Karavaev R.Y., Gorodilova N.A., Donetskiy K.I. Production of polymer composite materials based on semipregs // Proceedings of VIAM. 2023. No. 5 (123). Ст. 06. URL: https://www.viam-works.ru. DOI: 10.18577/2307-6046-2023-0-5-64-74.

Production of polymer composite materials based on semipregs

Karavaev R.Y., Gorodilova N.A., Donetskiy K.I.
Abstract

The features of manufacturing polymer composite materials (PCM) based on semipregs processed by vacuum molding are considered. The main approaches and requirements for binders, fillers and processes taking place during molding are established. Attention is drawn to the research carried out by foreign manufacturers of semipregs. Darcy's law is presented as the main postulate when carrying out the processes of impregnation of fillers with a binder. The properties of PCM based on semipregs made of equal-strength and unidirectional fabrics and epoxy melt binder developed by SIC «Kurchatov Institute» – VIAM are given.

Keywords
polymer composite materials, semipreg, resin, vacuum forming, curing, porosity, Darcy's law
Reference list
  1. History of aviation materials science: VIAM – 75 years of search, creativity, discoveries. Ed. E.N. Kablov. Mosccow: Nauka, 2007, 343 p.
  2. Terebenin B.P. Technological features of manufacturing large-sized products from fiberglass. Fiberglass and other structural plastics. Moscow: Oborongiz, 1960, 168 p.
  3. Gunyaev G.M. Design of high-modulus polymer composites. Moscow: Mashinostroenie, 1977, 159 p.
  4. Mikhailin Yu.A. Structural polymeric composite materials. St. Petersburg: Nauchnye osnovy i tekhnologii, 2008, 822 p.
  5. Brautman L. Destruction and fatigue. Moscow: Mir, 1978, 153 p.
  6. Donetskiy K.I., Karavaev R.Yu., Bystrikova D.V., Gracheva A.D. Сarbon fiber based on a volume-reinforcing braided preform for an element of a propeller blade. Trudy VIAM, 2022, no. 12 (118), paper no. 03. Available at: http://www.viam-works.ru (accessed: December 16, 2022). DOI: 10.18577/2307-6046-2022-0-12-27-38.
  7. Donetskiy K.I., Usacheva M.N., Khrulkov A.V. Infusion methods for the manufacture of polymer composite materials (review). Part 1. Trudy VIAM, 2022, no. 6 (112), paper no. 06. Available at: http://www.viam-works.ru (accessed: December 16, 2022). DOI: 10118577/2307-6046-2022-0-6-58-67.
  8. Donetskiy K.I., Karavayev R.YU., Raskutin A.Ye., Dun V.A. Carbon fibers composite material on the basis of volume reinforcing triax braiding preformes. Trudy VIAM, 2019, no. 1 (73), paper no. 07. Available at: http://viam-works.ru (accessed: December 16, 2022). DOI: 10.18577/2307-6046-2019-0-1-55-63.
  9. Donetskiy K.I., Bystrikova D.V., Karavaev R.Yu., Timoshkov P.N. Application of polymeric composite materials for creation of elements of transmissions of aviation engineering (review). Trudy VIAM, 2020, no. 3 (87), paper no. 09. Available at: http://www.viam-works.ru (accessed: December 16, 2022). DOI: 10.18577/2307-6046-2020-0-3-82-93.
  10. Ridgard C. Advances in Low Temperature Curing Prepregs for Aerospace Structures. Proc. SAMPE 2000 Conf. Long Beach: Society for the Advancement of Materials and Process Engineering, 2000, vol. 31, pp. 1–10.
  11. Ridgard C. Out of Autoclave Composite Technology for Aerospace. Defense and Space Structures. Proc. SAMPE 2009 Conf. Baltimore: Society for the Advancement of Materials and Process Engineering, 2009, vol. 54, pp. 1–13.
  12. Ridgard C. Next Generation Out of Autoclave Systems. Proc. SAMPE 2010 Conf. Seattle: Society for the Advancement of Materials and Process Engineering, 2010, vol. 33, pp. 1–18.
  13. Boyd J., Maskell R.K. Product Design for Low Cost Manufacturing of Composites for Aerospace Applications. Proc. SAMPE 2001 Conf. Long Beach: Society for the Advancement of Materials and Process Engineering, 2001, vol. 48, pp. 59–90.
  14. Repecka L., Boyd J. Vacuum-bag-only-curable prepregs that produce void-free parts. Proc. SAMPE 2002 Conf. Long Beach: Society for the Advancement of Materials and Process Engineering, 2002, vol. 47, pp. 1–13.
  15. Bond G.G., Griffith J.M., Hahn G.L. et al. Non-Autoclave Prepreg Manufacturing Technology. Proc. SAMPE 2008 Conf. Memphis: Society for the Advancement of Materials and Process Engineering, 2008, vol. 12, pp. 58–74.
  16. Kablov E.N. New Generation Materials and Technologies for Their Digital Processing. Herald of the Russian Academy of Sciences, 2020, vol. 90, no. 2, pp. 225–228.
  17. Kablov E.N. The role of fundamental research in the creation of new generation materials. Report XXI Mendeleev Congress on General and Applied Chemistry: in 6 vols. St. Petersburg, 2019, vol. 4, p. 24.
  18. Kablov E.N. Aviation materials science in the XXI century. Prospects and tasks. Aviation materials. Selected works of VIAM 1932–2002. Moscow: MISIS; VIAM, 2002, pp. 23–47.
  19. Gaskell D.R. An Introduction to Transport Phenomena in Materials Engineering. Macmillan Publishing Company, 1992, 687 p.
  20. Kratz J., Hubert P. Anisotropic air permeability in out-of-autoclave prepregs: Effect on honeycomb panel evacuation prior to cure. Composites. Part A: Applied Science and Manufacturing, 2013, vol. 49, pp. 179–191.
  21. Lee C.W., Gibson T., Tienda K.A., Storage T.M. Reaction Rate and Viscosity Model Development For Cytec s Cycom 5320 Family of Resins. Proc. SAMPE Tech.2010 Conf. Salt Lake City: Society for the Advancement of Materials and Process Engineering, 2010, vol. 6, pp. 1–15.
  22. Grunenfelder L.K., Nutt S.R. Prepreg age monitoring via differential scanning calorimetry. Journal of Reinforced Plastics and Composites, 2012, vol. 31, pp. 295–302.
  23. Kim D., Centea T., Nutt S.R. Out-Time Effects on Cure Kinetics and Viscosity for an Out-Of-Autoclave (OOA Prepreg: Modeling and Monitoring). Journal of Reinforced Plastics and Composites, 2014, vol. 100, pp. 63–69.
  24. Kratz J., Hsiao K., Fernlund G., Hubert P. Thermal models for MTM45-1 and Cycom 5320 out-of-autoclave prepreg resin. Journal of Composite Materials, 2012, vol. 47, pp. 341–352.
  25. Grunenfelder L.K., Nutt S.R. Out Time Effects on VBO Prepreg and Laminate Properties. Proc. SAMPE 2011 Conf. Long Beach: Society for the Advancement of Materials and Process Engineering, 2011, vol. 31, pp. 23–36.
  26. Centea T., Hubert P. Measuring the impregnation of an out-of-autoclave prepreg by micro-CT. Composites Science and Technology, 2011, vol. 71, pp. 593–599.
  27. Cender T.A., Simacek P., Advani S.G. Resin film impregnation in fabric prepregs with dual length scale permeability. Composites. Part A: Applied Science and Manufacturing, 2013, vol. 53, pp. 118–128.