Valeev R.A., Piskorsky V.P., Korolev D.V., Morgunov R.B. Optimization of the cobalt content as a way of temperature stabilization of rare earth magnets // Proceedings of VIAM. 2023. No. 3 (121). Ст. 06. URL: https://www.viam-works.ru. DOI: 10.18577/2307-6046-2023-0-3-58-66.

Optimization of the cobalt content as a way of temperature stabilization of rare earth magnets

Valeev R.A., Piskorsky V.P., Korolev D.V., Morgunov R.B.
Abstract

Experimental data on the use of rare earth metals in combination with cobalt as the basis of permanent magnets are presented. Data analysis and calculations of the functionality of such magnets show that such magnets will have noticeably higher stability and will demonstrate unusually small deviations of properties under temperature variations. The proposed magnets will significantly increase the signal-to-noise ratio when removing the signal from the electrodynamical devices. 

Keywords
permanent magnets, coercive force, residual induction, temperature stability, rare earth magnets
Reference list
  1. Malyutin D.M. Payload Stabilization System on a Dynamically Adjustable Gyro. Pribory i metody izmereniy, 2016, no. 7, pp. 32–34.
  2. Chirkin D.S., Roslovets P.V., Tatarinov F.V., Novikov L.Z. Reducing the drift of a dynamically tuned gyroscope from run to run. Inzhenernyy zhurnal: nauka i innovatsii, 2017, is. 1, pp. 1–14. DOI: 10.18698/2308-6033-2017-01-1579.
  3. Deleile F. Onboard inertial coordinate system for the European launch vehicle "ARIAN-6" based on a wave solid-state gyroscope. Pribory i metody izmereniy, 2018, vol. 26, no. 4, pp. 3–13. DOI: 10.17285/0869-7035.2018.26.4.003-013.
  4. Podporin S.A., Veliev E.B. Heading guidance systems for modern offshore support vessels. Bulletin of the Sevastopol NTU. Series: Mechanics, energy, ecology, 2014, is. 153, pp. 99–106.
  5. Topilskaya S.V., Borodulin D.S., Kornyukhin A.V. Experimental evaluation of allowable mechanical impacts on a dynamically adjustable gyroscope. Vestnik MGTU im. N.E. Baumana. Ser.: Priborostroyenie, 2018, no. 4, pp. 69–79. DOI: 10.18698/0236-3933-2018-4-69-79.
  6. Morgunov R.B., Piskorskiy V.P., Valeev R.A., Korolev D.V. The thermal stability of rare-earth magnets supported by means of the magnetocaloric effect. Aviacionnye materialy i tehnologii, 2019, no. 1 (54), pp. 88–94. DOI: 10.18577/2071-9140-2019-0-1-88-94.
  7. Marinescu M., McGinnis K., Liu J.F., Walmer M.H. High (BH)max permanent magnets with near-zero reversible temperature coefficient of BR. Proceedings of 20th International Workshop on Rare Earth Permanent Magnets and Their Applications. 2008, pp. 1–6.
  8. Li A., Li W., Wang H. et al. The study on thermal expansion of sintered Sm2Co17 magnets. IEEE Transactions Magnetics, 2009, vol. 45, no. 10, pp. 4402–4404.
  9. Tian J., Qu X., Zhang S. et al. Magnetic properties and microstructure of radially oriented Sm(Co, Fe, Cu, Zr) ring magnets. Material Letters, 2007, vol. 61, pp. 5271–5274.
  10. Tian J., Pan D., Zhou H. et al. Radial cracks and fracture mechanism of radially oriented ring 2:17 type SmCo magnets. Journal of Alloys and Compounds, 2009, vol. 476, pp. 98–101.
  11. Peshekhonov V.G. Prospects for the development of gyroscopy. Giroskopiya i navigatsiya, 2020, vol. 28, no. 2, pp. 3–10. DOI: 10.17285/0869-7035.0028.
  12. Siraya T.N. Statistical interpretation of Allan variations as characteristics of measuring and navigation devices. Giroskopiya i navigatsiya, 2020, vol. 28, no. 1, pp. 3–18.
  13. Kablov E.N., Startsev V.O. Measurement and forecasting of materials samples’ temperature during weathering in different climatic zones. Aviacionnye materialy i tehnologii, 2020, no. 4 (61), pp. 47–58. DOI: 10.18577/2071-9140-2020-0-4-47-58.
  14. Kablov E.N. Innovative developments of FSUE «VIAM» SSC of RF on realization of «Strategic directions of the development of materials and technologies of their processing for the period until 2030». Aviacionnye materialy i tehnologii, 2015, no. 1 (34), pp. 3–33. DOI: 10.18577/2071-9140-2015-0-1-3-33.
  15. Piskorsky V.P., Valeev R.A., Korolev D.V., Morgunov R.B., Rezchikova I.I. Terbium and gadolinium dopin g influence on thermal stability and magnetic properties of sintered magnets Pr–Tb–Gd–Fe–Co–B. Trudy VIAM, 2019, no. 7 (79), paper no. 07. Available at: http://www.viam-works.ru (accessed: August 12, 2022). DOI: 10.18577/2307-6046-2019-0-7-59-66.
  16. Korolev D.V., Piskorskii V.P., Valeev R.A., Bakradze M.M., Dvoretskaya E.V., Koplak O.V., Morgunov R.B. Rare-earth RE–TM–B micromag-nets engineering (review). Aviation materials and technology, 2021, no. 1 (62), paper no. 05. Available at: http://www.journal.viam.ru (accessed: August 12, 2022). DOI: 10.18577/2713-0193-2021-0-1-44-60.
  17. Kablov E.N., Ospennikova O.G., Piskorskij V.P., Rezchikova I.I., Valeev R.A., Davydova E.A. Phase composition of the Pr–Dy–Fe–Co–B sintered materials. Aviacionnye materialy i tehnologii, 2015, no. S2 (39), pp. 5–10. DOI: 10.18577/2071-9140-2015-0-S2-5-10.
  18. Perigo E.A., Takiishi H., Motta C.C., Faria R.N. On the squareness factor behavior of RE–FeB (RE = Nd or Pr) magnetic above room temperature. IEEE Transactions on Magnetics, 2009, vol. 45, no. 10, pp. 4431–4434.
  19. Chuang Y.C., Wu C.H., Chang T.D. et al. Structure and magnetic properties of cobalt-rich Pr–Co–B alloys. Journal of the Less-Common Metals, 1985, vol. 144, pp. 249–256.
  20. Ido H., Wallace W.E., Suzuki T. et al. Magnetic and crystallographic properties of NdCo4M (M = B, Al and Ga). Journal of Applied Physics, 1990, vol. 67, no. 9, pp. 4635–4637.
  21. Pedziwiatr A.T., Jiang S.Y., Wallace W.E. et al. Magnetic properties of RCo4B compounds where R = Y, Pr, Nd, Gd and Er. Journal of Magnetism and Magnetic Materials, 1987, vol. 66, pp. 69–73.
  22. Dub O.M., Chaban N.F., Kuzma Y.B. New borides of Pr5–xCo2+xB6 – type structure containing iron and cobalt. Journal of the Less-Common Metals, 1986, vol. 117, pp. 297–302.
  23. Sergeev V.V., Bulygina T.I. Hard magnetic materials. Moscow: Energy, 1980, 224 p.