Tkachuk A.I., Lyubimova A.S., Kuznetcova P.A. Opportunities of the development of plant-based epoxy resins (review) // Proceedings of VIAM. 2022. No. 8 (114). Ст. 04. URL: https://www.viam-works.ru. DOI: 10.18577/2307-6046-2022-0-8-49-64.

Opportunities of the development of plant-based epoxy resins (review)

Tkachuk A.I., Lyubimova A.S., Kuznetcova P.A.
Abstract

This paper provides an overview of the development of plant-based epoxy resins. The review presents the main types of plant raw materials; the methods of obtaining epoxy resins based on vegetable raw materials are listed; general factors influencing the yield of the target product are identified: reaction temperature, concentration and type of organic acids. Based on the studied literature data, it can be concluded that the production of plant-based epoxy resins will become a topic for promising research and development of additives for adhesives, paints or composite materials in the future.

Keywords
epoxy resins, thermosetting resins, biopolymers, vegetable oil, fatty resins, epoxidation of double bonds, glycidation of the hydroxyl group, epichlorohydrin
Reference list
  1. Kablov E.N., Startsev V.O. Systematical analysis of the climatics influence on mechanical properties of the polymer composite materials based on domestic and foreign sources (review). Aviacionnye materialy i tehnologii, 2018, no. 2 (51), pp. 47–58. DOI: 10.18577/2071-9140-2018-0-2-47-58.
  2. Kablov E.N., Chursova L.V., Babin A.N., Mukhametov R.R., Panina N.N. Development of FSUE «VIAM» in the field of melt binders for polymer composite materials. Polimernye materialy i tekhnologii, 2016, vol. 2, no. 2, pp. 37–42.
  3. Kablov E.N., Erofeev V.T., Zotkina M.M., Dergunova A.V., Moiseev V.V., Rimshin V.I. Plasticized epoxy composites for manufacturing of composite reinforcement. Journal of Physics: Conference Series, 2020, vol. 1687, p. 012031.
  4. Mukhametov R.R., Petrova A.P. Thermosetting binders for polymer composites (review). Aviacionnye materialy i tehnologii, 2019, no. 3 (56), pp. 48–58. DOI: 10.18577/2071-9140-2019-0-3-48-58.
  5. Valueva M.I., Zelenina I.V., Zharinov M.A., Akhmadieva K.R. World market of high temperature polyimide carbon plastic (review). Trudy VIAM, 2019, no. 12 (84), paper no. 08. Available at: http://www.viam-works.ru (accessed: April 22, 2022). DOI: 10.18577/2307-6046-2019-0-12-67-79.
  6. Kablov E.N., Laptev A.B., Prokopenko A.N., Gulyaev A.I. Relaxation of polymeric composite materials under the prolonged action of static load and climate (review). Part 1. Binders. Aviation materials and technologies, 2021, no. 4 (65), paper no. 08. Available at: http://www.journal.viam.ru (accessed: April 22, 2022). DOI: 10.18577/2071-9140-2021-0-4-70-80.
  7. Gotlib E.M., Vdovina T.V., Yamaleeva E.S. Increasing the biodegradability of epoxy materials due to modification with vegetable oils and their oxygen-containing derivatives. Izvestiya vuzov. Prikladnaya khimiya i biotekhnologiya, 2020, vol. 10, no. 4, pp. 700–707. DOI: 10.21285/2227-2925-2020-10-4-700-707.
  8. Kostin A. Bioplastics: prospects in Russia. Plastiks, 2015, no. 3 (143), pp. 44–50.
  9. Samarth N.B., Mahanwar P.A. Modified Vegetable Oil Based Additives as a Future Polymeric Material – Review. Open Journal of Organic Polymer Materials, 2015, no. 5, pp. 1–22. DOI: 10.4236/ojopm.2015.5100.
  10. Prokhorenko S.V., Ivancheva A.D. State and problems of utilization of polymeric materials. Polymers-money, 2007, no. 4, pp. 27–32.
  11. Straathof A.J.J., Bampouli A. Potential of commodity chemicals to become bio-based according to maximum yields and petrochemical prices. Biofuels, Bioproducts and Biorefining, 2017, no. 11 (5), pp. 798–810. DOI: 10.1002/bbb.1786.
  12. FDA Regulations on Bisphenol A (BPA). Use in Food Contact Application. Available at: https://www.fda.gov/food/food-additives-petitions/bisphenol-bpa-use-food-contact-application#regulations (accessed: April 26, 2022).
  13. Wang S., Wong D.S., Jang S., Huang S. Novel plant-wide process design for producing dichlorohydrin by glycerol hydrochlorination. Journal of the Taiwan Institute of Chemical Engineers, 2017, vol. 73, pp. 50–61. DOI: 10.1016/j.jtice.2016.05.055.
  14. Zhu J., Garg A., Mekhissi K., Chandradhekhara K. Curing and mechanical characterization
  15. of a soybased epoxy resin system. Journal of Applied Polymer Science, 2004, vol. 91, no. 6, pp. 3513–3518.
  16. Tan S.G., Chow W.S. Biobased Epoxidized Vegetable Oils and Its Greener Epoxy Blends: A Review. Polymer-Plastics Technology and Engineering, 2010, vol. 49, pp. 1581–1590.
  17. Latif F.E.A., Zainal A.Z., Cardona F. et al. Bio-Resin Production through Ethylene Unsaturated Carbon Using Vegetable Oils. Processes, 2020, no. 8 (1), pp. 2–15. DOI: 10.3390/pr8010048.
  18. Baroncini E.A., Yadav S.K., Palmese G.R., Stanzione J.F. Recent advances in bio-based epoxy resins and bio-based epoxy curing agents. Journal of Applied Polymer Science, 2016, vol. 45, pp. 133. DOI: 10.1002/app.44103.
  19. Salimon J., Haron M.D.J., Jahangirian H. et al. Lipase Epoxidation Optimizing of Jatropha Curcas Oil Using Perlauric Acid. Digest Journal of Nanomaterials and Biostructures, 2014, vol. 9, pp. 1159–1169.
  20. Dodiuk H., Goodman S.H. Handbook of Thermoset Plastics. San Diego: William Andrew, 2014, 768 p.
  21. Markets M.A. Epoxidized Soybean Oil Market by Raw Material, by Applications, by End-Use Industry, by Region-Global Trends and Forecast to 2020: Markets and Markets. 2015. Available
  22. at: https://www.prnewswire.com/news-releases/epoxidized-soybean-oil-market-by-raw-materialby-
  23. application-by-end-use-industry-by-region---global-trends-and-forecasts-to-2020-300142755.html
  24. (accessed: April 27, 2022).
  25. Thermoplastic composites: recyclable materials. Available at: https://www.arkema.com/en/
  26. markets-and-solutions/solutions/biobased (accessed: April 27, 2022).
  27. Samper M.D., Petrucci R., Sanchez-Nacher L. et al. New Environmentally friendly composite laminates with epoxidized linseed oil (ELO) and slate fiber fabrics. Composites. Part B: Engineering, 2015, vol. 71, pp. 203–209.
  28. Cavusoglu J., Cayli G. Polymerization reactions of epoxidized soybean oil and maleate esters of oil-soluble resoles. Journal of Applied Polymer Science, 2015, vol. 7, p. 132. DOI: 10.1002/app.41457.
  29. Benyahya S., Aouf C., Caillol S. et al. Functionalized green tea tannins as phenolic prepolymers for bio-based epoxy resins. Industrial Crops and Products, 2014, vol. 53, pp. 296–307.
  30. Fache M., Boutevin B., Caillol S. Epoxy thermosets from model mixtures of the lignin-to-vanillin process. Green Chemistry, 2016, no. 18, pp. 712–725.
  31. Ding J., Ur Rahman O., Peng W. et al. A novel hydroxyl epoxy phosphate monomer enhancing the anticorrosive performance of waterborne Graphene/Epoxy coatings. Applied Surface Science, 2018, vol. 427, pp. 981–991. DOI: 10.1016/J.APSUSC.2017.08.224.
  32. Czub P. Kompozycje epoksydowe z wykorzystaniem modyfikowanych olejów rooelinnych. Polimery, 2008, vol. 53, pp. 182–189.
  33. Lari G.M., Pastore G., Mondelli C., Pérez-Ramírez J. Towards sustainable manufacture of epichlorohydrin from glycerol using hydrotalcite-derived basic oxides. Green Chemistry, 2018, no. 20 (1), pp. 148–159.
  34. Wang M., Zhou J., Mao G., Zheng X. Synthesis of TS-1 from an inorganic reactant system and its catalytic properties for allyl chloride epoxidation. Industrial & Engineering Chemistry Research, 2012, vol. 51 (39), pp. 12730–12738.
  35. Almena A., Martín M. Technoeconomic Analysis of the Production of Epichlorohydrin from Glycerol. Industrial & Engineering Chemistry Research, 2016, vol. 55 (12), pp. 3226–3238.
  36. Lukin P.M., Saveliev A.N., Saveliev N.I. Low-waste technology for the production of epichlorohydrin from glycerin. Ekologiya i promyshlennostʹ Rossii, 2016, no. 20 (6), pp. 8–13. DOI: 10.18412/1816-0395-2016-6-8-13.
  37. Dmitriev G.S., Khaustov E.N., Zanaveskin L.N. Synthesis of epichlorohydrin from biodiesel production waste. Available at: http://refdb.ru/look/1174105-p3.html (accessed: April 28, 2022).
  38. Manthey N.W., Cardona F., Aravinthan T. Cure kinetic study of epoxidized hemp oil cured with a multiple catalytic system. Journal of Applied Polymer Science, 2012, vol. 125, pp. 511–517.
  39. Cai S., Wang L. Epoxidation of Unsaturated Fatty Acid Methyl Esters in the Presence of SO3H-functional Bronsted Acidic Ionic Liquid as Catalyst. Chinese Journal of Chemical Engineering, 2011, vol. 19, pp. 57–63.
  40. Sinadinovi´c-Fišer S., Jankovi´c M., Borota O.M. Epoxidation of castor oil with peracetic acid formed in situ in the presence of an ion-exchange resin. Chemical Engineering and Processing, 2012, vol. 62, pp. 106–113.
  41. Leveneur S., Zheng J., Taouk B. et al. Interaction of thermal and kinetic parameters for a liquid-liquid reaction system: Application to vegetable oils epoxidation by peroxycarboxylic acid. Journal of the Taiwan Institute of Chemical Engineers, 2014, vol. 45, pp. 1449–1458.
  42. Zeleke T.D., Ayana Y.M. Epoxidation of Vernonia Oil in Acidic Ion Exchange Resin. American Journal of Applied Chemistry, 2017, no. 5 (1), pp. 1–6.
  43. Manthey N.W., Cardona F., Aravinthan T. Cure kinetic study of epoxidized hemp oil cured with a multiple catalytic system. Journal of Applied Polymer Science, 2012, vol. 125, pp. 511–517.
  44. Mungroo R., Pradhan N.C., Goud V., Dalai A.K. Epoxidation of Canola Oil with Hydrogen Peroxide Catalyzed by Acidic Ion Exchange Resin. Journal of the American Oil Chemists' Society, 2008, vol. 85 (9), pp. 887–896. DOI: 10.1007/s11746-008-1277-z.
  45. Abdullah B.M., Salimon J. Epoxidation of Vegetable Oils and Fatty Acids: Catalysts, Methods and Advantages. Journal of Applied Sciences, 2010, vol. 10, pp. 1545–1553. DOI: 10.3923/jas.2010.1545.1553.
  46. Uyama H., Kuwabara M., Tsujimoto T., Kobayashi S. Enzymatic synthesis and curing of biodegradable epoxidecontaining polyesters from renewable resources. Biomacromolecules, 2003, vol. 4 (2), pp. 211–215. DOI: 10.1021/bm0256092.
  47. Eitner J., Kraft M. Eco-friendly formulations based on vegetable oils. Available at: https://renewable-carbon.eu/news/eco-friendly-formulations-based-on-vegetable-oils (accessed: April 28, 2022).
  48. Saurab T., Patnaik M., Bhagt S.L., Renge V.C. Epoxidation of Vegetable Oils: A Review. International Journal of Emerging Technology and Advanced, 2011, vol. 2, pp. 491–501.
  49. Goud V.V., Dinda S., Paatwardhan A.V., Pradhan N.C. Epoxidation of Jatropha (Jatropha curcas) oil by peroxyacids. Asia-Pacific Journal of Chemical Engineering, 2010, vol. 5, pp. 346–354.
  50. Mushtaq M., Tan I.B., Devi C. et al. Epoxidation of Fatty Acid Methyl Esters derived from Jatropha oil. Proceedings of the 2011 National Postgraduate Conference (Kuala Lumpur, Malaysia, 19–20 September 2011), 2011, vol. 11, pp. 1–4.
  51. Oyama S.T. Mechanisms in Homogeneous and Heterogeneous Epoxidation Catalysis. Blacksburg: Elsevier, 2008. Available at: http://www.elsevier.com (accessed: April 29, 2022).
  52. Goud V.V., Patwardhan A.V., Dinda S., Pradhan N.C. Kinetics of epoxidation of jatropha oil with peroxyacetic and peroxyformic acid catalysed by acidic ion exchange resin. Chemical Engineering Science, 2007, vol. 62, pp. 4065–4076.