Sukhov D.I., Kaplansky Yu.Yu., Rogalev A.M., Kurkin S. E. The features of processing Cr-rich nickel based alloy by selective laser melting // Proceedings of VIAM. 2023. No. 1 (119). Ст. 02. URL: https://www.viam-works.ru. DOI: 10.18577/2307-6046-2023-0-1-15-27.

The features of processing Cr-rich nickel based alloy by selective laser melting

Sukhov D.I., Kaplansky Yu.Yu., Rogalev A.M., Kurkin S. E.
Abstract

In this paper the structure and mechanical properties of SLM-built EP648 alloy are investigated. The research results of alloy via SEM, HR-TEM allowed detecting CrN particles and Me23C6 carbides in γ-matrix. The complex analysis of hot cracking in EP648 alloy was done. The effect of scan strategy type and oxygen content on hot crack volume density was shown. The connection between scan strategy type and tensile properties at room temperature was researched.

Keywords
Cr-rich nickel based alloy, additive manufacturing, selective laser melting, nitride, carbide, cracks
Reference list
  1. Market Research Future, Global Aerospace Additive Manufacturing Market Research Report – Forecast 2016–2021. Available at: https://www.marketresearchfuture.com/reports/aerospace-additive-manufacturingmarket-1551 (accessed: April 01, 2022).
  2. Campbell T.A., Ivanova O.S. Additive manufacturing as a disruptive technology: implications of three-dimensional printing. Technology & Innovation, 2013, vol. 15, no. 1, pp. 67–79. DOI: 10.3727/194982413x13608676060655.
  3. Gebler M., Schoot Uiterkamp A.J.M., Visser C. A global sustainability perspective on 3D printing technologies. Energy Policy, 2014, vol. 74 (C), pp. 158–167. DOI: 10.1016/j.enpol.2014.08.033.
  4. Najmon J.C., Raeisi S., Tovar A. Review of additive manufacturing technologies and applications in the aerospace industry. Additive Manufacturing for the Aerospace Industry. Elsevier, 2019, pp. 7–31. DOI: 10.1016/B978-0-12-814062-8.00002-9.
  5. Yadroitsev I., Yadroitsava I., Du Plessis A. Basics of laser powder bed fusion. Fundamentals of Laser Powder Bed Fusion of Metals. Elsevier, 2021, pp. 15–38. DOI: 10.1016/B978-0-12-824090-8.00024-X.
  6. Scalmalloy. Available at: https://www.apworks.de/scalmalloy (accessed: 04.04.2022).
  7. Katsarelis C., Chen P., Gradl P. et al. Additive Manufacturing of NASA HR-1 Material for Liquid Rocket Engine Component Applications. Available at: https://ntrs.nasa.gov/search.jsp? R=20200001007 (accessed: April 04, 2022).
  8. Ferrium C64. Available at: https://www.carpentertechnology.com/alloy-finder/ferrium-c64 (accessed: December 09, 2022).
  9. Deng D., Peng R. L., Brodin H., Moverare J. Microstructure and mechanical properties of Inconel 718 produced by selective laser melting: sample orientation dependence and effects of post heat treatments. Materials Science & Engineering A, 2018, vol. 713, pp. 294–306. DOI: 10.1016/j.msea.2017.12.043.
  10. Vrancken B., Thijs L., Kruth J.-P., Humbeeck J.V. Heat treatment of Ti6Al4V produced by Selective Laser Melting: Microstructure and mechanical properties. Journal of Alloys Compound, 2012, vol. 541, pp. 177–185.
  11. Li R., Liu J., Shi Yu. et al. 316L Stainless Steel with Gradient Porosity Fabricated by Selective Laser Melting. Journal of Materials, Engineering and Performance, 2009, vol. 19, no. 5, pp. 667–671.
  12. Ferreri N.C., Ghorbanpour S., Bhowmik S. et al. Effects of build orientation and heat treatment on the evolution of microstructure and mechanical properties of alloy Mar-M-509 fabricated via laser powder bed fusion. International Journal of Plasticity, 2019, vol. 121, pp. 116–133.
  13. Panin P.V., Zavodov A.V., Lukina E.A. Effect of thermal exposure on microstructure evolution and mechanical properties of cast beta-solidifying TiAl-based alloy doped with Gd. Intermetallics, 2022, vol. 145, art. 107534. DOI: 10.1016/j.intermet.2022.107534.
  14. Panin P.V., Bogachev I.A., Lukina E.A. Production and investigation of powders for additive synthesis from a new beta-solidifying TiAl-based alloy. Journal of Physics: Conference Series, 2021, vol. 2144, art. 012004. DOI: 10.1088/1742-6596/2144/1/012004.
  15. Aslanian G.G., Sukhov D.I., Mazalov PB, Sulyanova E.A. Fractographic study of Co–Cr–Ni–W–Ta alloy samples obtained by selective laser melting. Trudy VIAM, 2019, no. 4 (76), paper no. 01. Available at: http://www.viam-works.ru (accessed: July 01, 2022). DOI: 10.18577/2307-6046-2019-0-4-3-10.
  16. Mazalov I.S., Evgenov A.G., Prager S.M. Perspectives of heat resistant structurally stable alloy VZh159 application for additive production of high-temperature parts of GTE. Aviacionnye materialy i tehnologii, 2016, no. S1, pp. 3–7. DOI: 10.18577/2071-9140-2016-0-S1-3-7.
  17. Zhang B., Li Y., Bai Q. Defect Formation Mechanisms in Selective Laser Melting: A Review. Chinese Journal of Mechanical Engineering, 2017, vol. 30, pp. 515–527. DOI: 10.1007/s10033-017-0121-5.
  18. Ghoussoub J.N., Tang Y.T., Dick-Clerand W.J.B. et al. On the Influence of Alloy Composition on the Additive Manufacturability of Ni-Based Superalloys. Metallurgical and Materials Transactions A, 2022, vol. 53A, pp. 962–983. DOI: 10.1007/s11661-021-06568-z.
  19. Sukhov D.I., Petrushin N.V., Zaitsev D.V., Tikhonov M.M. Features of VZhL21 Nickel-base Superalloy Structure Formation During Selective Laser Melting, Vacuum Heat Treatment and Hot Isostatic Compaction. Metallurgist, 2019, vol. 63, no. 3–4, pp. 409–421.
  20. Marchese G. Study of the Microstructure and Cracking Mechanisms of Hastelloy X Produced by Laser Powder Bed Fusion. Materials, 2018, vol. 11 (1), pp. 106. DOI: 10.3390/ma11010106.
  21. Martin J.H., Yahata B.D., Hundley J.M. et al. 3D printing of high-strength aluminum alloys. Nature, 2017, vol. 549, pp. 365–369.
  22. Vrancken B. Influence of Process Parameters and Alloy Composition on Crack Mitigation in Selective Laser Melting. Available at: https://www.osti.gov (accessed: April 04, 2022).
  23. Sabzi H.E., Maeng S., Liang X. et al. Controlling crack formation and porosity in laser powder bed fusion: Alloy design and process optimisation. Additive Manufacturing, 2020, vol. 34, art. 101360. DOI: 10.1016/j.addma.2020.101360.
  24. Evgenov A.G., Sukhov D.I., Nerush S.V., Rogalev A.M. Mechanical properties and structure of an alloy of the Ni–Cr–W–Mo–Al–Ti–Nb system obtained by selective laser alloying. Tekhnologiya mashinostroyeniya, 2016, no. 3, pp. 5–9.
  25. Kablov E.N., Evgenov A.G., Mazalov I.S., Shurtakov S.V., Zaitsev D.V., Prager S.M. Structure and properties of EP648 and VZh159 alloys synthesized by selective laser melting after simulation annealing. Materialovedenie, 2020, no. 6, pp. 3–10.
  26. Evgenov A.G., Rogalev A.M., Nerush S.V., Mazalov I.S. A study of properties of EP648 alloy manufactured by the selective laser sintering of metal powders. Trudy VIAM, 2015, no. 2, paper no. 02. Available at: http://www.viam-works.ru (accessed: July 01, 2022). DOI: 10.18577/2307-6046-2015-0-2-2-2.
  27. Evgenov A.G., Gorbovec M.A., Prager S.M. Structure and mechanical properties of heat resistant alloys VZh159 and EP648, prepared by selective laser fusing. Aviacionnye materialy i tehnologii, 2016, no. S1, pp. 8–15. DOI: 10.18577/2071-9140-2016-0-S1-8-15.
  28. Ospennikova O.G., Naprienko S.A., Medve-dev P.N., Zaitsev D.V., Rogalev A.M. Features of the formation of the structural-phase state of the EP648 alloy during selective lase manufacture. Trudy VIAM, 2021, no. 8 (102), paper no. 01. Available at: http://www.viam-works.ru (accessed: July 01, 2022). DOI: 10.18577/2307-6046-2021-0-8-3-11.
  29. Ospennikova O.G., Min M.G., Rogalev A.M., Vadeev V.E. On the chemical composition, structure and mechanical properties of alloy EP648 fabricated by deformation, project die casting and selective laser melting. Voprosy Materialovedeniya, 2020, no. 1 (101), pp. 44–54. DOI: 10.22349/1994-6716-2020-101-1-44-54.
  30. Zhang J.-S. Creep of Second Phase Particles Strengthened Materials. High Temperature Deformation and Fracture of Materials. Elsevier, 2010, pp. 3–13. DOI: 10.1533/9780857090805.1.3.
  31. Baik S.I., Wang S.Y., Liaw P.K., Dunand D.C. Increasing the creep resistance of Fe–Ni–Al–Cr superalloys via Ti additions by optimizing the B2/L21 ratio in composite nano-precipitates. Acta Materialia, 2018, vol. 157, pp. 142–154. DOI: 10.1016/j.actamat.2018.07.025.
  32. Smallman R.E., Ngan A.H.W. Modern Physical Metallurgy: Eighth Edition. Elsevier Inc., 2013, 697 р. DOI: 10.1016/C2011-0-05565-5.