Stepanova E.V., Ivakhnenko Yu.A., Maximov V.G., Istomin A.V. Investigation of technologically significant physical properties of various brands of polyvinyl alcohol // Proceedings of VIAM. 2024. No. 2 (132). Ст. 03. URL: https://www.viam-works.ru. DOI: 10.18577/2307-6046-2024-0-2-23-33.

Investigation of technologically significant physical properties of various brands of polyvinyl alcohol

Stepanova E.V., Ivakhnenko Yu.A., Maximov V.G., Istomin A.V.
Abstract

The article presents the results of research on several brands of partially hydrolyzed polyvinyl alcohol. Rheological characteristics (dependence of viscosity on temperature and activation energy of flow) of aqueous polymer solutions are determined. The completeness of the dissolution of polyvinyl alcohol was determined by optical microscopy. The types of foreign particles present in the solution characteristic of each method of dissolution and type of polymer have been identified. It has been established that the use of polyvinyl alcohol with a relatively low molecular weight is required to obtain technologically optimal solutions.

Keywords
polyvinyl alcohol, low molecular weight polymer, high molecular weight polymer, rheological characteristics, viscosity, activation energy
Reference list
  1. Kablov E.N. The role of fundamental research in the creation of new generation materials. Reports XXI Mendeleev Congress on General and Applied Chemistry: in 6 vols. St. Petersburg, 2019, vol. 4, p. 24.
  2. Onishchenko G.G., Kablov E.N., Ivanov V.V. Scientific and technological development of Russia in the context of achieving national goals: problems and solutions. Innovatsii, 2020, no. 6 (260), pp. 3–16.
  3. Startsev V.O., Antipov V.V., Slavin A.V., Gorbovets M.A. Modern domestic polymer composite materials for aviation industry (review). Aviation materials and technologies, 2023, no. 2 (71), paper no. 10. Available at: http://www.journal.viam.ru (accessed: December 22, 2023). DOI: 10.18577/2713-0193-2023-0-2-122-144.
  4. Ivakhnenko Yu.A., Kuzmin V.V., Bespalov A.S. State and prospects for the development of heat and sound insulating fireproof materials. Problemy bezopasnosti poletov, 2014, no. 7, pp. 27–30.
  5. Buchilin N.V., Maksimov V.G., Babashov V.G. Ceramic filters for molten aluminum (review). Steklo i keramika, 2015, no. 7, pp. 20–28.
  6. Maksimov V.G., Varrik N.M., Babashov V.G. Features of obtaining ceramic materials from sintering-active powders. Novye ogneupory, 2023, no. 10, pp. 14–21.
  7. Lebedeva Yu.E., Shchegoleva N.E., Voronov V.A., Solntcev S.S. Al2O3 and ZrO2 ceramic materials obtained by sol-gel method. Trudy VIAM, 2021, no. 4 (98), paper no. 05. Available at: http://www.viam-works.ru (accessed: December 11, 2023). DOI: 10.18577/2307-6046-2021-0-4-61-73.
  8. Aristova Е.Yu., Denisova V.А., Drozhzhin V.S. et al. Composite materials using hollow microspheres. Aviacionnye materialy i tehnologii, 2018, no. 1 (50), pp. 52–57. DOI: 10.18577/2071-9140-2018-0-1-52-57.
  9. Duyunova V.A., Serebrennikova N.Yu., Nefedova Yu.N., Sidelnikov V.V., Somov A.V. Methods of forming metal-polymer composite materials (review). Aviation materials and technologies, 2022, no. 1 (66), paper no. 06. Available at: http://www.journal.viam.ru (ассеssed: December 22, 2023). DOI: 10.18577/2713-0193-2022-0-1-65-77.
  10. Dushin M.I., Donetskiу K.I., Timoshkov P.N., Karavaev R.Yu. Research of process of out-of-autoclave formation semipregs on the basis of carbon fillers (rеview). Trudy VIAM, 2018, no. 9 (69), paper no. 03. Available at: http://www.viam-works.ru (accessed: December 12, 2023). DOI: 10.18577/2307-6046-2018-0-9-21-31.
  11. Sidorina A.I., Safronov A.M., Kutsevich K.E., Klimenko O.N. Carbon fabrics for aircraft products. Trudy VIAM, 2020, no. 12 (94), paper no. 05. Available at: http://www.viam-works.ru (accessed: December 11, 2023). DOI: 10.18577/2307-6046-2020-0-12-47-58.
  12. Rosenberg M.E. Polyvinyl acetate based polymers. Leningrad: Khimiya, 1983, 176 p.
  13. Ushakov S.N. Polyvinyl alcohol and its derivatives: in 2 vols. Moscow; Leningrad: USSR Academy of Sciences Publishing House, 1960, vol. 1, 552 p.
  14. Konkin A.A. Carbon and other heat-resistant fibrous materials. Moscow: Khimiya, 1974, 376 p.
  15. Zhilyakova E.T., Popov N.N., Khalikova M.A., Novikova M.Yu., Pridachina D.V. Technological characteristics of a supramicrostructured combined prolongator-thickener Na-CMC and PVA. Mezhdunarodnyy zhurnal eksperimentalnogo obrazovaniya, 2015, no. 4–2, pp. 450–452.
  16. State Standatd 10779–78. Polyvinyl alcohol. Technical specifications (with Amendments No. 1, 2). Moscow: Publ. house of standards, 1978, 23 p.
  17. Kharchenko I.M. Thermochemical transformations of polyvinyl alcohol fiber in the presence of pyrolytic additives during the production of carbon fiber: abstract thesis, Cand. Sc. (Chem.). Moscow, 2006, 174 p.
  18. Buzov B.A., Alymenkova N.D. Materials science in the production of light industry products. Moscow: ACADEMA, 2004, 135 p.
  19. Lebedeva A.V., Olekhnovich R.O., Morozkina S.N., Uspenskaya M.V. Study of obtaining nanofibers from aqueous solutions of polyvinyl alcohol by electrospinning. Vestnik VGUIT, 2022, vol. 84, no. 2, pp. 210–220. DOI: 10.20914/2310-1202-2022-2-210-220.
  20. Perepelkin K.E. Physico-chemical foundations of the processes of forming chemical fibers. Moscow: Khimiya, 1978, 320 p.
  21. Tager A.A. Physico-chemistry of polymers. 4th ed. Moscow: Nauchnyy mir, 2007, 576 p.
  22. Schramm G. Fundamentals of practical rheology and rheometry. Trans. from Engl. I.A. Lavygina; ed. V.G. Kulichikhin. Moscow: KolosS, 2003, 312 p.
  23. Pakshver E.A., Perepelkin K.E., Fikhman V.D., Varshavsky V.Ya., Zverev M.P. Carbon-chain synthetic fibers. Moscow: Khimiya, 1973, 589 p.
  24. Kruppennikova V.E., Radnaeva V.D., Tanganov B.B. Determination of dynamic viscosity using a Brookfield RVDV-II+Pro rotational viscometer. Ulan-Ude: VSTU, 2011, 47 p.
  25. Bartenev G.M. Determination of the activation energy of viscous flow of polymers from experimental data. Vysokomolekulyarnye soyedineniya, 1964, vol. 6, no. 2, pp. 335–340. DOI: 10.1016/0032-3950(64)90322-3.