Varrik N.M., Maximov V.G., Yudin A.V., Babashov V.G. On the criteria of suitability of ceramic products for the manufacture of equipment for continuous casting of aluminum // Proceedings of VIAM. 2024. No. 2 (132). Ст. 05. URL: https://www.viam-works.ru. DOI: 10.18577/2307-6046-2024-0-2-49-56.

On the criteria of suitability of ceramic products for the manufacture of equipment for continuous casting of aluminum

Varrik N.M., Maximov V.G., Yudin A.V., Babashov V.G.
Abstract

Ceramic tooling is increasingly being used in the metallurgical industry, particularly in casting workshops of non-ferrous metals. Currently, various types of heat-resistant ceramics have been developed for injection molds and crucibles. Abroad, ceramics made from the natural mineral wollastonite, which also contains plasticizers and fluxing additives, are most often used for the manufacture of tooling. To obtain such products NRC «Kurchatov Institute» – VIAM has developed сeramics based on high silica fiber. In this paper, some aspects of the durability and criteria for evaluating their operational properties of ceramic products for the manufacture of tooling for continuous casting of aluminum are considered.

Keywords
ceramic tooling, aluminum casting, silica fiber, corrosion resistance
Reference list
  1. Onishchenko G.G., Kablov E.N., Ivanov V.V. Scientific and technological development of Russia in the context of achieving national goals: problems and solutions. Innovatsii, 2020, no. 6 (260), pp. 3–16.
  2. Oglodkov M.S., Romanenko V.A., Kozhekin A.E. Directions of development melting and casting technologies of aluminum-lithium alloys (review). Aviation materials and technologies, 2023, no. 2 (71), paper no. 04. Available at: http://www.journal.viam.ru (accessed: October 02, 2023). DOI: 10.18577/2713-0193-2023-0-2-51-62.
  3. Echin A.B., Deynega G.I., Narsky A.R. New developments of NRC «Kurchatov Institute» – VIAM in the field of materials for casting processes of superalloys. Trudy VIAM, 2023, no. 8 (126), paper no. 02. Available at: http://www.viam-works.ru (accessed: October 02, 2023). DOI: 10.18577/2307-6046-2023-0-8-13-24.
  4. Voronov V.A., Chaynikova A.S., Tkalenko D.M. Aspects of usage of organic or aqueous binders based on III or IV group elements oxides in the production of ceramic molds for chemically active alloys casting (review). Aviation materials and technologies, 2021, no. 2 (63), paper no. 08. Available at: http://www.journal.viam.ru (accessed: February 20, 2023). DOI: 10.18577/2713-0193-2021-0-2-73-84.
  5. Loshchinin Yu.V., Shorstov S.Yu., Kuzmina I.G. Research of influence of technology factors on thermal conductivity of ceramic casting molds. Aviacionnye materialy i tehnologii, 2019, no. 2 (55), pp. 89–94. DOI: 10.18577/2071-9140-2019-0-2-89-94.
  6. Antipina S.A., Vereshchagin V.I. Heat-resistant material for aluminum casting. Izvestiya Tomskogo politekhnicheskogo universiteta, 2009, no. 3, pp. 8–11.
  7. Method of manufacturing ceramic melting crucibles: pat. 2713049 Rus. Federationn; appl. 17.12.18; publ. 03.02.20.
  8. Rusanova L.N., Rusin M.Yu., Gorchakova L.I. et al. Ceramics from natural wollastonite for foundry installations of the aluminum industry. Ogneupory i tekhnicheskaya keramika, 2008, no. 5, pp. 39–44.
  9. Kalugin V.G., Kostyrev Yu.P., Kuksin I.G. Structural and thermal insulation materials and pro-ducts based on wollastonite for the aluminum industry. Novye ogneupory, 2004, no. 9, pp. 8–9.
  10. Garashchenko A.N., Vinogradov A.V., Kobylkov N.V., Nikolchenkin A.A., Antipov E.A. Experimental and computational modeling of fire and thermal protection composite materials under high-temperature exposure. Aviation materials and technologies, 2022, no. 3 (68), paper no. 08. Available at: http://www.journal.viam.ru (accessed: October 02, 2023). DOI: 10.18577/2713-0193-2022-0-3-84-97.
  11. Matrenin S.V., Slosman A.I. Technical ceramics: textbook. Tomsk: Publishing House of TPU, 2004, 75 p.
  12. Apakashev R.A., Davydov S.Ya. Study of the interaction of molten aluminum with the contact surface of a quartz refractory. Novye ogneupory, 2015, no. 4, pp. 46–48. DOI: 10.17073/1683-4518-2015-4-46-48.
  13. Maksimov V.G., Varrick N.M. On the issue of obtaining chemically resistant quartz ceramics with open porosity. Novosti materialovedeniya. Nauka i tekhnika, 2017, no. 1, art. 01. Available at: http://www.materialsnews.ru (accessed: October 10, 2023).
  14. Method for producing fibrous ceramic material: pat. 2358954 Rus. Federation; appl. 08.11.07; publ. 20.06.09.
  15. Babashov V.G., Ivahnenko Yu.A., Yudin A.V., Zimichev A.M. Ceramic material for parts of continuous casting units intended for production of non-ferrous alloys. Trudy VIAM, 2014, no. 12, paper no. 06. Available at: http://www.viam-works.ru (accessed: October 02, 2023). DOI: 10.18577/2307-6046-2014-0-12-5-5.