Ermishev V.Yu., Laptev A.B., Startsev V.O. Peculiarities of assessing the resistance of polymeric materials to biodegradation in laboratory conditions. Part 1. Degradation of polymeric materials in natural environments, selection of bacterial strains, nutrient media and cultivation conditions // Proceedings of VIAM. 2023. No. 7 (125). Ст. 12. URL: https://www.viam-works.ru. DOI: 10.18577/2307-6046-2023-0-7-138-148.
Peculiarities of assessing the resistance of polymeric materials to biodegradation in laboratory conditions
Part 1. Degradation of polymeric materials in natural environments, selection of bacterial strains, nutrient media and cultivation conditions
Abstract
Describes the stages of biodegradation in the environment of synthetic hydrocarbons having a polymeric structure. Special attention is paid to the selection of bacterial strains and nutrient media for testing the relevant materials in the laboratory. The role of microorganisms in the production of enzyme preparations is shown, indicating the classes of enzymes that are functionally significant in the processes of destruction of materials. Information about the parameters and conditions of laboratory experiments involving bacterial strains, which are assumed to have a biodestructor phenotype, is presented.
Keywords
biodegradation, bacterial strains, nutrient media, synthetic polymeric materials, enzyme preparations, biotechnologies
Reference list
- Birbilis N., Cavanaugh M., Buchheit R. Electrochemical behavior and localized corrosion associated with Al7Cu2Fe particles in aluminum alloy 7075-T651. Corrosion Science, 2006, vol. 48, pp. 4202–4215. DOI: 10.1016/j.corsci.2006.02.007.
- Zhang B., Patlolla V.R., Chiao D. Galvanic corrosion of Al/Cu meshes with carbon fibers and graphene and ITO-based nanocomposite coatings as alternative approaches for lightning strikes. The International Journal of Advanced Manufacturing Technology, 2013, vol. 67, pp. 1317–1323. DOI: 10.1007/s00170-012-4568-3.
- Yoshida S., Hiraga K., Takehana T. et al. A bacterium that degrades and assimilates poly(ethylene terephthalate). Science, 2016, vol. 353, pp. 759–759. DOI: 10.1126/science.aad6359.
- Kablov E.N., Laptev A.B., Prokopenko A.N., Gulyaev A.I. Relaxation of polymeric composite materials under the prolonged action of static load and climate (review). Part 1. Binders. Aviation materials and technologies, 2021, no. 4 (65), paper no. 08. Available at: http://www.journal.viam.ru (accessed: March 29, 2023). DOI: 10.18577/2071-9140-2021-0-4-70-80.
- Kablov E.N. Materials of a new generation and digital technologies for their processing. Vestnik Rossiyskoy akademii nauk, 2020, vol. 90, no. 4, no. 331–334.
- Kablov E.N., Startsev V.O. Systematical analysis of the climatics influence on mechanical properties of the polymer composite materials based on domestic and foreign sources (review). Aviacionnye materialy i tehnologii, 2018, no. 2 (51), pp. 47–58. DOI: 10.18577/2071-9140-2018-0-2-47-58.
- Krivushina A.A., Terekhov I.V., Moskvitina K.N., Malysheva S.F., Kuimov V.A. Efficiency of new fungicide compounds based on modified polysept for protection of polymer materials against biodeterioration. Trudy VIAM, 2021, no. 12 (106), paper no. 12. Available at: http://www.viam-works.ru (accessed: March 13, 2023). DOI: 10.18577/2307-6046-2021-0-12-107-116.
- Otake Y., Kobayashi T., Asabe H. et al. Biodegradation of low-density polyethylene, polystyrene, polyvinyl chloride, and urea formaldehyde resin buried under soil for over 32 years. Journal Applied Polymer Science, 1995, vol. 56, pp. 1789–1796. DOI: 10.1002/app.1995.070561309.
- Mohanan N., Montazer Z., Sharma P.K., Levin D.B. Microbial and Enzymatic Degradation of Synthetic Plastics. Frontiers in Microbiology, 2020, vol. 11, pp. 1–22. DOI: 10.3389/fmicb.2020.580709.
- Ermishev V.Yu. Metabolic possibilities of bacteria with respect to synthetic hydro-carbons used in the production of non-metallic materials (review). Trudy VIAM, 2023, no. 2 (120), paper no. 11. Available at: http://www.viam-works.ru (accessed: February, 16 2023). DOI: 10.18577/2307-6046-2023-0-2-132-146.
- Ahmed T., Shahid M., Azeem F. Biodegradation of plastics: current scenario and prospects for environmental safety. Environmental Science and Pollution Research, 2018, vol. 25, pp. 7287–7298. DOI: 10.1007/s11356-018-1234-9.
- Ghosh S., Pal S., Ray S. Study of microbes having potentiality for biodegradation of plastics. Environmental Science and Pollution Research, 2013, vol. 20, pp. 4339–4355. DOI: 10.1007/s11356-013-1706.
- Sinha V., Patel M.R., Patel J.V. Pet Waste Management by Chemical Recycling: A Review. Journal Polymer Environment, 2010, vol. 18, pp. 8–25. DOI: 10.1007/s10924-008-0106-7.
- Sоrensen L., Groven A.S., Hovsbakken I.A. et al. UV degradation of natural and synthetic microfibers causes fragmentation and release of polymer degradation products and chemical additives. Science of The Total Environment, 2021, vol. 755, pp. 1–17. DOI: 10.1016/j.scitotenv.2020.143170.
- Eskander S., Saleh H. Biodegradation: Process Mechanism. Environmental Science and Engineering, 2017, vol. 8, pp. 1–31. DOI: 10.1007/978-3-030-83783-9_73-1.
- Gamage A., Liyanapathiranage A., Manamperi A. et al. Applications of Starch Biopolymers for a Sustainable Modern Agriculture. Sustainability, 2022, vol. 14, pp. 60–85. DOI: 10.3390/su14106085.
- Nishida H., Tokiwa Y. Distribution of poly(3-hydroxybutyrate) and polycaprolactone aerobic degrading microorganisms in different environments. Journal of Environment Polymer Degradation, 1993, vol. 1, pp. 227–233. DOI: 10.1007/BF01458031.
- Caballero K.P., Karel S.F., Register R.A. Biosynthesis, and characterization of hydroxybutyrate-hydroxycaproate copolymers. International journal of biological macromolecules, 1995, vol. 17, pp. 86–92. DOI: 10.1016/0141-8130(95)93522-y.
- Mohn W.W., Wilson A.E., Bicho P., Moore E.B. Physiological and Phylogenetic Diversity of Bacteria Growing on Resin Acids. Systematic and Applied Microbiology, 1999, vol. 22, pp. 68–78. DOI: 10.1016/S0723-2020(99)80029-0.
- Shadia M., Abdel A. Production and some properties of two chitosanases from Bacillus alvei. Journal Basic Microbiology, 1999, vol. 39, pp. 79–87. DOI: 10.1002/(SICI)1521-4028(199905)39:2.
- Corti A., Solaro R., Chiellini E. Biodegradation of poly(vinyl alcohol) in selected mixed microbial culture and relevant culture filtrate. Polymer Degradation and Stability, 2002, vol. 75, pp. 447–458. DOI: 10.1016/S0079-6700(02)00149-1.
- Stiles M., Holzapfel W. Lactic acid bacteria of foods and their current taxonomy. International Journal of Food Microbiology, 1997, vol. 36, pp. 1–29. DOI: 10.1016/S0168-1605(96)01233-0.
- Decker E.L., Reski R. Current achievements in the production of complex biopharmaceuticals with moss bioreactors. Bioprocess and Biosystems Engineering, 2008, vol. 31, pp. 3–9. DOI: 10.1007/s00449-007-0151-y.
- Schocken M.J., Gibson D.T. Bacterial oxidation of the polycyclic aromatic hydrocarbons acenaphthene and acenaphthylene. Applied Environmental Microbiology, 1984, vol. 48, pp. 10–16. DOI: 10.1128/aem.48.1.10-16.1984.
- Morozova O.V., Shumakovich G.P., Shleev S.V. Laccase–Mediator Systems and Their Applications: A Review. Applied Biochemistry and Microbiology, 2007, vol. 43, pp. 523–535. DOI: 10.1134/S0003683807050055.
- Rosales E., Rodríguez Couto S., Sanromán A. New uses of food waste: application to laccase production by Trametes hirsute. Biotechnology Letters, 2002, vol. 24, pp. 701–704. DOI: 10.1023/A:1015234100459.