Zhitnyuk S.V., Medvedev P.N. Investigation of microstructure and phase composition of the metallic composite material Al–Si–Mg system modified by silicon carbide particles by mechanical alloying. Part 1 // Proceedings of VIAM. 2023. No. 1 (119). Ст. 08. URL: https://www.viam-works.ru. DOI: 10.18577/2307-6046-2023-0-1-97-106.

Investigation of microstructure and phase composition of the metallic composite material Al–Si–Mg system modified by silicon carbide particles by mechanical alloying

Part 1
Zhitnyuk S.V., Medvedev P.N.
Abstract

The development of composite materials based on aluminum alloys modified with ceramic fillers is one of the most important areas of materials science today. The most promising method for obtaining composite materials based on aluminum is the method of selective laser melting. The purpose of this work is to identify the features of the formation of the microstructure and phase composition of the composite powder in the process of mechanical alloying of aluminum alloy VAS1 and silicon carbide depending on time.

Keywords
gas atomization, selective laser melting, mechanical alloying, composite material, microstructure, aluminum alloy, silicon carbide
Reference list
  1. Kablov E.N. Innovative developments of FSUE «VIAM» SSC of RF on realization of «Strategic directions of the development of materials and technologies of their processing for the period until 2030». Aviacionnye materialy i tehnologii, 2015, no. 1 (34), pp. 3–33. DOI: 10.18577/2071-9140-2015-0-1-3-33.
  2. Buznik V.M., Kablov E.N. State and prospects of Arctic materials science. Vestnik RAN, 2017, vol. 87, no. 9, pp. 827–839.
  3. Kablov E.N. Dominant of the national technology initiative. Problems of accelerating the development of additive technologies in Russia. Metally Evrazii, 2017, no. 3, pp. 2–6.
  4. Gorbovets M.A., Belyayev M.S., Ryzhkov P.V. Fatigue strength of heat-resistant nickel alloys produced by selective laser melting. Aviaсionnye materialy i tehnologii, 2018, no. 3, pp. 50–55. DOI: 10.18577/2071-9140-2018-0-3-50-55.
  5. Bulina N.V., Malikov A.G., Orishich А.М., Klochkov G.G. Research of the structural-phase composition of laser weld joint depending on the thermal processing of the aluminum alloy V-1469. Aviacionnye materialy i tehnologii, 2019, no. 2 (55), pp. 31–39. DOI: 10.18577/2071-9140-2019-0-2-31-39.
  6. Lukina E.A., Zaitsev D.V., Romanenko V.A. Structure and properties of a composite material based on aluminum alloy with the addition of carbon nanotubes. Aviacionnye materialy i tehnologii, 2019, no. 4 (57), pp. 27–34. DOI: 10.18577/2071-9140-2019-0-4-27-34.
  7. Kosolapov D.V., Shavnev A.A., Kurbatkina E.I., Nyafkin A.N., Gololobov A.V. Study on structure and properties of dispersion hardened MMC based on aluminium alloy of Al–Mg–Si system. Trudy VIAM, 2020, no. 1, paper no. 06. Available at: http://www.viam-works.ru (accessed: September 15, 2022). DOI: 10.18577/2307-6046-2020-0-1-58-67.
  8. Lui K., Jiang X., Chen S., Yuan T. Effect of SiC addition on microstructure and properties of Al–Mg alloy fabricated by powder and wire cold metal transfer process. Journal of Materials Research and Technology, 2022, vol. 17, pp. 310–319.
  9. Khodabakhshi F., Gerlich A.P. On the stability, microstructure, and mechanical property of powder metallurgy Al–SiC nanocomposites during similar and dissimilar laser welding. Material Science & Engineering: A, 2019, vol. 759, pp. 688–702.
  10. Pei W., Zhengying W., Zhen C. The AlSi10Mg samples produced by selective laser melting: single track, densification, microstructure and behavior. Applied surface science, 2017, vol. 408, pp. 38–50. DOI: 10.1016/j.apsusc.2017.02.215.
  11. Tang M., Pistorius P.C. Anisotropic Mechanical Behavior of AlSi10Mg Parts Produced by Selective Laser Melting. The Journal of the Minerals, Metals & Materials Society, 2017, vol. 69, pp. 516–522. DOI: 10.1007/s11837-016-2230-5.
  12. Shavnev A.A., Nerush S.V., Kurbatkina E.I., Kosolapov D.V., Medvedev P.N. Investigation of the structure of a metal composite material of the Al–Si–Mg–SiC system obtained using mechanical alloying. Izvestiya vuzov. Poroshkovaya metallurgiya i funktsionalnye pokrytiya, 2022, no. 1, pp. 17–25. DOI: 10.17073/1997-308X-2022-1-17-25.
  13. Mohanavel V., Rajan K., Kumar S.S. et al. Effect of silicon carbide reinforcement on mechanical and physical properties of aluminum matrix composites. Materials Today: Proceedings, 2018, vol. 5, no. 1, pp. 2938–2944. DOI: 10.1016/j.matpr.2018.01.089.
  14. Famodimu O.H., Stanford M., Oduoza C.F., Zhang L. Effect of process parameters on the density and porosity of laser melted AlSi10Mg/SiC metal matrix composite. Frontiers of Mechanical Engineering, 2018, vol. 13, pp. 520–527.
  15. Riquelme A., Rodrigo P., Escalera-Rodríguez M.D., Rams J. Additively Manufactured Al/SiC Cylindrical Structures by Laser Metal Deposition. Materials, 2020, vol. 13, is. 15, art. 3331.
  16. Sulyanov S., Boysen H., Paulmann C. et al. 2θ-scanning 2D-area detector for high quality powder data collection using synchrotron radiation. European Powder Diffraction Conference, 2011, no. 1, pp. 175–180.
  17. Nerush S.V., Ermolayev A.S., Rogalev A.M., Vasilenko S.A. Research of retailoring process of the rotor blade feather end of the first stage of high-pressure turbine (HPT) from ZhS32-VI alloy by laser metal deposition with ZhS32-VI metal alloy powder dispersed by atomization. Trudy VIAM, 2016, no. 8, paper no. 4. Available at: http://www.viam-works.ru (accessed: September 15, 2022). DOI: 10.18577/2307-6046-2016-0-8-4-4.
  18. Diagrams of the state of binary metal systems: D44: a reference book in 3 vols. Ed. N.P. Lyakishev. Moscow: Mashinostroenie, 1996, vol. 1, 992 p.