Chaykun A.М., Bobrova I.I., Gerasimov D.M. Elastomers for sealing harness materials: properties, methods of receiving and feature of manufacturing // Proceedings of VIAM. 2023. No. 7 (125). Ст. 05. URL: https://www.viam-works.ru. DOI: 10.18577/2307-6046-2023-0-7-56-68.

Elastomers for sealing harness materials: properties, methods of receiving and feature of manufacturing

Chaykun A.М., Bobrova I.I., Gerasimov D.M.
Abstract

Article is devoted to the analysis of the elastomeric materials which are widely applied to manufacturing of sealing harness, which used in technological process of vacuum infusion when manufacturing polymeric composite materials (PCM). The schematic circuit of manufacturing of elastomeric sealing harness is given. The main processes of production of sealing harness as length elastomeric materials are described. The rubbers which are of interest for manufacturing of elastomeric pressurizing plaits are described. Recommendations about application of rubbers on the basis of different rubbers as bases for manufacturing elastomeric sealing harness are made.

Keywords
silicon rubbers, butyl rubber, elastomer, infusion, methods of processing PCM, sealing harness
Reference list
  1. Kablov E.N. Innovative developments of FSUE «VIAM» SSC of RF on realization of «Strategic directions of the development of materials and technologies of their processing for the period until 2030». Aviacionnye materialy i tehnologii, 2015, no. 1 (34), pp. 3–33. DOI: 10.18577/2071-9140-2015-0-1-3-33.
  2. Kablov E.N. The role of chemistry in the creation of new generation materials for complex technical systems. XX Mendeleev Congress on General and Applied Chemistry: in 5 vols. Ekaterinburg: Ural Branch of the Russian Academy of Sciences, 2016, vol. 1, pp. 25–26.
  3. Kablov E.N. The sixth technological order. Nauka i zhizn, 2010, no. 4, pp. 2–7.
  4. History of aviation materials science. VIAM – 80 years: years and people. Ed. E.N. Kablov. Moscow: VIAM, 2012, pp. 346–348.
  5. Kablov E.N. Aerospace materials science. Vse materialy. Entsiklopedicheskiy spravochnik, 2008, no. 3, pp. 2–14.
  6. Kolpachkov E.D., Petrova A.P., Kurnosov A.O., Sokolov I.I. Methods of molding aviation products from PCM (review). Trudy VIAM, 2019, no. 11 (83), paper no. 03. Available at: http://www.viam-works.ru (accessed: March 03, 2023). DOI: 10.18577/2307-6046-2019-0-11-22-36.
  7. Raskutin A.E. Russian polymer composite materials of new generation, their exploitation and implementation in advanced developed constructions. Aviacionnye materialy i tehnologii, 2017, no. S, pp. 349–367. DOI: 10.18577/2071-9140-2017-0-S-349-367.
  8. Callister U., Ristic D. Materials science: from technology to application (metals, ceramics, polymers). St. Petersburg: Nauchnye osnovy i tekhnologii, 2011, 896 p.
  9. Rudd C.D., Long A.C., Kendall K.N., Mangin C.G.E. Liquid Moulding Technologies. Wood Head Publishing and SAE International, 1997, pp. 42–57.
  10. Kryzhanovsky V.K., Kerber M.L., Burlov V.V. Manufacture of products from polymeric materials. St. Petersburg: Professiya, 2004, 464 p.
  11. Tkachuk A.I., Donetsky K.I., Terekhov I.V., Karavaev R.Yu. The use of thermosetting matrices for the manufacture of polymer composite materials by the non-autoclave molding methods. Aviation materials and technology, 2021, no. 1 (62), paper no. 03. Available at: https://journal.viam.ru (accessed: March 03, 2023). DOI: 10.18577/2713-0193-2021-0-1-22-33.
  12. Mikhailin Yu.A. Structural polymeric composite materials. 2nd ed. St. Petersburg: Nauchnye osnovy i tekhnologii, 2016, 820 p.
  13. Duyunova V.A., Serebrennikova N.Yu., Nefedova Yu.N., Sidelnikov V.V., Somov A.V. Methods of forming metal-polymer composite materials (review). Aviation materials and technologies, 2022, no. 1 (66), paper no. 06. Available at: http://www.journal.viam.ru (ассеssed: March 09, 2023). DOI: 10.18577/2713-0193-2022-0-1-65-77.
  14. Slavin A.V., Donetskiy K.I., Khrulkov A.V. Prospects for the use of polymer composite materials in aircraft structures in 2025–2035 (review). Trudy VIAM, 2022, no. 11 (117), paper no. 08. Available at: http://www.viam-works.ru (accessed: March 09, 2023). DOI: 10.1877/2307-6046-2022-0-11-81-92.
  15. Donetskiy K.I., Usacheva M.N., Khrulkov A.V. Infusion methods for the manufacture of polymer composite materials (review). Part 1. Trudy VIAM, 2022, no. 6 (112), paper no. 06. Available at: http://www.viam-works.ru (accessed: March 09, 2023). DOI: 10118577/2307-6046-2022-0-6-58-67.
  16. Khrulkov A.V., Donetskiy K.I., Usacheva M.N., Goryansky A.N. Infusion methods for the manufacture of polymer composite materials (review). Part 2. Trudy VIAM, 2022, no. 6 (112), paper no. 05. Available at: http://www.viam-works.ru (accessed: March 09, 2023). DOI: 10.1877/2307-6046-2022-0-7-50-62.
  17. Belinis P.G., Donetskiy K.I., Lukyanenko Yu.V., Rogozhnikov V.N., Mayer Yu., Bystrikova D.V. Volume reinforcing solid-woven preforms for manufacturing of polymer composite materials (review). Aviacionnye materialy i tehnologii, 2019, no. 4 (57), pp. 18–26. DOI: 10.18577/2071-9140-2019-0-4-18-26.
  18. Vacuum injection process for manufacturing fiber reinforced composite products involves evacuating second chamber causing resin to flow into preform in adjacent evacuated first chamber: pat. 10013409 DE; appl. 17.03.00; publ. 23.04.00.
  19. A large reference book of rubber workers: at 2 parts. Moscow: Tekhinform, 2012, 1385 p.
  20. Technology of rubber: Formulation and testing: trans. from Engl. Ed. J.S. Dick. St. Petersburg: Nauchnye osnovy i tekhnologii, 2010, 620 p.
  21. Fedyukin D.P., Makhlis F.A. Technical and technological properties of rubbers. Moscow: Khimiya, 1985, 240 p.
  22. Makhlis F.A., Fedyukin D.L. Terminological guide to rubber. Moscow: Chemistry, 1989, 400 p.
  23. Kornev A.E., Bukanov A.M., Sheverdyaev O.N. Technology of elastomeric materials. Moscow: NPPA "Istek", 2009, 502 p.
  24. Agayants I.M. Five centuries of rubber and rubber. Moscow: Modern-A, 2002, 432 p.
  25. Koshelev F.F., Kornev A.E., Bukanov A.M. General rubber technology. 4th ed. Moscow: Khimiya, 1978, 528 p.
  26. Ososhnik I.A., Shutilin Yu.F., Karmanova O.V. Manufacture of rubber technical products. Ed. Yu.F. Shutilin. Voronezh: Voronezh State Tech. Acad., 2007, 972 p.
  27. Grishin B.S. Materials of the rubber industry (information-analytical database): in 2 vols. Kazan: KSTU, 2010, 1084 p.
  28. Rubber and resine. Science and technology: trans. from Engl. Ed. A.A. Berlin, Yu.L. Morozov. Dolgoprudny: Intellect, 2011, 768 p.
  29. Nudelman Z.N. Fluororubbers: basics, processing, application. Moscow: RIAS, 2007, 383 p.
  30. Lepetov V.A., Yurtsev L.N. Calculations and design of rubber products. 3rd ed., rev. and add. Leningrad: Khimiya, 1987, 406 p.
  31. Shetz M. Silicone rubber. Moscow: Khimiya, 1975, 400 p.