Kuzmina N.A. Development of X-ray diffraction analysis in VIAM On the 130th anniversary of the birth of E.F. Bakhmetev, the first head of the X-ray laboratory of the institute // Proceedings of VIAM. 2023. No. 5 (123). Ст. 02. URL: https://www.viam-works.ru. DOI: 10.18577/2307-6046-2023-0-5-21-32.

Development of X-ray diffraction analysis in VIAM On the 130th anniversary of the birth of E.F. Bakhmetev, the first head of the X-ray laboratory of the institute

Kuzmina N.A.
Abstract

Presents the history of the development of х-ray diffraction analysis in VIAM in different periods of the institute's existence. The article describes the activities of the first head of the х-ray Laboratory, Evgeny Fedorovich Bakhmetev, an outstanding specialist in the field of х-ray structural research of metals and alloys, the founder and developer of the theory of metal recrystallization. The development of х-ray research equipment is traced in the historical context of the tasks of developing new materials and methods for controlling the structure of alloys.

Keywords
metal physics, biography, archival documents, All-Russian Research Institute of Aviation Materials
Reference list
  1. Bochvar A.A., Zhdanov G.S., Umansky Ya.S., Bakhmetev E.F. On the theory of recrystallization. Metal recrystallization. Moscow; Leningrad: Gosmashmetizdat, 1932, vol. II, is. 2, pp. 161–172
  2. Bakhmetev E.F., Kosolapov G.F. X-ray determination of the residual distortion of the atomic lattice in pressed duralumin. On the nature of structural changes during metal deformation at elevated temperatures. Moscow; Leningrad: Tsvetmetizdat, 1933, pp. 74–85.
  3. Bakhmetev E.F., Rovinsky B.M. Investigation of the thermal effect in duralumin during impact deformation. On the nature of structural changes during metal deformation at elevated temperatures. Moscow; Leningrad: Tsvetmetizdat, 1933, рр. 61–73.
  4. Trapeznikov A.K. X-ray study of the CuAl2 structure. Moscow; Leningrad: Sector of departmental and correspondence literature, 1934, 28 p.
  5. Kozhina N.K. To the method of X-ray analysis of duralumin recrystallization. Moscow; Leningrad: Gosmashmetizdat, 1934, 16 p.
  6. Bakhmetev E.F. X-ray determination of the structure of FeAl3. Moscow: ONTI NKTP USSR, 1935, 38 p.
  7. Logunov A.V., Petrushin N.V., Kuleshova E.A., Dolzhansky Yu.M. Predicting the influence of structural factors on the mechanical properties of heat-resistant alloys. Metallovedenie i termicheskaya obrabotka metallov, 1981, no. 6, pp. 16–20.
  8. Svetlov I.L., Sukhanov N.N., Krivko A.I. Temperature-orientational dependence of short-term strength characteristics, Young's modulus and coefficient of linear expansion of ZhS6F single crystals. Problemy prochnosti, 1987, no. 4, pp. 51–56.
  9. Krivko A.I., Epishin A.I., Svetlov I.L., Samoilov A.I. Elastic properties of single crystals of nickel alloys. Problemy prochnosti, 1988, no. 2, pp. 68–75.
  10. Chumakov V.A., Stepanov V.M., Ivanov V.G. et al. Casting technology for gas turbine engine blades using the method of directed crystallization. Liteynoe proizvodstvo, 1978, no. 1, pp. 23–24.
  11. Krivko A.I., Epishin A.I., Svetlov I.L., Samoilov A.I. Calculation of thermal stresses and thermal stability of anisotropic materials. Message II. Problemy prochnosti, 1989, no. 4, pp. 43–48.
  12. Treninkov I.A., Alekseev A.A., Zaitsev D.V., Filonova E.V. Researches of phase and structural changes, and also residual stresses in the course of high-temperature creep in VZhM4 alloy. Aviacionnye materialy i tehnologii, 2011, no. 2, pp. 11–19.
  13. Oglodkov M.S., Hohlatova L.B., Kolobnev N.I., Alekseev A.A., Lukina E.A. Influence of thermomechanical processing on properties and Al–Cu–Mg–Li–Zn system alloy structure. Aviacionnye materialy i tehnologii, 2010, no. 4, pp. 7–11.
  14. Treninkov I.A., Alekseev A.A., Polyakov S.N. Method of determination of residual stress in monocrystals of nickel superalloys using diffractometer of wide application with Cu Kβ-radiation. Aviacionnye materialy i tehnologii, 2010, no. 1, pp. 8–12.
  15. Kochubey A.Ya., Medvedev P.N. The use of direct pole figures in the study of structure formation processes during heating of deformed metals and alloys. Novosti materialovedeniya. Nauka i tekhnika, 2016, no. 5 (23), paper no. 2. Available at: http://www.materialsnews.ru (accessed: January 16, 2023).
  16. Medvedev P.N., Muboyadzhyan S.A. X-ray diffraction studies of electron beam ceramic thermal barrier coating layer based on ZrO2·Y2O3. Trudy VIAM, 2017, no. 1 (49), paper no. 03. Available at: http://www.viam-works.ru (accessed: January 16, 2023). DOI: 10.18577/2307-6046-2017-0-1-3-3.
  17. Naprienko S.A., Medvedev P.N., Raevskikh A.N., Popov M.A. Diffraction methods of research in the analysis of the plastic deformation zone under the fracture surface. Vestnik Moskovskogo gosudarstvennogo tekhnicheskogo universiteta im. N.E. Baumana. Ser.: Mashinostroyenie, 2019, no. 4 (127), pp. 97–110.
  18. Vasilev A.I., Panin P.V., Putyrskiy S.V., Rogalev A.M. Investigation of hot isostatic pressing and heat treatment effect on structure and mechanical properties of 3D-printed samples made from VT6-PS grade material. Trudy VIAM, 2021, no. 7 (101), paper no. 03. Available at: http://www.viam-works.ru (accessed: January 16, 2023). DOI: 10.18577/2307-6046-2021-0-7-22-30.
  19. Kolyadov E.V., Visik E.M., Gerasimov V.V., Arginbaeva E.G. The influence of directional solidification parameters on the structure and properties of the intermetallic alloys. Trudy VIAM, 2019, no. 3 (75), paper no. 02. Available at: http://www.viam-works.ru (accessed: October 16, 2022). DOI: 10.18577/2307-6046-2019-0-3-14-26.
  20. Zhitnyuk S.V., Medvedev P.N., Sorokin O.Yu., Kachaev A.A. Investigation of the crystallographic texture of corundum ceramics obtained by spark plasma sintering. Kristallografiya, 2022, vol. 67, no. 2, pp. 194–200.
  21. Kuzmina N.A., Ezubchenko S.N. Method for obtaining direct pole figures from single crystals of heat-resistant alloys. Metallurgiya mashinostroeniya, 2012, no. 3, pp. 33–34.
  22. Kuzmina N.A., Vasikova L.M. Influence of the sample rotation speed on the quality of the spectrum in determining the crystallographic orientation of single-crystal castings of heat-resistant alloys. Metallurgiya mashinostroeniya, 2009, no. 5, pp. 19–20.
  23. Kuzmina N.A., Lifshits V.A., Potrakhov E.N., Potrakhov N.N. Comparative structure control of single-crystal castings of nickel superalloys x-ray diffraction methods of oscillation and Laue. Trudy VIAM, 2019, no. 9 (81), paper no. 02. Available at: http://www.viam-works.ru (accessed: January 16, 2023). DOI: 10.18577/2307-6046-2019-0-9-15-25.
  24. Kuzmina N.A., Pyankova L.A. Control of crystallographic orientation of monocrystalline nickel castings heat-resistant alloys by х-ray diffractometry. Trudy VIAM, 2019, no. 12 (84), paper no. 02. Available at: http://www.viam-works.ru (accessed: October 12, 2022). DOI: 10.18577/2307-6046-2019-0-12-11-19.
  25. Kablov E.N., Bondarenko Yu.A., Kablov D.E. Features of structure and heat resisting properties of monocrystals of 001> high-rhenium nickel hot strength alloys received in the conditions of high-gradient directed crystallization. Aviacionnye materialy i tehnologii, 2011, no. 4, pp. 25–31.
  26. Bazyleva O.A., Bondarenko Yu.A., Timofeeva O.B., Chabina E.B. Intermetallic compositions based on Ni3Al alloyed with rhenium. Metallurgiya mashinostroeniya, 2011, no. 4, pp. 30–34.
  27. Bondarenko Yu.A., Echin A.B., Surova V.A., Narsky A.R. About the directed crystallization of heat-resistant alloys with the use of a cooler. Liteynoe proizvodstvo, 2011, no. 5, pp. 36–39.
  28. Bondarenko Yu.A., Bazyleva O.A., Echin A.B., Surova V.A., Narsky A.R. High-gradient directional crystallization of parts from alloy VKNA-1V. Liteynoe proizvodstvo, 2012, no. 6, pp. 12–16.
  29. Bazyleva O.A., Bondarenko Yu.A., Timofeeva O.B., Khvatsky K.K. Influence of crystallographic orientation on the structure and properties of the VKNA-1V alloy. Metallurgiya mashinostroeniya, 2012, no. 4, pp. 8–12.
  30. Bondarenko Yu.A., Echin A.B., Surova V.A., Narsky A.R. Influence of directional crystallization conditions on the structure of GTE blade-type parts. Liteynoe proizvodstvo, 2012, no. 7, pp. 14–16.
  31. Kuzmina N.A., Ezubchenko S.N. Method for obtaining direct pole figures from single crystals of heat-resistant alloys. Metallurgiya mashinostroyeniya, 2012, no. 3, pp. 33–34.
  32. History of aviation materials science. VIAM – 80 years: years and people. Ed. E.N. Kablov. Moscow: VIAM, 2012, 520 p.