Zavarzin S.V., Oglodkov M.S., Chesnokov D.V., Kozlov I.A. Hot corrosion and protection of materials of gas turbine engines (review) // Proceedings of VIAM. 2022. No. 3 (109). Ст. 11. URL: https://www.viam-works.ru. DOI: 10.18577/2307-6046-2022-0-3-121-134.

Hot corrosion and protection of materials of gas turbine engines (review)

Zavarzin S.V., Oglodkov M.S., Chesnokov D.V., Kozlov I.A.
Abstract

In this paper, we consider the issues of the mechanism of hot corrosion. The analysis of modern methods of laboratory research of corrosion processes occurring at elevated temperatures is carried out. A significant part of the work is devoted to modern technology of protection against corrosion of metallic materials. The development of technologies for slurry, chemical, pyrochemical, electrochemical and sol-gel coatings, as well as methods of diffusion saturation of the surface, is relevant today. Nevertheless, the technology of ion-plasma treatment is the most effective method of applying protective coatings.

Keywords
high-temperature corrosion, hot corrosion, sulfide-oxide corrosion, sodium sulfate, sodium chloride, protective coatings, ion-plasma treatment
Reference list
  1. Prashar G., Vasudev H. Hot corrosion behavior of super alloys. Materials Today: Proceedings, 2020, vol. 26, pp. 1131–1135.
  2. Reid W.T. External corrosion and deposits: boilers and gas turbines. New York: Elesevier, 1971, 199 p.
  3. Lai G.Y. High-temperature corrosion and materials applications. ASM International, 2007, 461 p.
  4. Rapp R.A. Hot corrosion of materials: a fluxing mechanism? Corrosion science, 2002, vol. 44, no. 2, pp. 209–221.
  5. Tschinkel J.G. Formation of sodium sulfate in gas turbine combustors. Corrosion, 1972, vol. 28, no. 5, pp. 161–169.
  6. Stringer J. High-temperature corrosion of superalloys. Materials Science and Technology, 1987, vol. 3, no. 7, pp. 482–493.
  7. Eliaz N., Shemesh G., Latanision R.M. Hot corrosion in gas turbine components. Engineering failure analysis, 2002, vol. 9, no. 1, pp. 31–43.
  8. Gupta D.K., Rapp R.A. The Solubilities of NiO, Co3O4, and Ternary Oxides in Fused Na2SO4 at 1200 K. Journal of the Electrochemical Society, 1980, vol. 127, no. 10, pp. 2194–2201.
  9. Zhang Y.S., Rapp R.A. Solubility of α‐Fe2O3 in Fused Na2SO4 at 1200 K. Journal of the Electrochemical Society, 1985, vol. 132, no. 3, pp. 734.
  10. Zhang Y.S. Solubilities of Cr2O3 in Fused Na2SO4 at 1200 K. Journal of the Electrochemical Society, 1986, vol. 133, no. 3, pp. 655.
  11. Jose P.D., Gupta D.K., Rapp R.A. Solubility of α‐Al2O3 in Fused Na2SO4 at 1200 K. Journal of the Electrochemical Society, 1985, vol. 132, no. 3, pp. 735.
  12. Spengler C.J., Viswanathan R. Effect of sequential sulfidation and oxidation on the propagation of sulfur in an 85 Ni–15 Cr alloy. Metallurgical and Materials Transactions B, 1972, vol. 3, no. 1, pp. 161–166.
  13. El-Dahshan M.E., Whittle D.P., Stringer J. Effect of presulfidation on the oxidation behavior of Co-based alloys. Part I. Presulfidation at sulfur partial pressures above the dissociation pressure of cobalt sulfide. Oxidation of metals, 1974, vol. 8, no. 4, pp. 179–209.
  14. Hancock P. Vanadic and chloride attack of superalloys. Materials Science and Technology, 1987, vol. 3, no. 7, pp. 536–544.
  15. Rapp R.A., Goto K.S. The hot corrosion of metals by molten salts. ECS Proceedings Volumes, 1981, vol. 10, pp. 159–177.
  16. Otsuka N., Rapp R.A. Hot Corrosion of Preoxidized Ni by a Thin Fused Na2SO4 Film at 900 °C. Journal of the Electrochemical Society, 1990, vol. 137, no. 1, pp. 46–52.
  17. Zhang X., Rapp R.A. Electrochemical Impedance of a Platinum Electrode in Fused Na2SO4 Melts in SO2‒O2 Environments. Journal of the Electrochemical Society, 1993, vol. 140, no. 10, pp. 2857–2862.
  18. Numata H., Nishikata A., Haruyama S. Electrochemical studies of corrosion of iron, nickel and nickel alloys in alkali sulfate melt. Transactions of the Japan Institute of Metals, 1983, vol. 24, pp. 303–310.
  19. Fang W.C., Rapp R.A. Electrochemical Reactions in a Pure Na2SO4 Melt. Journal of the Electrochemical Society, 1983, vol. 130, no. 12, pp. 2335–2340.
  20. McKee D.W., Romeo G. Carbon deposition and the role of reducing agents in hot-corrosion processes. Metallurgical Transactions, 1973, vol. 4, no. 8, pp. 1877–1885.
  21. Barklow R.H., Goebel J.A., Pettit F.S. Erosion-corrosion of coatings and superalloys in high-velocity hot gases. ASTM special technical publication, 1979, no. 664, pp. 163–192.
  22. Kameswari S. The role of NaCl in the hot-corrosion behavior of nimonic alloy 90. Oxidation of metals, 1986, vol. 26, no. 1, pp. 33‒44.
  23. Hancock P.J., Hancock H.A., Caley W.F. et al. A review of recent studies of the role of zinc as an inhibitor of hot corrosion from molten sulphates. Materials Science and Engineering A, 1989, vol. 120, pp. 313–318.
  24. Donachie M.J.Jr., Sprague R.A., Russell R.N. et al. Sulfidation of Hot Section Alloys in Gas Turbine Engines. ASTM Special Technical Publication, 1967, no. 421, pp. 85–105.
  25. Shubin I.Yu., Nikitin Ya.Yu., Puchkov Yu.A. et al. Investigation of resistance to high-temperature gas and salt corrosion of high-temperature intermetallic titanium alloy VTI-4. Vestnik MGTU im. N.E. Bauman. Ser.: Mechanical engineering, 2020, no. 6, pp. 84–106.
  26. Goward G.W. Progress in coatings for gas turbine airfoils. Surface and coatings technology, 1998, vol. 108, pp. 73–79.
  27. Nicholls J.R. Designing oxidation-resistant coatings. JOM, 2000, vol. 52, no. 1, pp. 28–35.
  28. Narushko E.O. Protective coatings against high-temperature gas corrosion of axial compressor blades in the aircraft industry. BNTU repository, 2011, pp. 110–115. Available at: https://rep.bntu.by (accessed: December 03, 2021).
  29. Longa-Nava Y., Zhang Y.S., Takemoto M. et al. Hot corrosion of nickel-chromium and nickel-chromium-aluminum thermal-spray coatings by sodium sulfate-sodium metavanadate salt. Corrosion, 1996, vol. 52, no. 09, pp. 680–689.
  30. Muboyadzhyan S.A., Budinovsky S.A. Condensed and condensation-diffusion coatings for turbine blades from heat-resistant alloys with a directional crystal structure. Metallovedenie i termicheskaya obrabotka metallov, 1996, no. 4, pp. 15–18.
  31. Kablov E.N., Muboyadzhyan S.A., Budinovsky S.A., Lutsenko A.N. Ion-plasma protective coatings for blades of gas turbine engines. Metally, 2007, no. 5, pp. 23–34.
  32. Kablov E.N., Nikiforov A.A., Demin S.A., Chesnokov D.V., Vinogradov S.S. Promising coatings for corrosion protection of carbon steels. Stal, 2016, no. 6, pp. 70–81.
  33. Solncev S.S., Denisova V.S., Rozenenkova V.A. Reaction cure – the new direction in technology ofhigh-temperature composite coatings and materials. Aviacionnye materialy i tehnologii, 2017, no. S, pp. 329–343. DOI: 10.18577/2071-9140-2017-0-S-329-343.
  34. Goncharov B.E., Sipatov A.M., Cherkashneva N.N., Pleskan A.Yu., Samokhvalov N.Yu., Vaganova M.L., Sorokin O.Yu., Solntsev St.S., Evdokimov S.A. Studies of thermal shock resistance of an anti-oxidation coating for a multi-layered ceramic composite. Aviation materials and technologies, 2021, no. 4 (65), paper no. 06 (accessed: December 3, 2021). DOI: 10.18577/2713-0193-2021-0-51-58.
  35. Bianco R., Rapp R.A. Pack cementation diffusion coatings. Metallurgical and ceramic protective coatings, 1996, pp. 236–260.
  36. Sánchez L., Bolivar F.J., Hierro M.P. et al. Effect of Ce and La additions in low temperature aluminization process by CVD–FBR on 12 % Cr ferritic/martensitic steel and behaviour in steam oxidation. Corrosion science, 2008, vol. 50, no. 8, pp. 2318–2326.
  37. Jiang C.Y., Yang Y.F., Zhang Z.Y. et al. A Zr-doped single-phase Pt-modified aluminide coating and the enhanced hot corrosion resistance. Corrosion Science, 2018, vol. 133, pp. 406–416.
  38. Xu Z., Dai J., Niu J. et al. Isothermal oxidation and hot corrosion behaviors of diffusion aluminide coatings deposited by chemical vapor deposition. Journal of Alloys and Compounds, 2015, vol. 637, pp. 343–349.
  39. Picas J.A., Menargues S., Martin E. et al. Characterization of duplex coating system (HVOF + PVD) on light alloy substrates. Surface and coatings technology, 2017, vol. 318, pp. 326–331.
  40. Wänstrand O., Larsson M., Kassman-Rudolphi А. An experimental method for evaluation of the load-carrying capacity of coated aluminium: the influence of coating stiffness, hardness and thickness. Surface and Coatings Technology, 2000, vol. 127, no. 2–3, pp. 107–113.
  41. Tang P., He D., Li W. et al. Achieving superior hot corrosion resistance by PVD/HVOF duplex design. Corrosion Science, 2020, vol. 175, art. 108845. DOI: 10.1016/j.corsci.2020.108845.
  42. Doleker K.M., Ozgurluk Y., Kahraman Y. et al. Oxidation and hot corrosion resistance of HVOF/EB-PVD thermal barrier coating system. Surface and Coatings Technology, 2021, vol. 409, art. 126862. DOI: 10.1016/j.surfcoat.2021.126862.
  43. Muboyadzhyan S.A., Budinovskij S.A. Ion-plasma technology: prospective processes, coatings, equipment. Aviacionnye materialy i tehnologii, 2017, no. S, pp. 39–54. DOI: 10.18577/2071-9140-2017-0-S-39-54.
  44. Muboyadzhyan S.A., Kablov E.N. Vacuum Plasma Technique of Protective Coatings Production of Complex Alloys. Metallovedenie i termicheskaya obrabotka metallov, 1995, no. 2, pp. 15–18.
  45. Budinovskij S.A., Muboyadzhyan S.A., Gayamov A.M., Kosmin A.A. Development and research of the combined heat resisting ion-plasma coverings for the heat resisting nickel alloys alloyed by a reniye. Aviacionnye materialy i tehnologii, 2008, no. 3 (8), pp. 3–11.
  46. Kablov E.N., Muboyadzhyan S.A. Erosion-Resistant Coatings for Gas Turbine Engine Compressor Blades. Russian metallurgy (Metally), 2017, vol. 2017, no. 6, pp. 494–504.
  47. Smirnov A.A., Budinovsky S.A. Improvement of heat resistance of condensation and diffusion coatings for turbine blades from ZhS32 alloy. Aviacionnye materialy i tehnologii, 2016, no. 2, pp. 3–10. DOI: 10.18577/2071-9140-2016-0-2-3-10.
  48. Gorlov D.S., Muboyadzhyan S.A., Shhepilov A.A., Aleksandrov D.A. The research of erosion resistance and heat resistance of the ion-plasma damping coatings. Aviacionnye materialy i tehnologii, 2016, no. 2, pp. 11–17. DOI: 10.18577/2071-9140-2016-0-2-11-17.
  49. Kosmin A.A., Budinovskiy S.A., Muboyadzhyan S.A. Heat and corrosion resistant coating for working turbine blades from promising high-temperature alloy VZhL21. Aviacionnye materialy i tehnologii, 2017, no. 1 (46), pp. 17–24. DOI: 10.18577/2071-9140-2017-0-1-17-24.
  50. Goyal K., Singh H., Bhatia R. Hot corrosion behaviour of carbon nanotubes reinforced chromium oxide composite coatings at elevated temperature. Materials Research Express, 2018, vol. 5, no. 11, art. 116408. DOI: 10.1088/2053-1591/aadc34.