Yashin M.S., Kapitanenko D.V. Investigation of the structure and properties of the VT3-1 alloy in relation to the technology for obtaining stampings of disks and turbine blades // Proceedings of VIAM. 2023. No. 8 (126). Ст. 05. URL: https://www.viam-works.ru. DOI: 10.18577/2307-6046-2023-0-8-52-63.

Investigation of the structure and properties of the VT3-1 alloy in relation to the technology for obtaining stampings of disks and turbine blades

Yashin M.S., Kapitanenko D.V.
Abstract

Рroperties and structure of forgings made of titanium alloy VT3-1, obtained by isothermal deformation under the conditions of the National Research Center «Kurchatov Institute» – VIAM presented in present paper. The draft was carried out according to the scheme of blades with a degree of deformation of 60 % and according to the scheme of disks with a degree of deformation of 80 %. The forgings were subjected to low-temperature, isothermal and double annealing. It has been investigated that the VT3-1 alloy has a high technological plasticity in the temperature range below the polymorphic transformation limit. Stampings show the required level of properties when deformed in the (α + β)-area.

Keywords
titanium, isothermal deformation, annealing, stamping, titanium heat resistant alloy VT3-1
Reference list
  1. Kablov E.N., Putyrsky S.V., Yakovlev A.L., Krokhina V.A., Naprienko S.A. Investigation of resistance to fatigue failure of forgings from high-strength titanium alloy VT22M, manufactured with final deformation in (α + β)- and β-regions. Titan, 2021, no. 1 (70), pp. 26–33.
  2. Kablov E.N., Ospennikova O.G., Lomberg B.S. Complex innovative technology of isothermal punching on air in mode of superplasticity of disks from superhot strength alloys. Aviacionnye materialy i tehnologii, 2012, no. S, pp. 129–141.
  3. Kablov E.N., Bakradze M.M., Gromov V.I., Voznesenskaya N.M., Yakusheva N.A. New high strength structural and corrosion-resistant steels for aerospace equipment developed by FSUE «VIAM» (review). Aviacionnye materialy i tehnologii, 2020, no. 1 (58), pp. 3–11. DOI: 10.18577/2071-9140-2020-0-1-3-11.
  4. Nochovnaya N.A., Shiryaev A.A., Sharapkin D.S. Complex of mechanical and operational properties of rolled blanks from metastable-β-titanium alloy VT47. Aviation materials and technologies, 2022, no. 3 (68), paper no. 05. Available at: http://www.journal.viam.ru (accessed: May 16, 2023). DOI: 10.18577/2713-0193-2022-0-3-50-59.
  5. Ponomarenko D.A., Skugorev A.V., Sidorov S.A., Shpagin A.S. Influence of heat exchange between workpiece and die on forming process of aerospace parts by special isothermal presses). Trudy VIAM, 2016, no. 10, paper no. 3. Available at: http://www.viam-works.ru (accessed: May 12, 2023). DOI: 10.18577/2307-6046-2016-0-10-3-3.
  6. Razuvaev E.I., Moiseev N.V., Kapitanenko D.V., Bubnov M.V. Modern technologies of plastic working of metals. Trudy VIAM, 2015, no. 2, paper no. 03. Available at: http://www.viam-works.ru (accessed: May 12, 2023). DOI: 10.18577/2307-6046-2015-0-2-3-3.
  7. Putyrskij S.V., Arislanov A.A., Artemenko N.I., Yakovlev A.L. Different methods of wear resistance increase of titanium alloys and comparative analysis of their efficiency for VT23M titanium alloy. Aviacionnye materialy i tehnologii, 2018, no. 1, pp. 19–24. DOI: 10.18577/2071-9240-2018-0-1-19-24.
  8. Moiseev N.V., Razuvaev E.I. Formation of a recrystallized structure in deformed semi-finished products from titanium alloys of a transitional class, obtained by isothermal stamping. Metallovedeniye i termicheskaya obrabotka metallov, 2002, no. 7, pp. 43–47.
  9. Egorova Yu.B., Davydenko L.V., Belova S.B., Chibisova E.V. Prediction of the mechanical properties of forgings from titanium alloys VT6 and VT3-1 depending on the chemical composition and structure. Izvestiya vuzov. Tsvetnaya metallurgiya, 2018, no. 1, pp. 12–21.
  10. Burgonova O.Yu., Pantyukhova K.N., Belozerova E.P. Determination of the rational mode of heat treatment of the VT3-1 alloy to increase plasticity before pressure treatment. Omskiy nauchnyy vestnik, 2017, no. 3 (153), pp. 44–48.
  11. Skugorev A.V., Kapitanenko D.V., Shishkov S.Yu., Melnikova D.A. Formation of the structure and mechanical properties of high-alloy titanium alloys during isothermal forging in air. Titan, 2021, no. 3 (72), pp. 34–40.
  12. Golovkin S.A., Pervov M.L., Vozdvizhenskaya M.V., Skobeleva A.S. Isothermal stamping of precision blanks of gas turbine engine blades for dimensionless processing of the airfoil profile. Zagotovitelnye proizvodstva v mashinostroyenii (kuznechno-pressovoye, liteynoye i drugiye proizvodstva), 2016, no. 10, pp. 24–27.
  13. Yakovlev A.L., Arislanov A.A., Putyrsky S.V., Nochovnaya N.A. Study of mechanical properties and structure of large-sized semi-finished products made of VT6ch titanium alloy. Aviacionnye materialy i tehnologii, 2020, no. 4 (61), pp. 12–18. DOI: 10.18577/2071-9140-2020-0-4-12-18.
  14. Kablov E.N. Innovative developments of FSUE «VIAM» SSC of RF on realization of «Strategic directions of the development of materials and technologies of their processing for the period until 2030». Aviacionnye materialy i tehnologii, 2015, no. 1 (34), pp. 3–33. DOI: 10.18577/2071-9140-2015-0-1-3-33.
  15. Dzunovich D.A., Lukina E.A., Yakovlev A.L. Influence of heat treatment parameters on producibility and mechanical properties of sheets made from high-strength titanium alloy VT23. Aviacionnye materialy i tehnologii, 2018, no. 3 (52), pp. 3–10. DOI: 10.18577/2071-9140-2018-0-3-3-10.
  16. Putyrskiy S.V., Yakovlev A.L., Nochovnaya N.A., Krokhina V.A. Research of different heat treatment modes influence on properties of semi-finished products and welded joints from titanium alloy ВТ22М. Aviacionnye materialy i tehnologii, 2019, no. 1 (54), pp. 3–10. DOI: 10.18577/2071-9140-2019-0-1-3-10.