Petrushin N.V., Golinets S.A, Rimsha E.G., Ryzhkov P.V. Mechanical properties of corrosion-resistant nickel-based superalloy VZhL23 // Proceedings of VIAM. 2023. No. 8 (126). Ст. 01. URL: https://www.viam-works.ru. DOI: 10.18577/2307-6046-2023-0-8-3-12.

Mechanical properties of corrosion-resistant nickel-based superalloy VZhL23

Petrushin N.V., Golinets S.A, Rimsha E.G., Ryzhkov P.V.
Abstract

The results of experimental studies of short-term strength, long-term strength, multi-cycle fatigue and low-cycle fatigue of the castable corrosion-resistant nickel-based superalloy VZhL23 for turbine blades of GTI and GTE are presented.

Comparative analysis of the obtained values of long-term strength, multi-cycle fatigue and low-cycle fatigue of VZhL23 with the most heat-resistant foreign alloy IN-792 is carried out. It has been established that according to the set of mechanical properties VZhL23 is not inferior to IN-792.

Keywords
castable corrosion-resistant nickel-based superalloys, mechanical properties, microstructure, testing temperature, strength characteristics, fatigue
Reference list
  1. Getsov L.B. Materials and strength of gas turbines: in 2 books. Rybinsk: Gas turbine technologies, 2010, book 1, 605 p.
  2. Getsov L.B. Materials and strength of gas turbines: in 2 books. Rybinsk: Gas turbine technologies, 2011, books 2, 493 p.
  3. Logunov A.V. Heat-resistant nickel alloys for shoulder blades and disks of gas turbines. Rybinsk: Gas turbine technologies, 2017, 854 p.
  4. Superplanes II. Heat-resistant materials for aerospace and industrial power plants: in 2 book. Eds. Ch.T. Sims, N.S. Stoloff, U.K. Hagel; Moscow: Metallurgiya, 1995, book 2, 384 p.
  5. Kablov E.N. Materials of the new generation – the basis of innovation of technological leadership and national security of Russia // Intellekt i tekhnologii, 2016, no. 2 (14), pp. 16–21.
  6. Bazyleva O.A., Ospennikova O.G., Arginbaeva E.G., Letnikova E.Yu., Shestakov A.V. Development trends of nickel-based intermetallic alloys. Aviacionnye materialy i tehnologii, 2017, no. S, pp. 104–115. DOI: 10.18577/2071-9140-2017-0-S-104-115.
  7. Kablov E.N. Materials and technologies of the VIAM for the "Aviator" // Permskiye aviatsionnye dvigateli, 2014, no. 31, pp. 43–47.
  8. Gromov V.I., Yakusheva N.A., Vostrikov A.V., Cherkashneva N.N. High strength structural steels for gas-turbine engine shafts (review). Aviation materials and technology, 2021, no. 1 (62), paper no. 01. Available at: http://www.journal.viam.ru (accessed: December 06, 2022). DOI: 10.18577/2713-0193-2021-0-1-3-12.
  9. Kablov E.N. Innovative developments of FSUE «VIAM» SSC of RF on realization of «Strategic directions of the development of materials and technologies of their processing for the period until 2030». Aviacionnye materialy i tehnologii, 2015, no. 1 (34), pp. 3–33. DOI: 10.18577/2071-9140-2015-0-1-3-33.
  10. Foundry of a nickel-based heat-resistant alloy and a product made from it: pat. RU 2633679 C1; appl. 20.12.16; publ. 16.10.17.
  11. Gorbovets M.A., Hodinev I.A., Ryzhkov P.V. Low-cycle fatigue at high temperatures of heat-resistant nickel-based alloy manufactured by selective laser melting. Aviacionnye materialy i tehnologii, 2019, no. 4 (57), pp. 65–73. DOI: 10.18577/2071-9140-2019-0-4-65-73.
  12. Gorbovets M.A., Khodinev I.A., Monin S.A. Influence of average cycle stress on characteristics of low-cycle fatigue of high-temperature nickel alloy VZh175. Aviation materials and technologies, 2023, no. 1 (70), paper no. 10. Available at: http://www.journal.viam.ru (accessed: April 07, 2023). DOI: 10.18577/2713-0193-2023-0-1-126-136.
  13. Casting shoulder blades of gas turbine engines: alloys, technologies, coating. 2nd ed. Ed. E.N. Kablov. Moscow: Nauka, 2006, 632 p.
  14. Sidorov V.V., Kablov D.E., Rigin V.E. Metallurgy of foundry heat-resistant alloys: technology and equipment. Moscow: VIAM, 2016, 368 p.
  15. State Standard 10145–81. Metals. The method of testing long-term strength. Moscow: Publishing house of standards, 1981, 9 p.
  16. State Standard 3248–81. Metals. The testing method for creep. Moscow: Publishing house of standards, 1981, 11 p.
  17. State Standard 25.502–79. Methods of mechanical testing of metals. Fatigue test methods. Moscow: Publishing house of standards, 1986, 25 p.
  18. Solovyev A.E., Golynets S.A., Khvatsky K.K., Aslanyan I.R. Performing of static tensile tests on Zwick/Roell machines. Trudy VIAM, 2015, no. 8, paper no. 12. Available at: http://viam-works.ru (accessed: December 05, 2022).
  19. Shkolnik L.M. Forest test methodology: reference. Moscow: Metallurgiya, 1978, 304 p.
  20. Svetlov I.L., Petrushin N.V., Epishin A.I., Karashaew M.M., Elyutin E.S. Single crystals of nickel-based superalloys alloyed with rhenium and ruthenium (review). Part 1. Aviation materials and technologies, 2023, no. 1 (70), paper no. 03. Available at: http://www.journal.viam.ru (accessed: April 04, 2023). DOI: 10.18577/2713-0193-2023-0-1-30-50.
  21. Reed R.C. The Superalloys. Fundamentals and Applications. Cambridge: United Kingdom at University Press. 2006, 372 p.
  22. Kovpak V.I. Prediction of heat resistance of metal materials. Kyiv: Naukova Dumka, 1981, 240 p.
  23. Kablov E.N., Golubovsky E.R. The heat resistance of nickel alloys. Moscow: Mechanical Engineering, 1998, 463 p.
  24. Donachie M.J., Donachie S.J. Selection of superalloys for design // Mechanical Engineers Handbook. Third Ed. John Wiley & Sons, Inc, 2006, pp. 287–334.
  25. Du B., Yang J., Cui C., Sun X. Effects of grain size on the high-cycle fatigue behavior of IN792 superalloy // Materials & Design, 2015, vol. 65, pp. 57‒64. DOI: 10.1016/j.matdes.2014.08.059.
  26. Gorbovets M.A., Khodinev I.A., Karanov V.A., Yushin V.D. Influence of the type of loading on high-cycle fatigue of heat-resistant alloys. Trudy VIAM, 2019, no. 3 (75), paper no. 11. Available at: http://www.viam-works.ru (accessed: December 06, 2022). DOI: 10.18577/2307-6046-2019-0-3-96-104.
  27. Collins J. Damage to materials in structures. Analysis, prediction, prevention. Moscow: Mir, 1984, 624 p.