Petrova A.P., Lukina N.F., Isaev A.Yu., Smirnov O.I. The effect of the adhesive primer EP-0234 on the properties of adhesive compounds obtained using adhesive VK-36 // Proceedings of VIAM. 2022. No. 6 (112). Ст. 04. URL: https://www.viam-works.ru. DOI: 10.18577/2307-6046-2022-0-6-39-48.

The effect of the adhesive primer EP-0234 on the properties of adhesive compounds obtained using adhesive VK-36

Petrova A.P., Lukina N.F., Isaev A.Yu., Smirnov O.I.
Abstract

It is shown that the use of EP-0234 epoxy primer, used as an adhesive sublayer under VK-36 epoxy-polysulfone adhesive leads to an increase in the holding time between the process of chemical oxidation in chromic acid (An.Ox.chrome) of the glued surfaces of aluminum alloys and the start of technological bonding work for up to 30 days (instead of 2 days for anodized surfaces without primer) without deterioration of the glued samples, and in some cases – to their improvement.

Keywords
adhesive film, adhesive primer, strength of adhesive joints, thermal aging, resistance to moisture, vibration, long-term strength
Reference list
  1. Kozlov V.A., Lyakin V.I., Kiselev V.Ya. Influence of surface modification of vulcanized rubbers on adhesive strength. Klei. Germetiki. Tekhnologii, 2006, no. 12, pp. 11–15.
  2. Kirillov V.N., Vapirov Yu.M., Drozd E.A. Research of atmospheric firmness of polymeric composite materials in the conditions of the atmosphere of warm wet and moderately warm climate. Aviacionnye materialy i tehnologii, 2012, no. 4, pp. 31–38.
  3. Petrova A.P., Lukina N.Ph., Isaev A.Yu. Operability of glued joints on epoxy film adhesives at simultaneous influence of loadings and climatic factors. Trudy VIAM, 2019, no. 9 (81), paper no. 06. Available at: http://www.viam-works.ru (accessed: March 16, 2022). DOI: 10.18577/2307-6046-2019-0-9-47-56.
  4. Fedoseev M.S., Shcherban' M.G., Derzhavinskaya L.F. Increasing the adhesion of epoxy adhesive compositions to aluminum using promoters of epoxy- and aminoalkoxysilanes. Klei. Germetiki. Tekhnologii, 2020, no. 5, pp. 7–13.
  5. Aronovich D.A., Varlamov V.P., Voitovich V.A. et al. Bonding in mechanical engineering: reference book. Moscow: Nauka i tehnologii, 2005, vol. 1, 544 p.
  6. Laptev A.B., Barbotko S.L., Nikolaev E.V. The main research areas of the persistence properties of materials under the influence of climatic and operational factors. Aviacionnye materialy i tehnologii, 2017, no. S, pp. 547–561. DOI: 10.18577/2071-9140-2017-0-S-547-561.
  7. Startsev O.V., Prokopenko K.O., Litvinov A.A. et al. Investigation of thermal moisture aging of aviation fiberglass. Klei. Germetiki. Tekhnologii, 2009, no. 8, pp. 18–22.
  8. Petrovа А.Р., Kuznetsova V.А., Lukina N.Ph., Isayev A.Yu. Influence of corrosion inhibit-ing primer on properties of the glued joints executed using organic silicon glue-hermetic. Trudy VIAM, 2020, no. 10 (92), paper no. 02. Available at: http://www.viam-works.ru (accessed: March 03, 2022). DOI: 10.18577/2307-6046-2020-0-10-13-20.
  9. Aviation materials: reference book in 13 vols. Ed. E.N. Kablov. Moscow: VIAM, 2019, vol. 10, part 1: Adhesives. Adhesive prepregs, pp. 17–20.
  10. Kablov E.N. Innovative developments of FSUE «VIAM» SSC of RF on realization of «Strategic directions of the development of materials and technologies of their processing for the period until 2030». Aviacionnye materialy i tehnologii, 2015, no. 1 (34), pp. 3–33. DOI: 10.18577/2071-9140-2015-0-1-3-33.
  11. Kablov E.N. Russia in the market of intellectual resources. Ekspert, 2015, no. 28 (951), pp. 48–51.
  12. Kablov E.N. What is the future to be made of? Materials of a new generation, technologies for their creation and processing – the basis of innovation. Krylya Rodiny, 2016, no. 5, pp. 8–18.
  13. Petrova A.P., Anikhovskaya L.I. Influence of adhesive primer EP-0234 on the properties of adhesive joints made with phenol-rubber adhesive VK-50. Klei. Germetiki. Tekhnologii, 2016, no. 1, pp. 19–24.
  14. Potsius A.V. Adhesives, adhesion, bonding technology: trans. from Engl. St. Petersburg: Profession, 2007, 376 p.
  15. Tsverava V.G., Rusin M.Yu., Nepovinnykh V.I., Himitsaev A.S. Analysis of the influence of accelerated climatic aging on the strength of adhesive joints. Klei. Germetiki. Tekhnologii, 2018, no. 8, pp. 28–31.
  16. Isaev A.Yu., Rubtsova E.V., Kotova E.V., Sutyagin M.N. Research of properties of glues and glue binding, made with use of modern domestic component base. Trudy VIAM, 2021, no. 3 (97), paper no. 05. Available at: http://www.viam-works.ru (accessed: October 6, 2021). DOI: 10.18577/2307-6046-2021-0-3-58-67.
  17. Nikolaev E.V., Kirillov V.N., Skirta A.A., Grashhenkov D.V. Study of moisture transport rules and development of a standard on measurement of the diffusion coefficient and moisture content limit to evaluate mechanical properties of carbon fiber reinforced plastics. Aviacionnye materialy i tehnologii, 2013, no. 3, pp. 44–48.
  18. Kablov E.N., Laptev A.B., Prokopenko A.N., Gulyaev A.I. Relaxation of polymeric composite materials under the prolonged action of static load and climate (review). Part 1. Binders. Aviation materials and technologies, 2021, no. 4 (65), paper no. 08. Available at: http://www.journal.viam.ru (accessed: February 6, 2022). DOI: 10.18577/2071-9140-2021-0-4-70-80.