Kozlov I.A., Nikiforov A.A., Dyomin S.A., Vdovin A.I. Use of metal powder composition of the zinc–aluminum system for application of a protective coating by the method of cold gas-dynamic spraying // Proceedings of VIAM. 2022. No. 7 (113). Ст. 08. URL: https://www.viam-works.ru. DOI: 10.18577/2307-6046-2022-0-7-89-98.

Use of metal powder composition of the zinc–aluminum system for application of a protective coating by the method of cold gas-dynamic spraying

Kozlov I.A., Nikiforov A.A., Dyomin S.A., Vdovin A.I.
Abstract

In mechanical engineering, coating by cold gas-dynamic spraying (CGN) is most often used to eliminate mechanical damage (cracks, scratches) and defects, as well as to provide corrosion protection on steel parts. Improving the effectiveness of protective coatings applied by the CGN method by creating new powder materials is the main task of research in this area.

Keywords
zinc coatings, aluminum coatings, mechanical alloying, Dimet-405, cold gas dynamic spraying
Reference list
  1. Kablov E.N. Innovative developments of FSUE «VIAM» SSC of RF on realization of «Strategic directions of the development of materials and technologies of their processing for the period until 2030». Aviacionnye materialy i tehnologii, 2015, no. 1 (34), pp. 3–33. DOI: 10.18577/2071-9140-2015-0-1-3-33.
  2. Kablov E.N., Startsev O.V. The basic and applied research in the field of corrosion and ageing of materials in natural environments (review). Aviacionnye materialy i tehnologii, 2015, no. 4 (37), pp. 38–52. DOI: 10.18577/2071-9140-2015-0-4-38-52.
  3. Kablov E.N., Startsev O.V., Medvedev I.M. Review of international experience on corrosion and corrosion protection. Aviacionnye materialy i tehnologii, 2015, no. 2 (35), pp. 76–87. DOI: 10.18577/2071-9140-2015-0-2-76-87.
  4. Kablov E.N., Kutyrev A.E., Vdovin A.I., Kozlov I.A., Afanasyev-Khodykin A.N. The research of possibility of galvanic corrosion in brazed connections used in aviation engine construction. Aviation materials and technologies, 2021, no. 4 (65), paper no. 01. Available at: http://www.journal.viam.ru (accessed: May 12, 2022). DOI: 10.18577/2713-0193-2021-0-4-3-13.
  5. Konovalov V.V., Dubinskiy S.V., Makarov A.D., Dotsenko A.M. Research of correlation dependencies between mechanical properties of aviation materials. Aviacionnye materialy i tehnologii, 2018, no. 2 (51), pp. 40–46. DOI: 10.18577/2071-9140-2018-0-2-40-46.
  6. Plokhikh A.I., Safonov M.D., Kolesnikov A.G., Karpukhin S.D. Mechanism of interlaminar stress relaxation in multilayer steel materials. Aviacionnye materialy i tehnologii, 2018, no. 2 (51), pp. 26–32. DOI: 10.18577/2071-9140-2018-0-2-26-32.
  7. Kurs M.G., Nikolayev E.V., Abramov D.V. Full-scale and accelerated tests of metallic and nonmetallic materials: key factors and specialized stands. Aviacionnye materialy i tehnologii, 2019, no. 1 (54), pp. 66–73. DOI: 10.18577/2071-9140-2019-0-1-66-73.
  8. Zakirova L.I., Laptev A.B. Properties of protective electroplating coatings for replacement of cadmium on steel fixing parts (review). Part 1. Morphology and corrosion resistance. Aviaсionnye materialy i tehnologii, 2020, no. 3 (60), pp. 37–46. DOI: 10.18577/2071-9140-2020-0-3-37-46.
  9. Kozlov I.A., Leshchev K.A., Nikiforov A.A., Demin S.A. Cold spray coatings (review). Trudy VIAM, 2020, no. 8 (90), paper no. 08. Available at: http://www.viam-works.ru (accessed: May 4, 2022). DOI: 10.18577/2307-6046-2020-0-8-77-93.
  10. Abiev R.Sh., Bibik E.E., Vlasov E.A. et al. New reference book of a chemist and technologist. Electrode processes. Chemical kinetics and diffusion. colloidal chemistry. St. Petersburg: Professional, 2004, 838 p.
  11. Kosarev V.F., Alkhimov A.P. Technology, equipment, tools. Obrabotka metallov, 2003, no. 3, pp. 28–30.
  12. Alkhimov A.P., Gulidov A.I., Kosarev V.F., Nesterovich N.I. Peculiarities of deformation of microparticles upon impact with a solid barrier. Prikladnaya mekhanika i tekhnicheskaya fizika, 2000, vol. 41, no. 1, pp. 204–209.
  13. Alkhimov A.P., Klinkov S.V., Kosarev V.F., Fomin V.M. Cold gas-dynamic spraying. Theory and practice. Moscow: Fizmatlit, 2010, 536 p.
  14. Alkhimov A.P., Kosarev V.F., Papyrin A.N. The method of "cold" gas-dynamic. DAN SSSR, 1990, vol. 315, no. 5, pp. 1062–1065.
  15. Baranov A.N., Guseva E.A., Komova E.M. Investigation of the corrosion resistance of steels used for the manufacture of dredge equipment for gold mining. Sistemy. Metody. Tekhnologii, 2014, no. 1 (21), pp. 102–106.
  16. Roslyakov V.I. Improving the corrosion resistance and reliability of household appliances during operation. Tekhniko-tekhnologicheskiye problemy servisa, 2012, no. 4 (22), pp. 29–32.
  17. Zamaletdinov I.I. Corrosion and protection of metals. Corrosion of powder materials: textbook. Perm: Perm. State Tech. University, 2007, pp. 18–19.
  18. Rossina N.G., Popov N.A., Zhilyakova M.A., Korelin A.V. Corrosion and protection of metals: textbook in 2 parts. Ekaterinburg: Ural University, 2019, part 1: Methods for studying corrosion processes, p. 108.