Nacharkina A.V., Zelenina I.V., Valueva M.I., Barbotko S.L. Fire safety of high-temperature carbon fiber reinforced plastics for aviation purposes (review) // Proceedings of VIAM. 2022. No. 7 (113). Ст. 12. URL: https://www.viam-works.ru. DOI: 10.18577/2307-6046-2022-0-7-134-150.

Fire safety of high-temperature carbon fiber reinforced plastics for aviation purposes (review)

Nacharkina A.V., Zelenina I.V., Valueva M.I., Barbotko S.L.
Abstract

Presents the results of studies of the fire safety parameters of high-temperature carbon fiber reinforced plastics made on the basis of various heat-resistant polymer binders, conducted in order to determine the possibility of their potential application in the designs of aircraft products, from the point of view of compliance with the requirements of regulatory documents in the field of aviation fire safety. It is shown that the considered carbon plastics have high values of fire safety characteristics and can be used in aircraft products.

Keywords
fire safety, polymer composite materials, carbon fiber reinforced plastics (CFRP), high-temperature CFRP, aircraft products
Reference list
  1. Transport category airplanes: 14 CFR Part 25 – Airworthness standards. Available at: http:www.faa.gov/regulations_policies/faa_regulations (accessed: February 07, 2022).
  2. Certification Specifications for Large Aeroplanes – CS-25. European Aviation Safety Agency, 2003, 473 p.
  3. Mikhailin Yu.A. Heat-resistant polymers and polymeric materials. St. Petersburg: Professiya, 2006, 624 p.
  4. Mouritz A.P., Gibson A.G. Fire Properties of Polymer Composite Materials. Springer, 2006, 398 p.
  5. Bychikhina L.V., Vorobyov V.N., Groshev Yu.M., Monastyrskaya E.V. Methods for studying the combustibility and fire safety of polymeric materials. Methods of testing and research of polymeric materials for aircraft construction. Moscow: VIAM, 1977, pp. 11.
  6. Airworthiness standards for very light aircraft: AP-OLS: approved by Resolution of the 25th session of the Council on Aviation and the Use of Airspace 05/12/2006. St. Petersburg: SZ RCAI, 2006, 100 p.
  7. Airworthiness standards for civil light aircraft: AP-23: approved by Decree of the 38th session of the Council on Aviation and the Use of Airspace on December 16, 2021. 4th ed. St. Petersburg: SZ RCAI, 2021, 216 p.
  8. Airworthiness standards for transport category aircraft: AP-25: approved by Resolution of the 37th session of the Council on Aviation and the Use of Airspace on April 27, 2020. 6th ed. St. Petersburg: SZ RCAI, 2020, 328 p.
  9. Airworthiness standards for rotorcraft of normal category: AP-27: approved by Resolution of the 37th session of the Council on Aviation and the Use of Airspace on April 27, 2020. 3rd ed. St. Petersburg: SZ RCAI, 2020, 129 p.
  10. Airworthiness standards for transport category rotorcraft: AP-29: approved by Resolution of the 37th session of the Council on Aviation and the Use of Airspace on April 27, 2020. 4th ed. St. Petersburg: SZ RCAI, 2020, 186 p.
  11. Airworthiness standards for aircraft engines: AP-33: approved by Resolution of the 36th session of the Council on Aviation and the Use of Airspace on March 15, 2018. 4th ed. with amendments 1–3. St. Petersburg: SZ RCAI, 2020, 81 p.
  12. Fire Safety Aspects of Polymeric Material. Vol. 6. Aircraft: Civil and Military. Washington D.C.: Publication NMAB 318-6, National Materials Advisory Board, 1977, 268 p.
  13. Barbotko S.L., Volny O.S., Bochenkov M.M. Analysis of the US Federal Aviation Administration proposals for the reform of aviation standards regarding the fire safety of used materials (review). Trudy VIAM, 2020, no. 6–7 (89), paper no. 11. Available at: http://www.viam-works.ru (accessed: February 7, 2022). DOI: 10.18577/2307-6046-2020-0-67-101-117.
  14. 1/4 Scale fire penetration testing of composite fuselage. Sixth triennial international fire & cabin safety research conference. Atlantic City, 2010. 22 p.
  15. Lyon R.E. Nongalogen fire-resistant plastics for aircraft interiors: technical report. DOT/FAA/AR-TN08/5. Springfield, Virginia: U.S. Department of Transportation Federal Aviation Administration, 2008, 33p.
  16. Sohel R., Fangueiro R. Advanced Composite Materials for Aerospace Engineering: Processing, Properties and Applications. Woodhead Publishing; Elsevier, 2016, 474 p.
  17. Mukhametov R.R., Petrova A.P. Thermosetting binders for polymer composites (review). Aviacionnye materialy i tehnologii, 2019, no. 3 (56), pp. 48–58. DOI: 10.18577/2071-9140-2019-0-3-48-58.
  18. Tkachuk A.I., Terekhov I.V., Gurevich Ya.M., Grigoreva K.N. Research of the influence of the modifying additives nature on the rheological and thermomechanical properties of a photopolymer composition based on epoxy vinyl ester resin. Aviacionnye materialy i tehnologii, 2019, no. 3 (56), pp. 31–40. DOI: 10.18577/2071-9140-2019-0-3-31-40.
  19. Sidorina A.I. Multiaxial carbon fabrics in the products of aviation technology (review). Aviation materials and technologies, 2021, no. 3 (64), paper no. 10. Available at: http://www.journal.viam.ru (accessed: April 11, 2025). DOI: 10.18577/2713-0193-2021-0-3-105-116.
  20. Barbotko S.L., Volny O.S., Kirienko O.A., Shurkova E.N. Evaluation of the fire safety of polymeric materials for aviation purposes: state analysis, test methods, development prospects, methodological features. Ed. E.N. Kablov. Moscow: VIAM, 2018, 424 p.
  21. Garashchenko A.N., Berlin A.A., Kulkov A.A. Methods and means of ensuring the required indicators of fire safety of structures made of polymer composites (review). Pozharovzryvobezopasnost, 2019, vol. 28, no. 2, pp. 9–30.
  22. Flame Retardant Chemicals: Technologies and Global Markets. BCC Research, 2018, 128 p.
  23. Barbotko S.L., Volny O.S., Bochenkov M.M. Analysis of the US Federal Aviation Administration proposals for the reform of aviation standards regarding the fire safety of used materials (review). Trudy VIAM, 2020, no. 6–7 (89), paper no. 11. Available at: http://www.viam-works.ru (accessed: February 7, 2022). DOI: 10.18577/2307-6046-2020-0-67-101-117.
  24. Buravov B.A., Bochkarev E.S., Al-Khamzawi A. et al. Current trends in the development of flame retardants for polymer compositions. Composition, properties, application. Izvestiya Volgogradskogo Gosudarstvennogo Tehnicheskogo Universiteta, 2020, no. 12 (247), pp. 7–24.
  25. Aseeva R.M., Zaikov G.E. Combustion of polymeric materials. Moscow: Khimiya, 1981. 280 p.
  26. Mikhailin Yu.A. Heat, thermal and fire resistance of polymeric materials. St. Petersburg: Nauchnye osnovy i tekhnologii, 2011, 416 p.
  27. Berlin A.A. Combustion of polymers and low flammability polymeric materials. Sorosovskiy obrazovatelnyy zhurnal, 1996, no. 9, рр. 57–63.
  28. Mittal K.L. Polyimides and Other High Temperature Polymers: Synthesis, Characterization and Applications. Utrecht: VSP, 2005, 570 p.
  29. Global Forecast for High Temperature Composite Resin (2023–2028 Outlook) – High Tech & Emerging Markets Report. Available at: https://www.marketresearch.com/Barnes-Reports-v2737/Global-Forecast-High-Temperature-Composite-30844419/ (accessed: February 10, 2022).
  30. Valueva M.I., Zelenina I.V., Zharinov M.A., Khaskov M.A. High-temperature carbon plastics based on thermosetting polyimide binder. Voprosy materialovedeniya, 2020, no. 3 (103), pp. 89–102.
  31. Sastri S.B., Armistead J.P., Keller T.M. Flame resistant phthalonitrile composites. Washington, DC: Naval Research Lab., International Aircraft fire and cabin safety research conference, 1998, 12 р. Available at: http://www.semanticscolar.org/paper/FLAME-RESISTANT-PHTALONITRILE-COMPOSITES-Sastri-Armistead/70a8302ea6967bb346122bcc16a8dd54ff17bd77 (дата обращения: 07.02.2022).
  32. Raskutin A.E. Heat-resistant carbon plastics for aircraft structures operating at temperatures up to 400 °C: thesis, Cand. Sc. (Tech.). Moscow, 2007, 166 p.
  33. Zelenina I.V., Gulyayev I.N., Kucherovskiy A.I., Mukhametov R.R. Heat-resistant CFRP for the impulse wheel of the centrifugal compressor. Trudy VIAM, 2016, no. 2 (38), paper no. 08. Available at: http://www.viam-works.ru (accessed: February 7, 2022). DOI: 10.18577/2307-6046-2016-0-2-8-8.
  34. Kablov E.N., Valueva M.I., I.V. Zelenina, Khmelnitskiy V.V., Aleksashin V.M. Carbon plastics based on benzoxazine oligomers – perspective materials. Trudy VIAM, 2020, no. 1, paper no. 07. Available at: http://www.viam-works.ru (accessed: February 7, 2022). DOI: 10.18577/2307-6046-2020-0-1-68-77.
  35. Gunyaeva A.G., Kurnosov A.O., Gulyaev I.N. High-temperature polymer composite materials developed FSUE «VIAM» for aero-space engineering: past, present and future (review). Trudy VIAM, 2021, no. 1 (95), paper no. 05. Available at: http://www.viam-works.ru (accessed: February 7, 2022). DOI: 10.18577/2307-6046-2021-0-1-43-53.
  36. Ishida H., Froimowicz P. Advanced and Emerging Polybenzoxazine Science and Technology. Elsevier, 2017. 1126 p.
  37. Kablov E.N. The role of fundamental research in the creation of new generation materials. Reports of XXI Mendeleev Congress on General and Applied Chemistry: in 6 vols. St. Petersburg, 2019, vol. 4, pp. 24.
  38. Chand S. Review Carbon fibers for composites. Journal of Materials Science, 2000, no. 35, pp. 1303–1313.
  39. Constantin L., Fan L., Pouey M. et al. Spontaneous formation of multilayer refractory carbide coatings in a molten salt media. Proceedings of the National Academy of Sciences of the United States of America, 2021, no. 118 (18). Available at: https://www.researchgate.net/publication/351245744 (accessed: February 07, 2022).
  40. Airworthiness standards for civil aircraft of the USSR. Ed. 3rd. Moscow: TsAGI, 1984, 464 p.
  41. ISO 13344:2015. Estimation of the lethal toxic potency of fire effluents. International Organization for Standardization. 2015. 20 p.
  42. Methods for determining compliance with the Federal Aviation Rules “Instance of an aircraft. Requirements and certification procedure”: approved by Order of the Ministry of Transport of the Russian Federation No. 132 of May 16, 2003. Moscow, 2004, 53 p.