Kapustianskaia M.A., Lyubimova A.S., Kovalenko A.V., Sidelnikov N.K., Tkachuk A.I., Slavin A.V. Development of a cold-curing polymer syntatic filler with enhanced physico-mechanical properties // Proceedings of VIAM. 2024. No. 11 (141). Ст. 04. URL: https://www.viam-works.ru. DOI: 10.18577/2307-6046-2024-0-11-33-43.

Development of a cold-curing polymer syntatic filler with enhanced physico-mechanical properties

Kapustianskaia M.A., Lyubimova A.S., Kovalenko A.V., Sidelnikov N.K., Tkachuk A.I., Slavin A.V.
Abstract

This paper presents the results of a study on the development of a cold-curing polymer syntactic filler composition for local strengthening of honeycomb panels, sealing end sections and filling technological voids of aircraft elements. About 100 compositions were studied, differing in components and their ratio in the system. The best composition based on test results was assigned the VPZ-25 brand. In terms of a number of properties, the developed material is at the same level or exceeds the characteristics of its foreign and domestic analogues.

Keywords
polymer filler, spheroplastic, PCM, honeycomb filler, epoxy binder, glass microspheres
Reference list
  1. Ketov Yu.A., Slovikov S.V. Syntactic polymer composite materials highly filled with granulated foam glass. Metody kontrolya i diagnostika v mashinostroyenii, 2019, vol. 6, no. 3, pp. 39–45.
  2. Panin S.V. Application of modern polymer composite materials in the airframe design of the MS-21 family of aircraft. Izvestiya Samarskogo nauchnogo tsentra Rossiyskoy akademii nauk, 2012, vol. 14, no. 4 (2), pp. 686–693.
  3. Aristov V.F., Vikhrov I.A. Radiotransparent cyanate ether syntactics (spheroplastics) based on hollow glass or polymer microspheres for spacecraft transceivers. Proc. XXI Int. scientific-practical. Conf., dedicated to the memory of the General Designer of Rocket and Space Systems, Academician M.F. Reshetnev. Moscow: Krasnoyarsk, 2017, pp. 66–67.
  4. Postnov V.I., Veshkin E.A., Makrushin K.V., Sudin Yu.I. Technological features of manufacturing polymer composite materials of main rotor blades for a light helicopter. Aviation materials and technologies, 2023, no. 1 (70), paper no. 06. Available at: http://www.journal.viam.ru (accessed: May 14, 2024). DOI: 10.18577/2713-0193-2023-0-1-82-92.
  5. Trostyanskaya E.B., Golovkin G.S., Dmitrenko V.P. Promising polymer composite materials and progressive technologies for their production of aircraft structural elements. Aviatsionnaya promyshlennost, 1987, no. 2, pp. 37–42.
  6. Shvetsov E.P., Sokolov I.I., Grebeneva T.A. Polymer nanomodified composite material for the construction industry. Novosti materialovedeniya. Nauka i tekhnika, 2016, no. 5 (23), paper no. 08. Available at: http://www.materialsnews.ru (accessed: March 01, 2024).
  7. Startsev V.O., Antipov V.V., Slavin A.V., Gorbovets M.A. Modern domestic polymer composite materials for aviation industry (review). Aviation materials and technologies, 2023, no. 2 (71), paper no. 10. Available at: http://www.journal.viam.ru (accessed: March 01, 2024). DOI: 10.18577/2713-0193-2023-0-2-122-144.
  8. Pavlyuk B.Ph. The main directions in the field of development of polymeric functional materials. Aviacionnye materialy i tehnologii, 2017, no. S, pp. 388–392. DOI: 10.18577/2071-9140-2017-0-S-388-392.
  9. Kablov E.N. The Role of Chemistry in Creating New-Generation Materials for Complex Technical Systems. Report of the XX Mendeleev Congress on General and Applied Chemistry. Ekaterinburg: Ural Branch of the Russian Academy of Sciences, 2016, pp. 25–26.
  10. Kablov E.N. Composites: Today and Tomorrow. Metally Evrazii, 2015, no. 1, pp. 36–39.
  11. Yakovenko T.V., Yarullina G.K., Garustovich I.V. et al. Spheroplasts as Thermal Insulating Protective Materials for Industrial Use. Uspekhi v khimii i khimicheskoy tekhnologii, 2016, vol. 3, no. 8, pp. 71–73.
  12. Mishurov K.S., Payarel S.M., Kurnosov A.O., Bokov V.V. Physical and mechanical properties of syntactic foam VPZ-24 with a maximum service temperature up to 320 °С. Trudy VIAM, 2022, no. 4 (110), paper no. 06. Available at: http://www.viam-works.ru (accessed: May 14, 2024). DOI: 10.18577/2307-6046-2022-0-4-52-60.
  13. Chursova L.V., Panina N.N., Grebeneva T.A., Kutergina I.Yu. Epoxy resins, hardeners, modifiers and binders based on them. St. Petersburg: Profession, 2020, 576 p.
  14. Sokolov I.I. Cold-curing spheroplasts based on adhesive binders for aviation products. Klei. Germetiki. Tekhnologii, 2013, no. 3, pp. 25–28.
  15. Kapustyanskaya M.A., Gurevich Ya.M., Mishurov K.S. Polymer filler for accelerated molding technology. Plasticheskiye massy, 2023, no. 11–12, pp. 50–53.
  16. Tkachuk A.I., Terekhov I.V., Afanasyeva E.A. Reactive type flame retardants for epoxy resins. Part 1. Trudy VIAM, 2020, no. 3 (87), paper no. 04. Available at: http://www.viam-works.ru (accessed: May 14, 2024). DOI: 10.18577/2307-6046-2020-0-3-41-48.
  17. Zastrogina O.B., Shvets N.I., Postnov V.I., Serkova E.A. Phenolformaldehyde binding new generation for interior materials. Aviacionnye materialy i tehnologii, 2012, no. S, pp. 265–272.
  18. Sarychev I.A., Serkova E.A., Khmelnitsky V.V., Zastrogin O.B. Thermosetting binders for aircraft floor panel materials (review). Trudy VIAM, 2019, no. 7 (79), paper no. 03. Available at: http://www.viam-works.ru (accessed: May 14, 2024). DOI: 10.18577/2307-6046-2019-0-7-26-33.
  19. Epocast 1618-D/B. Available at: https://freemansupply.com/products/liquid-tooling-materials/epoxy-aerospace-syntactics/epocast-1618-epoxy-syntactic (accessed: May 14, 2024).
  20. ITM25. Available at: https://itecma.ru/products/interernye-materialy/mats-pasty/15786/ (accessed: May 14, 2024).