Postnov V.I., Mantusova O.Yu., Postnova M.V., Barannikov A.A. Influence of thermocyclic effects on the properties of fiberglass // Proceedings of VIAM. 2023. No. 2 (120). Ст. 08. URL: https://www.viam-works.ru. DOI: 10.18577/2307-6046-2023-0-2-87-100.

Influence of thermocyclic effects on the properties of fiberglass

Postnov V.I., Mantusova O.Yu., Postnova M.V., Barannikov A.A.
Abstract

The article is devoted to the study of the influence of thermocyclic effects and operating temperature on the properties of polymer composite materials based on the fiberglass and epoxy binder. It is established that the «heating–cooling» cycles for fiberglass with different polymer matrix content and reinforcement options cause some decreases in strength and elastic dynamic characteristics, but this does not adversely affect the operation of protective screens or engine nacelles for gas turbine engines made of fiberglass.

Keywords
fiberglass, thermal cycling, reinforcement scheme, bending strength, shear strength
Reference list
  1. Kablov E.N. The role of chemistry in the creation of new generation materials for complex technical systems. Reports of XX Mendeleev Congress on General and Applied Chemistry. Ekaterinburg: Ural Branch of the Russian Academy of Sciences, 2016, pp. 25–26.
  2. Kablov E.N., Podzhivotov N.Yu., Lutsenko A.N. On the need to create a unified information and analytical center for aviation materials of the Russian Federation. Problemy mashinostroyeniya i avtomatizatsii, 2019, no. 3, pp. 28–34.
  3. Kablov E.N. What is the future to be made of? Materials of a new generation, technologies for their creation and processing – the basis of innovation. Krylya Rodiny, 2016, no. 5, pp. 8–18.
  4. Popov Y.O., Kolokolceva T.V., Gusev Y.A., Gromova A.A. Development of the constructive and technological solution for a sheet fibreglass for tail section skins of helicopter rotor blades. Trudy VIAM, 2016, no. 1 (37), paper no. 05. Available at: http://www.viam-works.ru (accessed: November 12, 2020). DOI: 10.18577/2307-6046-2016-0-1-42-49.
  5. Soloviev P.V., Dmitriev N.N. Influence of technological parameters and thermal cycling effects on the strength properties of modified carbon plastics. Vestnik Ufimskogo gosudarstvennogo aviatsionnogo tekhnicheskogo universiteta, 2019, vol. 23, no. 2 (84), pp. 75–80.
  6. Kablov E.N., Erasov V.S., Panin S.V., Kurs M.G., Gladkikh A.V., Avtaev V.V., Sorokina N.I., Lukyanychev D.A. Investigation of the combined effect of mechanical loads and climatic factors on the properties of materials in the composition of a large-sized design of the experimental wing compartment after 4 years of testing. Reports of II Int. sci.-tech. conf. "Corrosion, Aging, and Biostability of Materials in Marine Climates". Moscow: VIAM, 2016, p. 6.
  7. Kablov E.N., Startsev V.O., Inozemtsev A.A. The moisture absorption of structurally similar samples from polymer composite materials in open climatic conditions with application of thermal spikes. Aviacionnye materialy i tehnologii, 2017, no. 2 (47), pp. 56–68. DOI: 10.18577/2071-9140-2017-0-2-56-68.
  8. Kablov E.N., Startsev O.V., Krotov A.S., Kirillov V.N. Climatic aging of aviation composite materials. I. Mechanisms of aging. Deformatsiya i razrusheniye materialov, 2010, no. 11, pp. 19–27.
  9. Popov Yu.O., Koloкoltseva T.V., Gromova A.A., Gusev Yu.A. Influence of operational factors on the main physical and mechanical properties of a fiberglass product VPS-31. Trudy VIAM, 2021, no. 11 (105), paper no. 08. Available at: http://www.viam-works.ru (accessed: November 12, 2020). DOI: 10.18577/2307-6046-2021-0-11-82-90.
  10. Laptev A.B., Nikolayev E.V., Kolpachkov E.D. Thermodynamic characteristics of aging of polymeric composite materials under conditions of real exploitation. Aviaсionnye materialy i tehnologii, 2018, no. 3, pp. 80–88. DOI: 10.18577/2071-9140-2018-0-3-80-88.
  11. Veshkin E.A., Postnov V.I., Semenychev V.V., Barannikov A.A. Anisotropy of the properties of the polymer matrix in composite materials. Proceedings of the VI All-Rus. Sci.-techn. сonf."The role of fundamental research in the implementation of strategic directions for the development of materials and technologies for their processing for the period up to 2030". Moscow, 2020, pp. 14–35.
  12. Kablov E.N., Startsev V.O. Systematical analysis of the climatics influence on mechanical properties of the polymer composite materials based on domestic and foreign sources (review). Aviacionnye materialy i tehnologii, 2018, no. 2 (51), pp. 47–58. DOI: 10.18577/2071-9140-2018-0-2-47-58.
  13. Popov Yu.O., Kolokoltseva T.V., Khrulkov A.V. The new generation of materials and technologies for helicopter blade spars. Aviacionnye materialy i tehnologii, 2014, no. S2, pp. 5–9. DOI: 10.18577/2071-9140-2014-0-S2-5-9.
  14. Kablov E.N., Startsev V.O. Climatic aging of polymer composite materials for aviation purposes. II. Development of methods for studying the early stages of aging. Deformatsiya i razrusheniye materialov, 2020, no. 1, pp. 15–21.
  15. Kablov E.N., Startsev O.V., Medvedev I.M., Shelemba I.S. Fiber optic sensors for monitoring corrosion processes in units of aviation engineering (review). Aviacionnye materialy i tehnologii, 2017, no. 3 (48), pp. 26–34. DOI: 10.18577/2071-9140-2017-0-3-26-34.