Turchenko M.V., Lebedeva Yu.E., Prokofiev V.A., Zhitnyuk S.V. Investigation of the boron nitride effect on the machinability of SiC–ZrB2 system ceramic material // Proceedings of VIAM. 2024. No. 2 (132). Ст. 06. URL: https://www.viam-works.ru. DOI: 10.18577/2307-6046-2024-0-2-57-66.

Investigation of the boron nitride effect on the machinability of SiC–ZrB2 system ceramic material

Turchenko M.V., Lebedeva Yu.E., Prokofiev V.A., Zhitnyuk S.V.
Abstract

The production of SiC–ZrB2–BN system ceramic materials by spark plasma sintering (SPS) at temperatures of 1850–1950 °C is presented. The SPS method made it possible to obtain a ceramic material with a homogeneous structure and a grain size of 0.5–3 μm. The influence of the amount of boron nitride on the machinability and oxidative resistance of ceramics was studied. It has been established that with a boron nitride content of 20 % (vol.), the ceramic material retains a high level of mechanical properties and a good degree of workability, however, it has low oxidative resistance.

Keywords
machined ceramics, ceramic material, spark plasma sintering, zirconium boride, silicon carbide, boron nitride
Reference list
  1. Kablov E.N. Main directions of development of materials for aerospace technology of the XXI century. Perspektivnye materialy, 2000, no. 3, pp. 27–36.
  2. Sorokin O.Yu., Kuznetsov B.Yu., Lunegova Yu.V., Erasov V.S. High-temperature composites with a multi-layered structure (review). Trudy VIAM, 2020, no. 4–5 (88), paper no. 05. Available at: http://www.viam-works.ru (accessed: December 01, 2023). DOI: 10.18577/2307-6046-2020-0-45-42-53.
  3. Serebryakova T.I., Neronov V.A., Peshev P.D. High temperature borides. Moscow: Metallurgiya, 1991, 368 p.
  4. Kablov E.N., Grashchenkov D.V., Isaeva N.V., Solntsev S.St. Perspective High-Temperature Ceramic Composite Materials. Russian Journal of General Chemistry, 2011, vol. 81, no. 5, pp. 986–991.
  5. Kulagin N.D. High-temperature multicomponent ceramic materials based on carbides: preparation, structure, oxidative behavior: bachelor's thesis. Tomsk, 2022, 92 p. Available at: http://earchive.tpu.ru/handle/11683/71841 (accessed: December 01, 2023).
  6. Kablov E.N., Grashchenkov D.V., Isaeva N.V., Solntsev S.S., Sevastyanov V.G. Promising high-temperature ceramic composite materials. Rossiyskiy khimicheskiy zhurnal, 2010, vol. LIV, no. 1, pp. 20–24.
  7. Zhitnyuk S.V. Effect of sintering additives on the properties of silicon carbide-based ceramics (review). Trudy VIAM, 2019, no. 3 (75), paper no. 09. Available at: http://www.viam-works.ru (accessed: December 01, 2023). DOI: 10.18577/2307-6046-2019-0-3-79-86.
  8. Zhitnyuk S.V., Sorokin O.Yu., Zhuravleva P.L. Silicon carbide ceramics obtained by sintering granular powder. Trudy VIAM, 2020, no. 2 (86), paper no. 06. Available at: http://www.viam-works.ru (accessed: December 01, 2023). DOI: 10.18577/2307-6046-2020-0-2-50-59.
  9. Evdokimov S.A., Shchegoleva N.E., Kachaev A.A. Methods for joining ceramic composite materials based on SiC with ceramic and metallic materials (review). Aviation materials and technologies, 2022, no. 3 (68), paper no. 07. Available at: http://www.journal.viam.ru (accessed: December 01, 2023). DOI: 10.18577/2307-6046-2022-0-3-75-83.
  10. Burlachenko A.G., Buyakova S.P., Mirova Yu.A., Dedova E.S. Kinetics of self-healing in high-temperature ZrB2–SiC ceramics. Powder metallurgy: surface engineering, new powder composite materials. Welding: Sat. report XXI Int. symposium: at 2 parts. Minsk: Publishing house «Belarusian Science», 2019, part 1, pp. 431–435.
  11. Ordanyan S.S., Nesmelov D.D., Novoselov E.S. Statistical assessment of the mechanical characteristics of hot-pressed ceramics in the ZrB2–SiC system. Vestnik Tomskogo gosudarstvennogo universiteta. Matematika i mekhanika, 2023, no. 82, pp. 150–160.
  12. Pushkarev O.I., Umansky A.P. Preparation of wear-resistant composite ceramics based on silicon carbide by hot pressing. Processes of abrasive processing, abrasive tools and materials. Sanding abrasive – 99. Volgograd, 1999, pp. 45–47.
  13. Kuznetsov B.Yu., Sorokin O.Yu., Vaganova M.L., Osin I.V. Synthesis of model high-temperature ceramic matrices by the method of spark plasma sintering and the study of their properties for the production of composite materials. Aviacionnye materialy i tehnologii, 2018, no. 4 (53), pp. 37–44. DOI: 10.18577/2071-9140-2018-0-4-37-44.
  14. Vaganova M.L., Sorokin O.Yu., Osin I.V. Joining of ceramic materials by the method of spark plasma sintering. Aviacionnye materialy i tehnologii, 2017, no. S, pp. 306–317. DOI: 10.18577/2071-9140-2017-0-S-306-317.
  15. Sorokin O.Yu., Solntsev S.St., Evdokimov S.A., Osin I.V. Hybrid spark plasma sintering method: principle, possibilities, future prospects. Aviacionnye materialy i tehnologii, 2014, no. S6, pp. 11–16. DOI: 10.18577/2071-9140-2014-0-s6-11-16.
  16. Barinov V.Yu., Rogachev A.S., Vadchenko S.G., Moskovskikh D.O., Kolobov Yu.R. Spark plasma sintering of complex-shaped products using quasi-isostatic pressing. Mezhdunarodnyy zhurnal prikladnykh i fundamentalnykh issledovaniy, 2016, no. 1–3, pp. 312–315.
  17. Avramenko V.A., Papynov E.K., Shichalin O.O. et al. Spark plasma sintering as an innovative approach to the creation of new generation nanostructured ceramics. Nanomaterials and technologies: VI Int. conf. «Nanomaterials and technologies», V Int. conf. in materials science and II Int. conf. on functional materials. Ulan-Ude, 2016. pp. 82–90.
  18. Perevislov S.N. Structure, properties and areas of application of graphite-like hexagonal boron nitride. Novye ogneupory, 2019, no. 6, pp. 35–40.
  19. Way of receiving the fire-resistant mix containing boron nitride: pat. 2021124557 Rus. Federation; appl. 19.08.21; publ. 08.11.21.
  20. Dudchenok N.V., Chervoniy I.F. Research on hexagonal boron nitride technology. ScienceRise, 2016, vol. 12, no. 2 (29), pp. 31–34.