevich Ya.M., Grigoriev M.M., Chursova L.V., Babin A.N. Binders for non-autoclave molding of products from polymer composite materials. Klei. Germetiki. Tekhnologii, 2013, no. 10, pp. 18–27.
  2. Veshkin E.A., Postnov V.I., Abramov P.A. Ways to improve the quality of PCM parts during vacuum forming. Izvestiya Samarskogo nauchnogo tsentra Rossiyskoy akademii nauk, 2012, vol. 14, no. 4 (3), pp. 831–838.
  3. Postnova M.V., Postnov V.I. Development experience out-of-autoclave methods of formation PCM. Trudy VIAM, 2014, no. 4, paper no. 06. Available at: http://viam-works.ru (accessed: January 10, 2024). DOI: 10.18577/2307-6046-2014-0-4-6-6.
  4. Khrulkov A.V., Grigoriev M.M. Prospects for the market for non-autoclave technologies in the aircraft industry. Reports conf. «Non-autoclave technologies for processing new generation polymer composite materials». Moscow: VIAM, 2015, paper no. 09.
  5. Veshkin E.A. Technologies for non-autoclave molding of low-porosity polymer composite materials and large-sized structures made from them: thesis, Cand. Sc. (Tech.). Moscow, 2016, 146 p.
  6. 6 Trostyanskaya E.B., Mikhailin Yu.A., Kulik S.G., Stepanova M.A. Binders based on epoxy resins: textbook. Moscow, 1990, p. 27.
  7. Kogan D.I., Chursova L.V., Panina N.N. et al. Promising polymer materials for structural composite products with energy-efficient molding mode. Plasticheskie massy, 2020, no. 3–4, pp. 52–54.
  8. Ivanov N.V., Gurevich Ya.M., Khaskov M.A., Akmeev A.R. Studying of cure mode of VSE-34 binding and its influences on mechanical properties. Aviacionnye materialy i tehnologii, 2017, no. 2 (47), pp. 50–55. DOI: 10.18577/2071-9140-2017-0-2-50-55.
  9. Mukhametov R.R., Petrova A.P. Thermosetting binders for polymer composite materials: textbook. Ed. E.N. Kablov. Moscow: NRC «Kurchatov Institute» – VIAM, 2021, p. 363.
  10. Kablov E.N. Strategical Areas of Developing Materials and Their Processing Technologies for the Period up to 2030. Aviacionnye materialy i tehnologii, 2012, no. S, pp. 7–17.
  11. Kablov E.N., Kondrashov S.V., Melnikov A.A., Schur P.A. Application of functional and adaptive materials obtained by 3D printing (review). Trudy VIAM, 2022, no. 2 (108), paper no. 03. Available at: http://www.viam-works.ru (accessed: November 20, 2023). DOI: 10.18577/2307-6046-2022-0-2-3-3.
  12. Mishkin S.I., Malakhovskiy S.S. Fast curing resins and prepregs: receiving, properties and areas of application (review). Trudy VIAM, 2019, no. 5 (77), paper no. 04. Available at: http://viam-works.ru (accessed: November 10, 2023). DOI: 10.18577/2307-6046-2019-0-5-32-40.
  13. Donetskiy K.I., Khrulkov A.V. Principles of «green chemistry» in perspective manufacturing technologies of PCM articles. Aviacionnye materialy i tehnologii, 2014, no. S2, pp. 24–28. DOI: 10.18577/2071-9140-2014-0-S2-24-28.
  14. Bolshakov V.A., Antyufeeva N.V. Evaluation of the curing process model of the adhesive binder in prepreg. Aviation materials and technologies, 2023, no. 4 (73), paper no. 07. Available at: http://www.journal.viam.ru (accessed: November 25, 2023). DOI: 10.18577/2713-0193-2023-0-4-66-77.
  15. Startsev V.O., Antipov V.V., Slavin A.V., Gorbovets M.A. Modern domestic polymer composite materials for aviation industry (review). Aviation materials and technologies, 2023, no. 2 (71), paper no. 10. Available at: http://www.journal.viam.ru (accessed: November 15, 2023). DOI: 10.18577/2713-0193-2023-0-2-122-144.