Peskova A.V., Bakradze M.M., Tikhonov М.М., Kuko I.S. Investigation of the influence of the oxide layer on the surface of particles metal-powder compositions of copper-chromium alloys on their technological properties // Proceedings of VIAM. 2023. No. 1 (119). Ст. 03. URL: https://www.viam-works.ru. DOI: 10.18577/2307-6046-2023-0-1-28-38.

Investigation of the influence of the oxide layer on the surface of particles metal-powder compositions of copper-chromium alloys on their technological properties

Peskova A.V., Bakradze M.M., Tikhonov М.М., Kuko I.S.
Abstract

Researches were carried out metal-powder compositions of the copper-chromium alloy system Cu–(0,5–1,0 %)Cr, obtained by the method of gas atomization. The influence of the formed oxide layer on the surface of particles on the technological properties of the powder has been researched. After the selective laser fusion, a change in the color of the powder from copper to violet was detected, as well as a formation of conglomerates, which led to a decrease in properties. Researches were carried out of fluidity, bulk density, as well as an assessment of the particle morphology were carried out metal-powder compositions before and after selective
 laser fusion.

Keywords
copper alloys, powder, atomization, technological properties, bulk density, fluidity, powder oxidation, additive manufacturing
Reference list
  1. Kablov E.N. Innovative developments of FSUE «VIAM» SSC of RF on realization of «Strategic directions of the development of materials and technologies of their processing for the period until 2030». Aviacionnye materialy i tehnologii, 2015, no. 1 (34), pp. 3–33. DOI: 10.18577/2071-9140-2015-0-1-3-33.
  2. Kablov E.N. Additive technologies – the dominant of the national technological initiative. Intellekt i tekhnologii, 2015, no. 2 (11), pp. 52–55.
  3. Kablov E.N. New generation materials. Zashchita i bezopasnost, 2014, no. 4, pp. 28–29.
  4. Ospennikova O.G. Strategy of development of hot strength alloys and steels special purpose, protective and heat-protective coverings. Aviacionnye materialy i tehnologii, 2012, no. S, pp. 19–36.
  5. Kablov E.N. VIAM materials and technologies for Aviadvigatel. Permskiye aviatsionnye dvigateli, 2014, no. 31, pp. 43–47.
  6. Wan X., Xie W., Chen H. et al. First-principles study of phase transformations in Cu–Cr alloys. Journal of Alloys and Compounds, 2021, vol. 862, art. 158531.
  7. Fu H., Xu S., Li W. Effect of rolling and aging processes on microstructure and properties of Cu–Cr–Zr alloy. Materials Science and Engineering A, 2017, vol. 700, pp. 107–115.
  8. Shan L., Wang X., Chang Y., Wang Y. Improving the mechanical performance of Cu[sbnd]Cr alloy by dissolving Cu in the Cr second phase. Materials Characterization, 2021, vol. 176, art. 111104.
  9. Xia C., Zhang W., Kang Zh. et al. High strength and high electrical conductivity Cu–Cr system alloys manufactured by hot rolling-quenching process and thermomechanical treatments. Materials Science and Engineering A, 2012, vol. 538, pp. 295–301.
  10. Jha K., Neogy S., Kumar S. et al. Correlation between microstructure and mechanical properties in the age-hardenable Cu–Cr–Zr alloy. Journal of Nuclear Materials, 2021, vol. 546, art. 152775.
  11. Zhang Y., Volinsky A., Train H. et al. Aging behavior and precipitates analysis of the Cu–Cr–Zr–Ce alloy. Materials Science and Engineering A, 2016, vol. 650, pp. 248–253.
  12. Chbihi A., Sauvage X., Blavette D. Atomic scale investigation of Cr precipitation in copper. Acta Materialia, 2012, no. 11, vol. 60, pp. 4575–4585.
  13. Bakradze M.M., Peskova A.V., Kaplansky Yu.Yu. Influence of thermal post-treatment on the texture and anisotropy of mechanical properties in the Cu–Cr construction alloy manufactured by laser powder bed fusion. Aviation materials and technologies, 2022, no. 1 (66), paper no. 01. Available at: http://www.journal.viam.ru (accessed: August 15, 2022). DOI: 10.18577/2071-9140-2022-0-1-3-16.
  14. Kiparisov S.S., Libenson G.A. Powder metallurgy. Moscow: Metallurgiya, 1980, 496 p.
  15. Powder metallurgy. Materials, technology, properties, applications: a reference book. Kyiv: Naukova dumka, 1985, 624 p.
  16. Powders of non-ferrous metals: reference book. Ed. S.S. Naboychenko. Moscow: Metallurgiya, 1997, 542 p.
  17. Kablov E.N., Evgenov A.G., Rylnikov V.S., Afanasiev-Khodykin A.N. Investigation of fine-dispersed solder powders for diffusion vacuum soldering, obtained by melt atomization. Vestnik MGTU im. N.E. Baumana. Ser.: Mashinostroyenie, 2011, no. SP2, pp. 79–87.
  18. Volkov A. M., Shestakova A. A., Bakradze M. M. The comparison of powder produced by gas atomization and by plasma rotate electrode process in the point of production disk billets from Ni-base superalloys. Trudy VIAM, 2018, no. 11 (71), paper no. 02. Available at: http://www.viam-works.ru (accessed: August 08, 2022). DOI: 10.18577/2307-6046-2018-0-11-12-19.
  19. Denisova V.S., Lonskii S.L., Kurshev E.V., Malinina G.A. Investigation of structure formation of reaction cured coatings by scanning electron microscopy. Trudy VIAM, 2019, no. 4 (76), paper no. 09. Available at: http://www.viam-works.ru (accessed: August 07, 2022). DOI: 10.18577/2307-6046-2019-0-4-76-87.
  20. Evgenov A.G., Shurtakov S.V., Prager S.M., Malinin R.Yu. On the development of a universal calculation method for assessing the degradation of recycled metal powder materials, depending on the cyclicity of use in the selective laser melting process. Aviacionnye materialy i tehnologii, 2020, no. 4 (61), pp. 3–11. DOI: 10.18577/2071-9140-2020-0-4-3-11.