Shosheva A.L., Akhmadieva K.R., Valueva M.I., Nacharkina A.V. Bismaleimide resins (review). Part 2 // Proceedings of VIAM. 2023. No. 7 (125). Ст. 04. URL: https://www.viam-works.ru. DOI: 10.18577/2307-6046-2023-0-7-34-55.

Bismaleimide resins (review)

Part 2
Shosheva A.L., Akhmadieva K.R., Valueva M.I., Nacharkina A.V.
Abstract

The current paper is the second part of the scientific and technical review of bismaleimide (BMI) resins chemistry. Shows the modification of bismaleimide binders with epoxy resins, benzoxazines, cyanate esters and thermoplastics. The most significant physical and thermomechanical properties of polymer matrices based on modified bismaleimide resins and their main advantages are considered. Modern approaches to the synthesis and processing of heat-resistant bismaleimide resins are described.

Keywords
4, bismaleimide resins, heat-resistant polymers, 4'-bismaleimidodiphenylmethane, diallyl bisphenol A, epoxy resins, benzoxazine, cyanate esters, thermoplastics
Reference list
  1. Mukhametov R.R., Petrova A.P. Thermosetting binders for polymer composites (review). Aviacionnye materialy i tehnologii, 2019, no. 3 (56), pp. 48–58. DOI: 10.18577/2071-9140-2019-0-3-48-58.
  2. Stenzenberger H.D. Bismaleimide Resins. ASM Handbook. Ed. D.B. Miracle, S.L. Donaldson, 2001, vol. 21, pp. 97–104.
  3. Iredale R.J., Ward C., Hamerton I. Modern advances in bismaleimide resin technology: А 21st century perspective on the chemistry of addition polyimides. Progress in Polymer Science, 2017, vol. 69, pp. 1–21.
  4. Kablov E.N., Erofeev V.T., Zotkina M.M., Dergunova A.V., Moiseev V.V., Rimshin V.I. Plasticized epoxy composites for manufacturing of composite reinforcement. Journal of Physics: Conference Series «International Conference on Engineering Systems 2020». 2020, p. 012031.
  5. Valueva M.I., Zelenina I.V., Zharinov M.A., Akhmadieva K.R. World market of high temperature polyimide carbon plastic (review). Trudy VIAM, 2019, no. 12 (84), paper no. 08. Available at: http://www.viam-works.ru (accessed: December 10, 2022). DOI: 10.18577/2307-6046-2019-0-12-67-79.
  6. Evsyukov S.E., Pohlmann T., Wiel M. Modern approaches to the processing of bismaleimide resins. Current Trends in Polymer Science, 2020, vol. 20, pp. 2–14.
  7. Kablov E.N., Chursova L.V., Babin A.N., Mukhametov R.R., Panina N.N. Developments of FSUE "VIAM" in the field of melt binders for polymer composite materials. Polimernye materialy i tekhnologii, 2016, vol. 2, no. 2, pp. 37–42.
  8. Kablov E.N. Innovative developments of FSUE «VIAM» SSC of RF on realization of «Strategic directions of the development of materials and technologies of their processing for the period until 2030». Aviacionnye materialy i tehnologii, 2015, no. 1 (34), pp. 3–33. DOI: 10.18577/2071-9140-2015-0-1-3-33.
  9. Process for the Manufacture of Crosslinked Polymers which Contain Imide Groups: pat. US 4100140A; appl. 18.06.76; publ. 11.07.78.
  10. Shosheva A.L. Bismaleimide resins (review). Part 1. Trudy VIAM, 2022, no. 10 (116), paper no. 03. Available at: http://www.viam-works.ru (accessed: September December 15, 2022). DOI: 10.18577/2307-6046-2022-0-10-23-41.
  11. Park J.O., Jang S.H. Synthesis and Characterization of Bismaleimides from Epoxy Resins. Journal of Polymer Science, 1992, vol. 30, pp. 723–729.
  12. Kumar A.A., Lagar M.A., Rao R.M.V.G.K. Synthesis and characterization of siliconized epoxy-1,3-bis(maleimide)benzene intercrosslinked matrix materials. Polymer, 2002, vol. 43, pp. 693–702.
  13. Chattha M.S., Dickie R.A., Carduner K.R. Epoxy-modified diallylbisphenol A and bis(maleimidopheny1)methane thermoset compositions: composition and dynamic mechanical thermal analysis. Industrial  Engineering Chemistry Research, 1989, vol. 28, pp. 1438–1441.
  14. Kim D.S., Han M.J., Lee J.R. Cure Behavior and Properties of an Epoxy Resin Modified With a Bismaleimide Resin. Polymer Engineering and Science, 1995, vol. 35, pp. 1354–1357.
  15. Woo E.M., Chen L.B., Seferis J.C. Characterization of epoxy-bismaleimide network matrices. Journal of materials science, 1987, vol. 22, pp. 3665–3671.
  16. Chen Y., Wu Y., Geng C., Li Z., Dai G., Cui W. Curing Kinetics and the Properties of KH560-SiO2/Polyethersulfone/Bismaleimide-Phenolic Epoxy Resin Composite. Journal of Inorganic and Organometallic Polymers and Materials, 2019, vol. 30, pp. 1735–1743.
  17. Musto P., Martuscelli E., Ragosta G., Russo P., Scarinz G. An Interpenetrated System Based on a Tetrafunctional Epoxy Resin and a Thermosetting Bismaleimide: Structure – Properties Correlation. Journal of Applied Polymer Science, 1998, vol. 69, pp. 1029–1042.
  18. Seo J., Jang W., Ha H. Thermal Properties and Water Sorption Behaviors of Epoxy and Bismaleimide Composites. Macromolecular Research, 2007, vol. 15, pp. 10–16.
  19. Kumar A.A., Alagar M., Rao R.M.V.G.K. Preparation and Characterization of Siliconized Epoxy/Bismaleimide(N,N-Bismaleimido-4,4-diphenylmethane)Intercrosslinked Matrices for Engineering Applications. Journal of Applied Polymer Science, 2001, vol. 81, pp. 38–46.
  20. Gaina V., Gaina C. New Bismaleimide-Epoxy Resin System. Polymer-Plastics Technology and Engineering, 2009, vol. 48, pp. 525–529.
  21. Dolgova E.V., Lavrova K.S. Application of cyanate ester materials (review). Part 1. Aviation and space structures. Trudy VIAM, 2021, no. 4 (98), paper no. 04. Available at: http://www.viam-works.ru (accessed: December 23, 2022). DOI: 10.18577/2307-6046-2021-0-4-48-60.
  22. Nair C.P.R., Mathew D., Ninan K.N. Cyanate Ester Resins, Recent Developments. Advances in Polymer Science, 2001, vol. 155, p. 57.
  23. Domeier L.A., Gardner H.C. Bismaleimides and prepreg resins therefrom: pat. US 4691025A; appl. 22.12.83; publ. 01.09.87.
  24. Penczek P., Kaminska W. Polyfunctional Cyanate Monomers as Components of Polymer Systems. Advances in Polymer Sciences, 1990, vol. 97, pp. 48–49.
  25. Kessler M.R. Cyanate Ester Resins. Wiley Encyclopedia of Composites, Second Edition. John Wiley & Sons, 2012, pp. 1–9.
  26. Liu X., Yu Y., Li S. Study on cure reaction of the blends of bismaleimide and dicyanate ester. Polymer, 2006, vol. 47, pp. 3767–3773.
  27. Nair C.P.R., Francis T., Viayan T.M., Krishnan K. Sequential Interpenetrating Polymer Networks from Bisphenol A Based Cyanate Ester and Bimaleimide: Properties of the Neat Resin and Composites. Journal of Applied Polymer Science, 1999, vol. 74, pp. 2737–2746.
  28. Barton J.M., Humerton I., Jones J.R. The Synthesis, Characterisation and Thermal Behaviour of Functionalised Aryl Cyanate Ester Monomers. Polymer International, 1992, vol. 29, pp. 145–156.
  29. Hamerton I. High-performance thermoset–thermoset polymer blends: a review of the chemistry of cyanate ester-bismaleimide blends. High Performance Polymers, 1996, vol. 8, pp. 83–95.
  30. Chaplin A., Hamerton I., Herman H., Mudhar A.K., Shaw S.J. Studying water uptake effects in resins based on cyanate ester/bismaleimide blends. Polymer, 2000, vol. 41, pp. 3945–3956.
  31. Hamerton H., Herman H., Rees K.T., Chaplin A., Shaw S.J. Water uptake effects in resins based on alkenyl-modified cyanate ester–bismaleimide blends. Polymer International, 2001, vol. 50, pp. 475–483.
  32. Nair C.P.R., Francis T. Blends of Bisphenol A-Based Cyanate Ester and Bismaleimide: Cure and Thermal Characteristics. Journal of Applied Polymer Science, 1999, vol. 74, pp. 3365–3375.
  33. Lyu Y., Ishida H. Natural-sourced benzoxazine resins, homopolymers, blends and composites: A review of their synthesis, manufacturing and applications. Progress in Polymer Science, 2019, vol. 99, p. 101168.
  34. Kumar K.S.S., Nair C.P.R., Sadhana R., Ninan K.N. Benzoxazine–bismaleimide blends: Curing and thermal properties. European Polymer Journal, 2007, vol. 43, pp. 5084–5096.
  35. Kumar K.S.S., Nair C.P.R., Radhakrishnan T.S., Ninan K.N. Bis allyl benzoxazine: Synthesis, polymerization and polymer properties. European Polymer Journal, 2007, vol. 43, pp. 2504–2514.
  36. Wang Z. Zhao J., Ran Q. et al. Research on curing mechanism and thermal property of bisallyl benzoxazine and N,N′-(2,2,4-trimethylhexane-1,6-diyl) dimaleimide blend. ReactiveFunctional Polymers, 2013, vol. 73, pp. 668–673.
  37. Wang Y., Kou K., Zhuo L. et al. Thermal, mechanical and dielectric properties of BMI modified by the Bis allyl benzoxazine. Journal of Polymer Science, 2015, vol. 22, p. 51.
  38. Jin L., Agag T., Ishida H. Bis(benzoxazine-maleimide)s as a novel class of high performance resin: Synthesis and properties. European Polymer Journal, 2010, vol. 46, pp. 354–363.
  39. Jin J.Y., Cui J., Tang X.L., Ding Y.F., Li S.J., Wang J.C., Zhao Q.S., Hua X.Y., Cai X.Q. On polyetherimide modified bismaleimide resins, 1 Effect of the chemical backbone of polyetherimide. Macromolecular Chemistry and Physics, 1999, vol. 200, pp. 1956–1960.
  40. Jin J.Y., Cui J., Tang X.L. et al. Polyetherimide-modified bismaleimide resins. II. Effect of polyetherimide content. Journal of Applied Polymer Science, 2001, vol. 81, pp. 350–358.
  41. Wilkinson S.P., Ward T.C., McGrath J.E. Effect of thermoplastic modifier variables on toughening a bismaleimide matrix resin for high-performance composite materials. Polymer, 1993, vol. 34, pp. 870–884.
  42. Mai K., Huang J., Zeng H. Studies of the Stability of Thermoplastic-Modified Bismaleimide Resin. Journal of Applied Polymer Science, 1997, vol. 66, pp. 1965–1970.
  43. Liu X., Yu Y., Li S. Viscoelastic phase separation in polyethersulfone modified bismaleimide resin. European Polymer Journal, 2006, vol. 42, pp. 835–842.
  44. Hamerton I., Klewpatinond P. Synthesis and characterization of functionalized thermoplastics as reactive modifiers for bismaleimide resins. Polymer International, 2001, vol. 50, pp. 1309–1317.
  45. Mikhailin Yu.A. Heat-resistant polymers and polymeric materials. St. Petersburg: Professiya, 2006, 624 p.
  46. Chaplin A., Davies T.J., Jones D.A., Shaw S.J., Tudgey G.F. Novel hydrophobic, tough, and high temperature matrix resins for polymer composite. Plastics, Rubber and Composites, 1999, vol. 28, pp. 191–200.
  47. Liu X.Y., Zhan G.Z., Han Z.W. et al. Phase Morphology and Mechanical Properties of a Poly(ethersulfone)-Modified Bismaleimide Resin. Journal of Applied Polymer Science, 2007, vol. 106, pp. 77–83.
  48. Ding F., Chen Q., Lai S. Bismaleimide (BMI) Resin Modified by PEEK Bearing Pendant Reactive Propenyl Groups. Advanced Materials Research, 2011, vol. 197–198, pp. 1299–1305.
  49. Iijima T., Shiono H., Fukuda W., Tomoi M. Toughening of Bismaleimide Resin by Modification with Poly (ethylene phthalate) and Poly (ethylene phthalate-co-ethylene isophthalate ). Journal of Applied Polymer Science, 1998, vol. 65, pp. 1349–1357.
  50. Hu X., Zhang J., Yue C.Y., Zhao Q. Thermal and morphological properties of polyetherimide modified bismaleimide resins. High Perfomance Polymer, 2000, vol. 12, pp. 419–428.
  51. Babkin A.V., Erdni-Goryaev E.M., Solopchenko A.V. et al. Mechanical and thermal properties of modified bismaleimide matrices toughened by polyetherimides and polyimide. Polymers for Advanced Technologies, 2016, vol. 27, pp. 774–780.