Bespalova E.E., Beljaev А.А., Devin K.L. Low density radio engineering materials (review) // Proceedings of VIAM. 2022. No. 4 (110). Ст. 08. URL: https://www.viam-works.ru. DOI: 10.18577/2307-6046-2022-0-4-75-83.

Low density radio engineering materials (review)

Bespalova E.E., Beljaev А.А., Devin K.L.
Abstract

The article is devoted to the creation of radio-absorbing polymer composite materials of a dielectric type of reduced density. The main characteristics of a number of developed domestic and foreign foamed radio-absorbing materials are given, the technologies for their production, the scope of application are described and the features of radio-absorbing materials for use in anechoic camera are considered. The characteristics of the reduced density radio-absorbing materials developed at the Kurchatov Institute Research Center – VIAM are given.

Keywords
radio engineering materials, radio absorbing materials, porous materials, polymer composite materials, the lowered density, materials for anechoic camera, absorbers of electromagnetic waves
Reference list
  1. Zhelezina G.F., Solovyeva N.A., Makrushin K.V., Rysin L.S. Polymer composite materials for manufacturing engine air particle separation of advanced helicopter engine. Aviacionnye materialy i tehnologii, 2018, no. 1 (50), pp. 58–63. DOI: 10.18577/2071-9140-2018-0-1-58-63.
  2. Kablov E.N. Trends and guidelines for Russia's innovative development: Collection scientific-inform. materials. Moscow: VIAM, 2015, pp. 530–538.
  3. Devin K.L., Agafonova A.S., Sokolov I.I. Prospects for the use of radio-absorbing materials to ensure electromagnetic compatibility of avionics. Trudy VIAM, 2020, no. 8 (90), paper no. 09. Available at: http://www.viam-works.ru (accessed: November 22, 2021). DOI: 10.18577/2307-6046-2020-0-8-94-100.
  4. Mikhailin Yu.A. Special polymer composite materials. St. Petersburg: Nauchnye osnovy i tekhnologii, 2014, pp. 171–450.
  5. Boiprav O.V., Lobunov V.V., Lynkov L.M., Al-Mashat E.A.A. Research of interaction of infrared wave-length range electromagnetic radiation with radio-absorbent materials based on metal-containing elements. Aviacionnye materialy i tehnologii, 2020, no. 2 (59), pp. 89–94. DOI: 10.18577/2071-9140-2020-0-2-89-94.
  6. Bespalova E.E., Belyaev A.A., Shirokov V.V. Radar-absorbing materials for protection against high power microwave radiation. Trudy VIAM, 2015, no. 3, paper no. 07. Available at: http://www.viam-works.ru (accessed: March 17, 2022). DOI: 10.18577/2307-6046-2015-0-3-7-7.
  7. Kovneristy Yu.K., Lazareva I.Yu., Ravaev A.A. Materials that absorb microwave radiation. Moscow: Nauka, 1982, 164 p.
  8. Belyaev A.A., Bespalova E.E., Romanov A.M. Fireproof radio absorbing materials for anechoic cameras. Aviacionnye materialy i tehnologii, 2013, no. 1, pp. 53–55.
  9. Belyaev A.A., Agafonova A.S., Antipova E.A., Botanogova E.D. Constructional radio absorbing material of three-layered structure with approval layer. Trudy VIAM, 2013, no. 7, paper no. 02. Available at: http://www.viam-works.ru (accessed: November 22, 2021).
  10. Bespalova E.E., Kondrashov E.K. Features of updating of a composition of a fireproof material for anechoic chambers when changed of parameters radio absorbing filler. Aviacionnye materialy i tehnologii, 2014, no. 2, pp. 48–52. DOI: 10.18577/2071-9140-2014-0-2-48-52.
  11. Mikhailin Yu.A. Fibrous polymeric composite materials in engineering. St. Petersburg: Nauchnye osnovy i tekhnologii, 2013. 720 p.
  12. Mitsmakher M. Yu., Torgovanov V.A. Anechoic microwave chambers. Moscow: Radio i svyaz, 1982, pp. 89–95.
  13. Bogush V.A., Borbotko T.V., Gusinsky A.V. etc. Electromagnetic radiation. Methods and means of protection. Minsk: Bestprint, 2003, 401 p.
  14. Miychenko I.P. Technology of semi-finished products of polymeric materials. St. Petersburg: Nauchnye osnovy i tekhnologii, 2012, 373 p.
  15. Volkov V.P., Zelenetsky A.N., Sizova M.D. Obtaining radioprotective polymeric materials of low combustibility. Plasticheskiye massy, 2008, no. 6, pp. 42–46.
  16. Grashchenkov D.V., Shchetanov B.V., Tinyakova E.V., Shcheglova T.M. About possibility of use of quartz fiber as lightweight heat-protective material binding at receiving on the basis of Al2O3 fibers. Aviacionnye materialy i tehnologii, 2011, no. 4, pp. 8‒14.
  17. Aristova Е.Yu., Denisova V.А., Drozhzhin V.S. et al. Composite materials using hollow microspheres. Aviacionnye materialy i tehnologii, 2018, no. 1 (50), pp. 52–57. DOI: 10.18577/2071-9140-2018-0-1-52-57.
  18. Polymer composite materials: structure, properties, technology: textbook. Ed. A.A. Berlin. 3rd ed. St. Petersburg: Professiya, 2011, pp. 298–301.
  19. Bibikov S.B., Smolnikova O.N., Prokofiev M.V. Dielectric properties and microwave conductivity of porous radio-absorbing materials. Radiotekhnika, 2011, no. 3, pp. 62–76.
  20. Kablov E.N. Innovative developments of FSUE «VIAM» SSC of RF on realization of «Strategic directions of the development of materials and technologies of their processing for the period until 2030». Aviacionnye materialy i tehnologii, 2015, no. 1 (34), pp. 3–33. DOI: 10.18577/2071-9140-2015-0-1-3-33.
  21. Kablov E.N. The role of chemistry in the creation of new generation materials for complex technical systems. Reports XX Mendeleev Congress on General and Applied Chemistry. Ekaterinburg: Ural Branch of the Russian Academy of Sciences, 2016, pp. 25–26.
  22. Kablov E.N., Semenova L.V., Petrova G.N., Larionov S.A., Perfilova D.N. Polymer composite materials on a thermoplastic matrix. Izvestiya vysshikh uchebnykh zavedeniy, ser.: Khimiya i khimicheskaya tekhnologiya, 2016, vol. 59, no. 10, pp. 61–71.
  23. Lushina M.V., Parshin S.G., Rzhevsky A.A. Modern shielding and radio-absorbing materials. Sistemy upravleniya i obrabotka informatsii, 2011, no. 22, pp. 208–214, 223.
  24. Radar-absorbing materials like "Moss". Available at: http://www.radiostrim.ru/220-moh.htm (accessed: November 27, 2020).
  25. Radio-absorbing material. Available at: http://https://tesart.ru/products/item/amp/ (accessed: November 27, 2020).
  26. Emerson and Cuming_Microwave products. Available at: http://eltm.ru/editor/upload-files/Cuming_Microwave.pdf (accessed: November 27, 2020).
  27. RPM Frankonia PF foam type. Available at: http://radio.vilcom.ru/products/radiopogloshaushie_ materialy/549 (accessed: November 27, 2020).