Dikov I.A., Yakovleva S.I., Boychuk A.S., Chertishchev V.Yu. Defect classification for 2D fiber-reinforced composites (review) // Proceedings of VIAM. 2023. No. 3 (121). Ст. 07. URL: https://www.viam-works.ru. DOI: 10.18577/2307-6046-2023-0-3-67-83.

Defect classification for 2D fiber-reinforced composites (review)

Dikov I.A., Yakovleva S.I., Boychuk A.S., Chertishchev V.Yu.
Abstract

Up-to-date native and foreign regulatory and technical documents and scientific publications which are dedicated to the subject of fiber-reinforced composites’ defect classification and definition are observed at this article. The review of the most common defects of fiber reinforced plastics was made. The differences in terms of translation in regulatory and technical documents and scientific publications are shown. The variants of defect classification for 2D fiber-reinforced composites based on their common features and publications and documents’ areas of knowledge are observed. Data for non-destructive testing techniques which are recommended for different defects detection are given.

Keywords
defect, FRP, delamination, crack, inclusion, disbond, porosity, impact damage, wrinkle, nondestructive testing
Reference list
  1. History of aviation materials science. VIAM – 75 years of search, creativity, discoveries. Ed. E.N. Kablov. Moscow: Nauka, 2007, 343 p.
  2. Kablov E.N. Materials of the new generation – the basis of innovation, technological leadership and national security of Russia. Intellekt i tekhnologii, 2016, no. 2 (14), pp. 16–21.
  3. Tkachuk A.I., Donetsky K.I., Terekhov I.V., Karavaev R.Yu. The use of thermosetting matrices for the manufacture of polymer composite materials by the non-autoclave molding methods. Aviation materials and technology, 2021. no. 1 (62), paper no. 03. Available at: https://journal.viam.ru (accessed: September 26, 2022). DOI: 10.18577/2713-0193-2021-0-1-22-33.
  4. Gunyaeva A.G., Sidorina A.I., Kurnosov A.O., Klimenko O.N. Polymeric composite materials of new generation on the basis of binder VSE-1212 and the filling agents alternative to ones of Porcher Ind. and Toho Tenax. Aviacionnye materialy i tehnologii, 2018, no. 3 (52), pp. 18–26. DOI: 10.18577/2071-9140-2018-0-3-18-26.
  5. Mukhametov R.R., Petrova A.P. Thermosetting binders for polymer composites (review). Aviacionnye materialy i tehnologii, 2019, no. 3 (56), pp. 48–58. DOI: 10.18577/2071-9140-2019-0-3-48-58.
  6. Murashov V.V. Control and diagnostics of multilayer structures made of polymeric composite materials by acoustic methods: monograph. Moscow: Spektr, 2016, 244 p.
  7. Kablov E.N. Innovative developments of FSUE «VIAM» SSC of RF on realization of «Strategic directions of the development of materials and technologies of their processing for the period until 2030». Aviacionnye materialy i tehnologii, 2015, no. 1 (34), pp. 3–33. DOI: 10.18577/2071-9140-2015-0-1-3-33.
  8. State Standard 15467–79. Product quality management. Basic concepts. Terms and Definitions. Moscow: Standartinform, 2009, 25 p.
  9. State Standard 32794–2014. Polymer composites. Terms and Definitions. Moscow: Standartinform, 2015, 98 p.
  10. State Standard R 56787–2015. Polymer composites. Unbrakable control. Moscow: Standartinform, 2016, 71 p.
  11. ASTM Е2533-09. Standard Guide for Nondestructive Testing of Polymer Matrix Composites Used in Aerospace Applications. ASTM International, 2009, 47 p.
  12. State Standard R 56975–2016. Polymer composites. Indicators of the appearance of products from multilayer glass composites. Мoscow: Standartinform, 2016, 35 p.
  13. ASTM D2563-08. Standard Practice for Classifying Visual Defects in Glass-Reinforced Plastic Laminate Parts. ASTM International, 2008, 24 p.
  14. SAE ARP5089. Composite Repair NTD/NDI Handbook. SAE International, 2011, 98 p. DOI: 10.4271/ARP5089.
  15. ASTM D3878-07. Standard Terminology for Composite Materials. ASTM International, 2007, 5 p.
  16. Murashov V.V., Rumyantsev A.F. Defects in monolithic parts and multilayer structures made of polymer composite materials and methods for their detection. Part 1. Defects in monolithic parts and multilayer structures made of polymer composite materials. Kontrol. Diagnostika, 2007, no. 4, pp. 23–32.
  17. Murashov V.V., Rumyantsev A.F. Defects in monolithic parts and multilayer structures made of polymer composite materials and methods for their detection. Part 2. Methods for detecting defects in monolithic parts and multilayer structures made of polymer composite materials. Kontrol. Diagnostika, 2007, no. 5, pp. 31–42.
  18. Kartashova E.D., Muizemnek A.Yu. Technological defects of polymeric layered composite materials. Izvestiya vysshikh uchebnykh zavedeniy. Povolzhskiy region. Tekhnicheskie nauki, 2017, no. 2 (42), pp. 79–89. DOI: 10.21685/2072-3059-2017-2-7.
  19. Kulikov V.V., Petrova A.P. Analysis of types of defects in adhesive joints of aviation equipment and their repair. Klei. Germetiki. Tekhnologii, 2011, no. 5, pp. 24–27.
  20. Features of non-destructive testing of composite materials by low-frequency acoustic methods. Control. Measurement. Diagnostics. Available at: http://defectoscop.ru/page19.html (дата обращения: 26.09.2022).
  21. Azmah Hanim M.A., Brabazon D., Hashmi M.S.J. Cracks, microcracks, and fracture toughness of polymer composites: formation, testing method, nondestructive detection, and modifications. Failure Analysis in Biocomposites, Fibre-Reinforced Composites and Hybrid Composites. Woodhead Publishing, 2019, рр. 157–180. DOI: 10.1016/B978-0-08-102293-1.00008-5.
  22. Ivanov V.I., Belov P.A., Nasibullin T.S. Defects in composite materials as a source of acoustic emission. Znanie, 2016, no. 3–2 (32), pp. 23–29.
  23. Smith R.A. Use of 3D ultrasound data sets to map the localised properties of fibre-reinforced composites: PhD thesis. University of Nottingham, 2010. Available at: http://eprints.nottingham.ac.uk/31253/1/Full%20Thesis%20Chapters%20%282%29.pdf (accessed: September 26, 2022).
  24. Rivin G.L. Repair of structures made of polymer composite materials for aircraft: textbook. Ulyanovsk: UlGTU, 2000, 75 p.
  25. Saboktakin A. 3D textile preforms and composites for aircraft structures: a review. International Journal of Aviation, Aeronautics, and Aerospace, 2019, vol. 6, is. 1, art. 2. рр. 1–41. DOI: 10.15394/ijaaa.2019.1299.
  26. Katunin A., Dragan K., Dziendzikowski M. Damage identification in aircraft composite structures: A case study using various non-destructive testing techniques. Composite Structures, 2015, vol. 127, pp. 1–9. DOI: 10.1016/j.compstruct.2015.02.080.
  27. Practical Applications «New» NDT Techniques on Composite Material in the Aerospace Industry. 2014. Available at: http://ndt.aero/images/Presentation_26_Nov_2014.pdf (accessed: September 26, 2022).
  28. Ning W. Structural Health Condition Monitoring of Carbon-Fibre Based Composite Materials Using Acoustic Emission Techniques: Thesis M. Sc. University of Birmingham, 2015. Available at: https://core.ac.uk/download/pdf/33528371.pdf (accessed: September 26, 2022).
  29. Gaidachuk A.V., Kondratiev A.V., Omelchenko E.V. Analysis of technological defects arising in the serial production of integral aircraft structures from polymer composite materials. Aviatsionno-kosmicheskaya tekhnika i tekhnologiya, 2010, no. 3 (70), pp. 11–20.
  30. Vorobey V.V., Markin V.B. Quality control of manufacturing and repair technology of composite structures. Novosibirsk: Nauka, 2006, 190 p.
  31. Aung T.H. Analysis of defects in products made of polymeric materials and restoration of their bearing capacity by welding: Cand. Sc. (Tech.). Moscow: MATI – RGTU named after K.E. Tsiolkovsky, 2014, 197 p.
  32. Non-destructive testing: a reference book in 7 vols. Ed. V.V. Klyuev. Moscow: Mashinostroenie, 2004, vol. 3: Ultrasonic testing, 864 p.
  33. Adams R.D., Cawley P. A review of defect types and nondestructive testing techniques for composites and bonded joints. NDT International, 1988, vol. 21, no. 4, pp. 208–222.
  34. Cawley P., Adams R. Defect types and NDT for composites and bonded joints. Materials Science and Technology, 1989, vol. 5, pp. 406–447.
  35. Mehdikhani M., Gorbatikh L., Verpoest I., Lomov S.V. Voids in fiber-reinforced polymer composites: A review on their formation, characteristics, and effects on mechanical performance. Journal of Composite Materials, 2018, vol. 53, is. 12, pp. 1–91. DOI: 10.1177/0021998318772152.
  36. Baurova N.I., Zorin V.A. The use of polymer composite materials in the production and repair of machines: textbook. Moscow: MADI, 2016, 264 p.
  37. Crowley D.M., Ward C., Potter K. A Status of Acceptance Criteria and Process Requirements in Advanced Composites Manufacturing, and Whether They are Fit for Purpose. Bristol: SAE International, 2013, 10 p. DOI: 10.4271/2013-01-2144.
  38. Potter K. Understanding the origins of defects and variability in composites manufacture. ICCM-17. Edinburgh, 2009. Available at: http://www.iccm-central.org/Proceedings/ICCM17proceedings/papers/ P1.5%20Potter.pdf (дата обращения: 26.09.2022).
  39. Chertishchev V.Yu. Development of Technologies and Means of Acoustic Impedance Control of Multilayer Honeycomb Structures from Polymer Composite Materials: thesis, Cand. Sc. (Tech.). Moscow: Bauman MSTU, 2020, 180 p.
  40. Bossi R.H., Giurgiutiu V. Nondestructive testing of damage in aerospace composites. Polymer Composites in the Aerospace Industry. Elsevier Ltd., 2015, pp. 413–448. DOI: 10.1016/B978-0-85709-523-7.00015-3.
  41. Unnthorsson R., Jonsson M.T., Runarsson T.P. NDT methods for evaluating carbon fiber composites. Procceedings Composites Testing and Model Identification. Bristol, 2004, рр. 21–23.
  42. Kosarina E.I., Krupnina O.A., Demidov A.A., Mikhaylova N.A. Digital optical pattern and its depen-dence on the radiation image at non-destructive testing by method of digital radiography. Aviacionnye materialy i tehnologii, 2019, no. 1 (54), pp. 37–42. DOI: 10.18577/2071-9140-2019-0-1-37-42.
  43. Slavin A.V., Dalin M.A., Dikov I.A., Boychuk A.S., Chertishchev V.Yu. Current trends in development of acoustic non-destructive testing methods in aviation industry (review). Trudy VIAM, 2021, no. 12 (106), paper no. 11. Available at: http://www.viam-works.ru (accessed: September 26, 2022). DOI: 10.18577/2307-6046-2021-0-12-96-106.
  44. Vavilov V.P., Chulkov A.O., Nesteruk D.A., Plesovskikh A.V. A complex approach to the development of the method and equipment for thermal nondestructive testing of CFRP cylindrical parts. Composites. Part B: Engineering, 2015, vol. 68, pp. 375–384. DOI: 10.1016/j.compositesb.2014.09.007.