Volkova E.F., Mostyaev I.V., Akinina M.V., Alikhanyan A.A. Studies of the regularities of the heat treatment influence on the structure, phase composition and mechanical properties of medium-sized forgings made of heat-resistant alloy of the Mg‒Zn‒Zr‒REE system // Proceedings of VIAM. 2024. No. 1 (131). Ст. 02. URL: https://www.viam-works.ru. DOI: 10.18577/2307-6046-2024-0-1-13-26.

Studies of the regularities of the heat treatment influence on the structure, phase composition and mechanical properties of medium-sized forgings made of heat-resistant alloy of the Mg‒Zn‒Zr‒REE system

Volkova E.F., Mostyaev I.V., Akinina M.V., Alikhanyan A.A.
Abstract

The paper presents the results of determining the mechanical properties, comparative research of the microstructure and phase composition of medium-sized forgings made of heat-resistant magnesium alloy of the Mg–Zn–Zr–REE system in non-heat-treated and aged states. It was founded that the anisotropy of the main mechanical properties of forgings does not exceed 7–12,5 % in the longitudinal, transverse and altitude directions in all studied states. The highest and most stable level of properties is characteristic of the non-heat-treatedt state in the longitudinal direction. A special feature is the reduction of strength properties during aging by 5–8 %.

Keywords
wrought magnesium alloy, aging, mechanical properties, microstructure, phase composition, small anisotropy of properties, negative aging effect
Reference list
  1. Nicholas A., Rylnik S. Application of magnesium components in the aerospace industry. Aerokosmicheskiy kuryer, 2011, no. 1, pp. 42–44.
  2. Kozlov I.A., Vinogradov S.S., Tarasova K.G., Kulyushina N.V., Manchenko V.A. Plasma electrolytic oxidation of magnesium alloys (review). Aviacionnye materialy i tehnologii, 2019, no. 1 (54), pp. 23–36. DOI: 10.18577/2071-9140-2019-0-1-23-36.
  3. Kablov E.N. Main results and directions of development of materials for advanced aviation technology. 75 years. Aviation materials. Moscow: VIAM, 2007, pp. 20–26.
  4. Kablov E.N. New generation materials – the basis of innovation, technological leadership and national security of Russia. Intellekt i tekhnologii, 2016, no. 2 (14), pp. 16–21.
  5. Agnew S.R. Wrought magnesium: A 21st century outlook. JOM: the journal of the Minerals, Metals & Materials Society, 2004, vol. 56 (5), pр. 20–21.
  6. Akinina M.V., Mostyaev I.V., Volkova E.F., Alikhanyan A.A. Comparative studies of the structure, features of the phase composition and mechanical properties of deformed semi-finished products from VMD16 magnesium alloy. Aviation materials and technologies, 2022, no. 4 (69), paper no. 04. Available at: http://www.journal.viam.ru (accessed: September 17, 2023). DOI: 10.18577/2713-0193-2022-0-4-36-50.
  7. Akinina M.V., Mostyaev I.V., Volkova E.F., Alikhanyan A.A. Investigation of the influence of alloying elements on the temperature threshold of ignition and fire resistance of a VMD16 wrought magnesium alloy. Aviation materials and technologies, 2022, no. 3 (68), paper no. 06. Available at: http://www.journal.viam.ru (accessed: September 18, 2023). DOI: 10.18577/2713-0193-2022-0-3-60-74.
  8. Song J., She J., Chen D., Pan F. Latest research advances on magnesium and magnesium alloys worldwide. Journal of Magnesium Alloys, 2020, vol. 8, pр. 1–41.
  9. Hagihara K., Yokotani N., Umakoshi Y. Plastic deformation behavior of Mg12YZn with 18R long-period stacking ordered structure. Intermetallics, 2010, vol. 18, pр. 267–276.
  10. Gao J.J., Fu J., Zhang N., Chen Y.A. Structural features and mechanical properties of Mg–Y–Zn–Sn alloys with varied LPSO phases. Journal of Alloys and Compounds, 2018, vol. 768, pр. 1029–1038.
  11. Negishi Y., Nishimura T., Iwasawa S. et al. Aging and tensile properties of Mg–Gd–Nd–Zr and Mg–Dy–Nd–Zr alloys. Journal of Japan Institute of Light Metals, 1994, vol. 44 (10), pр. 555–561.
  12. Hagihara K., Okamoto T., Yamasaki M. et al. Electron backscatter diffraction pattern analysis of the deformation band formed in the Mg-based long-period stacking ordered phase. Scripta Materialia, 2016, vol. 117, pр. 32–36.
  13. Yamasaki M., Hagihara K., Inoue S. et al. Crystallographic classification of kink bands in an extruded Mg–Zn–Y alloy using intragranular misorientaion axis analysis. Acta Materialia, 2013, vol. 61, pр. 2065–2076.
  14. Kawamura Y., Yamasaki M. Formation and Mechanical Properties of Mg97Zn1RE2 Alloys with Long-Period Stacking Ordered Structure. Materials Transactions, 2007, vol. 48 (11), pр. 2986–2992.
  15. Volkova E.F., Rokhlin L.L., Ovsyannikov B.V. Modern deformable magnesium alloys: state and prospects for use in high-tech industries: textbook. Ed. E.N. Kablov. Moscow: VIAM, 2021, 392 p.
  16. Zheng K.Y., Dong J., Zeng X.Q., Ding W.J. Effect of precipitation aging on the fracture behavior of Mg‒11Gd‒2Nd‒0.4Zr cast alloy. Materials Science and Engineering, 2008, vol. 489 (1–2), pр. 44–54.
  17. Wang H.Y., Rong J., Yu Z.Y. et al. Tensile properties, texture evolutions and deformation anisotropy of asextruded Mg‒6Zn‒1Zr magnesium alloy at room and elevated temperatures. Materials Science and Engineering. A, 2017, vol. 697, article 149e157.
  18. Hagihara K., Kinoshita A., Sugino Y. et al. Effect of long-period stacking ordered phase on mechanical properties of Mg97Zn1Y2 extruded alloy. Acta Materialia, 2010, vol. 58, pр. 6282–6293.
  19. Erasov V.S., Oreshko E.I., Lutsenko A.N. Multilevel large-scale complex research of deformation of metal materials. Aviation materials and technologies, 2022, no. 1 (66), paper no. 11. Available at: http://www.journal.viam.ru (accessed: September 18, 2023). DOI: 10.18577/2713-0193-2022-0-1-129-142.
  20. Kablov E.N. Innovative developments of FSUE «VIAM» SSC of RF on realization of «Strategic directions of the development of materials and technologies of their processing for the period until 2030». Aviacionnye materialy i tehnologii, 2015, no. 1 (34), pp. 3–33. DOI: 10.18577/2071-9140-2015-0-1-3-33.
  21. Zamaraeva Yu.V., Loginov Yu.N., Proydakova L.A. Properties of a hot-pressed profile made of MA14 magnesium alloy, obtained under production conditions. Sfera glubokoy pererabotki alyuminiya, 2023, no. 2, pp. 28–31.