Aleksandrov D.A., Doronin O.N., Juravleva P.L., Benklyan A.S. The research of erosion-corrosion-resistant coatings for protection of titanium impellers for helicopter gas-turbine engine // Proceedings of VIAM. 2023. No. 9 (127). Ст. 08. URL: https://www.viam-works.ru. DOI: 10.18577/2307-6046-2023-0-9-90-100.

The research of erosion-corrosion-resistant coatings for protection of titanium impellers for helicopter gas-turbine engine

Aleksandrov D.A., Doronin O.N., Juravleva P.L., Benklyan A.S.
Abstract

The erosion-corrosion-resistant coatings applicable to protect impellers of a gas-turbine engine compressor made of titanium alloys are studied. The properties of promising systems of ion-plasma coatings are studied: (TiN–CrN), TiN/Ti/TiN, (TiN–Ti–Al–Cr–N)–TiN. Erosion and corrosion resistance tests were carried out, residual stresses in the coating were investigated, high-cycle fatigue tests and metallographic studies were carried out. The influence of the thickness and design of coatings on the erosion and corrosion resistance of titanium alloys, the endurance limit has been established.

Keywords
erosion resistance, residual stresses, ion-plasma coatings, titanium nitride, multilayer coatings
Reference list
  1. Kablov E.N., Kashapov O.S., Pavlova T.V., Nochovnaya N.A. Development of a pilot industrial technology for the manufacture of semi-finished products from pseudo-alpha-titanium alloy VT41. Titan, 2016, no. 2 (52), pp. 33–42.
  2. Kablov E.N., Kashapov O.S., Medvedev P.N., Pavlova T.V. Study of a α + β-titanium alloy based on a system of Ti–Al–Sn–Zr–Si–β-stabilizing alloying elements. Aviacionnye materialy i tehnologii, 2020, no. 1 (58), pp. 30–37. DOI: 10.18577/2071-9140-2020-0-1-30-37.
  3. Kablov E.N., Muboyadzhyan S.A. Erosion-resistant coatings for gas turbine engine compressor blades. Russian metallurgy (Metally), 2017, vol. 2017, no. 6, pp. 494–504.
  4. Muboyadzhyan S.A. Erosion-resistant coatings for GTE compressor blades. Metally, 2009, no. 3, pp. 3–20.
  5. Uglov V.V., Prikhodko Zh.L., Khodasevich V.V., Prikhodko I.I., Eizner A.B. Influence of the composition on the mechanical properties of coatings formed by the method of condensation with ion bombardment. Fizika i khimiya obrabotki materialov, 2003, no. 5, pp. 48–52.
  6. Jianliang L., Xuhai Z., Fangfang G. et al. Thick CrN/AlN superlattice coatings deposited by hot filament assisted HiPIMS for solid particle erosion and high temperature wear resistance. Surface & Coatings Technology, 2019, no. 377, pp. 124922–124933. Available at: http://www.elsevier.com/locate/surfcoat (дата обращения: 22.05.2023). DOI: 10.1016/j.surfcoat.2019.124922.
  7. Imamutdinov V.E., Veksler Yu.V., Styazhkin V.A. Erosion-heat-resistant coating for protection of compressor rotor parts. Konstruktsii iz kompozitsionnykh materialov, 2006, no. 4, pp. 228–230
  8. Grzesik W., Malecka J., Kwasny W. Identification of oxidation process of TiAlN coatings versus heat resistant aerospace alloys based on diffusion couples and tool wear tests. CIRP Annals – Manufacturing Technology, 2020, no. 69, pp. 41–44. DOI: 10.1016/j.cirp.2020.04.024.
  9. Zhang M., Cheng Y., Xin L. et al. Cyclic oxidation behaviour of Ti/TiAlN composite multilayer coatings deposited on titanium alloy. Corrosion Science, 2020, no. 166, pp. 108476–108486. DOI: 10.1016/j.corsci.2020.108476.
  10. Alexandrov D.A., Gorlov D.S. The Research of erosion resistance and residual stresses in layered ion-plasma coatings. Trudy VIAM, 2022, no. 12 (118), paper no. 08. Available at: http://www.viam-works.ru (accessed: May 22, 2023). DOI: 10.18577/2307-6046-2022-0-12-87-95.
  11. Duyunova V.A., Oglodkov M.S., Gerasimov M.V., Kozlov I.A., Knyazev A.V. Features of formation of electrolyte-plasma coatings from nickel-containing electrolytes on titanium alloys. Trudy VIAM, 2021, no. 7 (101), paper no. 09. Available at: http://www.viam-works.ru (accessed: May 22, 2023). DOI: 10.18577/2307-6046-2021-0-7-86-94.
  12. Zavarzin S.V., Duyunova V.A., Fomina M.A. High-temperature corrosion of titanium alloys (review). Trudy VIAM, 2023, no. 2 (122), paper no. 03. Available at: http://www.viam-works.ru (accessed: May, 22 2023). DOI: 10.18577/2307-6046-2023-0-4-27-39.
  13. Alexandrov D.A., Gorlov D.S., Budinovskii S.A. Application of a complex of ion-plasma technologies to protect the compressor blades of a helicopter gas-turbine engine from erosion wear and fretting. Trudy VIAM, 2021, no. 2 (96), paper no. 08. Available at: http://www.viam-works.ru (accessed: May, 22 2023). DOI: 10.18577/2307-6046-2021-0-2-71-80.
  14. Vereschaka A.A., Grigoriev S.N. Study of cracking mechanisms in multi-layered composite nanostructured coatings. Wear, 2017, no. 378–379, pp. 43–57. DOI: 10.1016/j.wear.2017.01.101.
  15. Tillmann W., Grisales D., Stangier D. et al. Residual stresses and tribomechanical behaviour of TiAlN and TiAlCN monolayer and multilayer coatings by DCMS and HiPIMS. Surface & Coatings Technology, 2021, no. 406, pp. 126664–126675. DOI: 10.1016/j.surfcoat.2020.126664.
  16. Xu Y.X., Riedl H., Holec D. et al. Thermal stability and oxidation resistance of sputtered Ti–Al–Cr–N hard coatings. Surface & Coatings Technology, 2017, no. 324, pp. 48–56. DOI: 10.1016/j.surfcoat.2017.05.053.
  17. Asanuma H., Polcik P., Kolozsvari S. et al. Cerium doping of Ti–Al–N coatings for excellent thermal stability and oxidation resistance. Surface & Coatings Technology, 2017, no. 326, pp. 165–172. DOI: 10.1016/j.surfcoat.2017.07.037.
  18. Sui X., Li G., Zhou H. et al. Evolution behavior of oxide scales of TiAlCrN coatings at high temperature. Surface & Coatings Technology, 2019, no. 360, pp. 133–139. DOI: 10.1016/j.surfcoat.2019.01.016.
  19. Peskova A.V., Sukhov D.I., Mazalov P.B. Exami-nation of the formation of the titanium alloy VT6 structure obtained by additive manufacturing. Aviacionnye materialy i tehnologii, 2020, no. 1 (58), pp. 38–44. DOI: 10.18577/2071-9140-2020-0-1-38-44.