Abstract

Influence of way of introduction of multiwall carbon nanotubes (MUNT) in model epoxy system nature of their distribution in the volume of polymeric composition is investigated. Rheological characteristics, glass transition temperatures and physicomechanical properties, and also microstructures of otverzhdenny samples of initial composition and samples are investigated, in which MUNT were entered with use of ultrasonic dispergator and the three-roll mixer into structure injection binding VSE-30 and binding VSE-22 overworked on prepregovy technology.

Keywords
epoxy binder, nanomodification, multi-walled carbon nanotubes, ultrasonic dispersion, electron microscopy, rheology
Reference list
  1. Kablov E.N., Kulagina G.S., Zhelezina G.F., Lonskii S.L., Kurshev E.V. Microstructure research of the unidirectional organoplastic based on Rusar-NT aramid fibers and epoxy-polysulfone binder. Aviacionnye materialy i tehnologii, 2020, no. 4 (61), pp. 19–26. DOI: 10.18577/2071-9140-2020-0-4-19-26.
  2. Kablov E.N., Kondrashov S.V., Yurkov G.Yu. Prospects for the use of carbon-containing nanoparticles in binders for polymer composite materials. Rossiyskiye nanotekhnologii, 2013, vol. 8, no. 3–4, pp. 24–42.
  3. Kablov E.N., Chursova L.V., Babin A.N., Mukhametov R.R., Panina N.N. Developments of FSUE "VIAM" in the field of melt binders for polymer composite materials. Polymer Materials and Technologies, 2016, vol. 2, no. 2, pp. 37–42.
  4. Kablov E.N. Composites: today and tomorrow. Metally Evrazii, 2015, no. 1, pp. 36–39.
  5. Kablov E.N., Gunyaev G.M. Nanomaterials – a breakthrough in materials science of the microcosm. 75 years. Aviation materials. Moscow: VIAM, 2007, pp. 225–232.
  6. Pavlyuk B.Ph. The main directions in the field of development of polymeric functional materials. Aviacionnye materialy i tehnologii, 2017, no. S, pp. 388–392. DOI: 10.18577/2071-9140-2017-0-S-388-392.
  7. Shitov R.O., Kitaeva N.S., Shiryakina Yu.M., Kurshev E.V. Research of influence of modifiers of varied nature on the thermo-oxidative stability of a model silicone binder. Trudy VIAM, 2020, no. 6–7 (89), paper no. 03. Available at: http://www.viam-works.ru (accessed: July 19, 2022). DOI: 10.18577/2307-6046-2020-0-67-19-28.
  8. Campbell F.C. Structural Composite Materials. Ohio: ASM International, 2010, 500 p.
  9. Singh N.P., Gupta V.K., Singh A.P. Graphene and carbon nanotube reinforced epoxy nanocomposites: A review. Polymer, 2019, vol. 180, art. 121724.
  10. Smoleń P., Czujko T., Komorek Z. et al. Mechanical and electrical properties of epoxy composites modified by functionalized multiwalled carbon nanotubes. Materials, 2021, vol. 14, no. 12, pp. 3325–3340.
  11. Marakhovsky P.S., Kondrashov S.V., Dyachkova T.P., Gurevich Ya.M., Mayorova I.A., Shvedkova A.K., Valevin E.O., Yurkov G.Yu. Structure formation and features of moisture absorption of epoxy nanocomposites with carbon nanotubes. Perspektivnye materialy, 2015, no. 6, pp. 48–56.
  12. Rajan J.S. Effective use of nano-carbons in controlling the electrical conductivity of epoxy composites. Composites Science and Technology, 2021, vol. 202, art. 108554.
  13. Asthana A., Srivastava V. Analysis of mechanical strength and Young’s modulus of ultrasonically functionalised CNT-epoxy composites. Advances in Materials and Processing Technologies, 2021, vol. 7, pp. 1–8.
  14. Zhang D., Huang Y., Chia L. Effects of carbon nanotube (CNT) geometries on the dispersion characterizations and adhesion properties of CNT reinforced epoxy composites. Composite Structures, 2022, vol. 296, art. 115942.
  15. Jen Y.M., Huang J.C. Synergistic effect on the thermomechanical and electrical properties of epoxy composites with the enhancement of carbon nanotubes and graphene nano platelets. Materials, 2019, vol. 12, no. 2, pp. 255–266.
  16. Han S., Meng Q., Araby S. et al. Mechanical and electrical properties of graphene and carbon nanotube reinforced epoxy adhesives: Experimental and numerical analysis. Composites. Part A: Applied Science and Manufacturing, 2019, vol. 120, pp. 116–126.
  17. Wang F.X., Liang W.Y., Wang Z.Q. et al. Preparation and property investigation of multi-walled carbon nanotube (MWCNT)/epoxy composite films as high-performance electric heating (resistive heating) element. Express Polymer Letters, 2018, vol. 12, no. 4, pp. 285–295.
  18. Methods and compositions for increasing productivity in composite manufacturing comprising profile drawing and applications thereof: pat. FI 125348 B; filed 11.05.09; publ. 10.01.11.
  19. Catalytic composition for synthesizing carbon nanotubes: pat. US 9731277 B2; filed 08.03.12; publ. 15.08.17.
  20. Polymer-based composites comprising carbon nanotubes as a filler, method for producing said composites, and associated uses: pat. US 7968660 B2; filed 10.06.09; publ. 28.06.11.
  21. Method for the preparation of a reinforced thermoset polymer composite: pat. US 8613980 B2; filed 17.07.09; publ. 24.12.13.
  22. Method of synthesizing a support catalyst for the production of carbon nanotubes: pat. US 7754181 B2: filed 09.12.05; publ. 13.07.10.
  23. Hybrid materials and related methods and devices: pat. US 9243146 B2: filed 11.10.05; publ. 26.01.16.
  24. Method for covalent functionalization of carbon nanotubes with simultaneous ultrasonic dispersion for introduction into epoxy compositions: pat. 2660852 Rus. Federation; filed 14.06.17; publ. 10.07.18.
  25. Method for modifying carbon nanomaterials: pat. 2548083 Rus. Federation; filed 18.06.13; publ. 10.04.15.
  26. Roy S., Petrova R.S., Mitra S. Effect of carbon nanotube (CNT) functionalization in epoxy-CNT composites. Nanotechnology reviews, 2018, vol. 7, no. 6, pp. 475–485.
  27. Yourdkhani M., Liu W., Baril-Gosselin S. et al. Carbon nanotube-reinforced carbon fibre-epoxy composites manufactured by resin film infusion. Composites Science and Technology, 2018, vol. 166, pp. 169–175.
  28. Kudryavtseva A.N., Tkachuk A.I., Grigorieva K.N., Gurevich Ya.M. The use of epoxy resin system VSE-30, processed by the infusion technology, for the manufacture of low and medium loaded structural polymer composite materials. Trudy VIAM, 2019, no. 1 (73), paper no. 04. Available at: http://www.viam-works.ru (accessed: July 18, 2022). DOI: 10.18577/2307-6046-2019-0-1-31-39.
  29. Antyufeeva N.V., Aleksashin V.M., Stolyankov Yu.V. Polymer composite curing degree evaluation by thermal analysis test methods. Aviacionnye materialy i tehnologii, 2015, № 3 (36), pp. 79–83. DOI: 10.18577/2071-9140-2015-0-3-79-83.
  30. Kondrashov S.V., Marakhovsky P.S., Mayorova I.A., Egorov A.A., Mansurova I.A., Yurkov G.Yu. Influence of the curing regime on the formation of the structure of epoxy composites in the presence of carbon nanotubes. Perspektivnye materialy, 2014, no. 6, pp. 56–63.
  31. Solovyanchik L.V., Kondrashov S.V. The prospects of using carbon nanotubes to impart functional properties to the surface of polymer materials (review). Trudy VIAM, 2021, no. 9 (103), paper no. 02. Available at: http://www.viam-works.ru (accessed: July 05, 2022). DOI: 10.18577/2307-6046-2021-0-9-11-21.
  32. Zagora A.G., Kondrashov S.V., Antyufeeva N.V., Pykhtin A.A. Research of influence of technological modes of production of epoxy nanocomposites with carbon nanotubes on their heat resistance. Trudy VIAM, 2019, no. 1 (73), paper no. 08. Available at: http://www.viam-works.ru (accessed: July 15, 2022). DOI: 10.18577/2307-6046-2019-0-1-64-73.
  33. Epoxy composition for the manufacture of products from PCM: pat. 2488612 Rus. Federation; filed 18.04.12; publ. 27.07.13.
  34. Kondrashov S.V., Merkulova Yu.I., Marakhovsky P.S., Dyachkova T.P., Shashkeev K.A., Popkov O.V., Startsev O.V., Kurshev E.V., Yurkov G.Yu. Features of the degradation of the physical and mechanical properties of epoxy nanocomposites with carbon nanotubes under heat and moisture exposure. Zhurnal prikladnoy khimii, 2017, vol. 90, no. 5, pp. 657–665.
  35. Deev I.S., Zhelezina G.F., Lonsky S.L., Kurshev E.V. Features of forming of the microstructure of the polymeric matrix in organoplasty on the basis of the multicomponent epoxy binding. Trudy VIAM, 2019, no. 5 (77), paper no. 03. URL: http://www.viam-works.ru (accessed: July 10, 2022). DOI: 10.18577/2307-6046-2014-0-7-6-6.