Kondrashov S.V., Solovyanchik L.V., Larionov S.A., Volnyj O.S. Investigation of the effect of flame retardants on the flammability and fluidity of the melt of aliphatic polyamides // Proceedings of VIAM. 2022. No. 2 (108). Ст. 04. URL: https://www.viam-works.ru. DOI: 10.18577/2307-6046-2022-0-2-52-63.

Investigation of the effect of flame retardants on the flammability and fluidity of the melt of aliphatic polyamides

Kondrashov S.V., Solovyanchik L.V., Larionov S.A., Volnyj O.S.
Abstract

The paper presents the results of a study of the effect of fire retardants on the flammability and melt flow rate of aliphatic polyamides of the PA 66L, PA 610L, PA 66KS grades. The degree of this influence depends on the grade of polyamide, the type of fire retardant and its quantitative content. Among the selected grades of polyamides, polyamide PA 66L has the highest fluidity. The efficiency of using decabromodiphenyloxide and antimony trioxide to reduce the duration of residual combustion of polyamides of the studied brands is shown, compositions related to the category of «self-extinguishing» are determined.

Keywords
polyamide, flame retardants, modified compositions based on polyamides, thermoplastics, decabromodiphenyloxide, antimony trioxide, melt fluidity index, combustibility, self-extinguishing
Reference list
  1. Sorokin A.E., Sagomonova V.A., Petrova A.P., Solovyanchik L.V. Manufacturing technologies of polymer composite materials on thermoplastics (review). ). Trudy VIAM, 2021, no. 3 (97), paper no. 07. Available at: http://www.viam-works.ru (accessed: October 6, 2021). DOI: 10.18577/2307-6046-2021-0-3-78-86.
  2. Gurenkov V.M., Gorshkov V.О., Chebotarev V.P., Prudskova Т.N., Andreeva Т.I. Comparative analysis of properties of polyetheretherketone of domestic and foreign production. Aviacionnye materialy i tehnologii, 2019, no. 3 (56), pp. 41–47. DOI: 10.18577/2071-9140-2019-0-3-41-47.
  3. Gulyaev A.I., Medvedev P.N., Sbitneva S.V., Petrov A.A. Experimental research of «fiber–matrix» adhesion strength in carbon fiber epoxy/polysulphone composite. Aviacionnye materialy i tehnologii, 2019, no. 4 (57), pp. 80–86. DOI: 10.18577/2071-9140-2019-0-4-80-86.
  4. Kablov E.N., Kulagina G.S., Zhelezina G.F., Lons-kii S.L., Kurshev E.V. Microstructure research of the unidirectional organoplastic based on Rusar-NT aramid fibers and epoxy-polysulfone binder. Aviacionnye materialy i tehnologii, 2020, no. 4 (61), pp. 19–26. DOI: 10.18577/2071-9140-2020-0-4-19-26.
  5. Sorokin A.E., Bejder E.Ya., Izotova T.F., Nikolaev E.V., Shvedkova A.K. Investigation of carbon fiber reinforced plastic on polyphenylenesulfide resin after accelerated and natural climatic test. Aviacionnye materialy i tehnologii, 2016, no. 3 (42), pp. 66–72. DOI: 10.18577/2071-9140-2016-0-3-66-72.
  6. Berlin A.A. Combustion of polymers and low flammability polymeric materials. Sorovskiy obrazovatelnyy zhurnal, 1996, no. 4, pp. 16–24.
  7. Kopylov V.V., Novikov S.N., Oksentevich L.A. et al. Polymeric materials with reduced flammability. Moscow: Khimiya, 1986, 222 p.
  8. Mailhos-Lefievre V., Sallet D., Martel B. Thermal degradation of pure and flame-retarded polyamides 11 and 12. Polymer degradation and stability, 1989, vol. 23, no. 4, pp. 327–336.
  9. Chizhova M.A., Khairullin R.Z. Toxicity of combustion products of polymeric materials with the introduction of flame retardants into their composition. Vestnik Kazanskogo tekhnologicheskogo universiteta, 2014, vol. 17, no. 9, pp. 144.
  10. Dzivitskaya G.G., Khatenko A.S., Ostrovskaya L.E., Ksenofontov M.A. Influence of fire retardants on increasing the thermal stability and fire resistance of polyurethane foams. Abstracts of the XII Symposium "Modern Chemical Physics". Tuapse, 2000, p. 38.
  11. Bogdanova V.V. Fire-extinguishing effect of flame retardants in synthetic polymers and natural combustible materials. Chemical Problems of Creating New Materials and Technologies: collect. of articles. Minsk, 2003, is. 2, pp. 344–375.
  12. Levchik S.V., Balabanovich A.I., Levchik G.F., Costa L. Effect of melamine and its salts on combustion and thermal decomposition of polyamide 6. Fire and Materials, 1997, vol. 21, no. 2, pp. 75–83.
  13. Levchik S.V. Studies of the regularities of the action of fire retardants in aliphatic polyamides. Moscow: Khimiya, 1998, pp. 3–13.
  14. Borukaev T.A., Sablirova Yu.M., Mikitaev A.K. The use of boron compounds as effective flame retardants for polymeric materials. Materialovedenie, 2006, no. 5, pp. 29–34.
  15. Zaikov G.E., Artsis M.I. Flame retardants for the polymer industry. Plasticheskiye massy, 2000, no. 8, pp. 48–54.
  16. Borukaev T.A., Otarova R.M., Shaov A.Kh., Kharaev A.M. The influence of the addition of salts based on melamine and mineral acids on the fire resistance, physical and mechanical properties of polyamide-6 and polypropylene. Norwegian Journal of Development of the International Science, 2016, no. 1, pp. 20–25.
  17. Fang K., Li J., Ke C. et al. Intumescent flame retardation of melamine-modified montmorillonite on polyamide 6: Enhancement of condense phase and flame retardance. Polymer Engineering & Science, 2011, vol. 51, no. 2, pp. 377–385.
  18. Kostyuchenko M.A., Revyako M.M. Study of the influence of combined flame retardants "phosphorus + triazine" on the combustibility and performance properties of extruded polyamides. Trudy BGTU, 2012, no. 4, pp. 40–43.
  19. Platonov M.M., Petrova G.N., Larionov S.A., Barbotko S.L. Optimization of the composition of a polymer composition with a reduced fire hazard based on polycarbonate for 3D printing technology with a molten polymer thread. Izvestiya vysshikh uchebnykh zavedeniy. Ser.: Chemistry and chemical technology, 2017, vol. 60, no. 1, pp. 87–94.
  20. Petrova G.N., Rumyanceva T.V., Beyder E.Ya. Influence of modifying additives on fireproof properties and technological effectiveness of polycarbonate. Trudy VIAM, 2013, no. 6, paper no. 06. Available at: http://www.viam-works.ru (accessed: October 13, 2021).
  21. Petrova G.N., Beyder E.Ya. Increasing of fire resistance of polybutylene terephthalate (review). Aviacionnye materialy i tehnologii, 2014, No. 4, pp. 58–64. DOI: 10.18577/2071-9140-2014-0-4-58-64.
  22. Ermakova N.V. On the smoke-generating ability of finishing materials. Auditorium, 2017, no. 3 (15), pp. 104–107.
  23. Platonov M.M., Petrova G.N., Larionov S.A., Barbotko S.L. Polymer composition on the basis of polydodecanolactam for 3D-printing technology by melted polymer string. Trudy VIAM, 2016, no. 10, paper no. 9. Available at: http://www.viam-works.ru (accessed: October 13, 2021). DOI: 10.18577/2307-6046-2016-0-10-9-9.
  24. Petrova G.N., Sapego Yu.A., Larionov S.A., Platonov M.M., Laptev A.B. Fireproof thermoplastic materials for 3D-technologies. Trudy VIAM, 2017, no. 9, paper no. 07. Available at: http://www.viam-works.ru (accessed: October 13, 2021). DOI: 10.18577/2307-6046-2017-0-9-7-7.
  25. Ushkov V.A. Flammability and smoke-forming ability of polymer composite materials. Vestnik MGSU, 2017, vol. 12, no. 8 (107), pp. 897–903.
  26. Fox D.W. Thermally stable flame-retardant thermoplastic molding composition: pat. US 4028335; filed 23.08.76; publ. 07.06.77.
  27. Ohkawa Y. Flame-Retardant Polyamide Composition and Use Thereof: pat. US 10587713; filed 25.01.05; publ. 19.04.07.
  28. Baer M. Flame retardant resin compositions: pat. US 4205142; filed 02.11.77; publ. 27.05.80.
  29. Khalturinsky N.A., Rudakova T.A. Physical aspects of combustion of polymers and the mechanism of action of inhibitors. Khimicheskaya fizika, 2008, vol. 27, no. 6, pp. 73–84.
  30. Hu Y., Wang S., Ling Z. et al. Preparation and combustion properties of flame retardant nylon 6/montmorillonite nanocomposite. Macromolecular Materials and Engineering, 2003, vol. 288, no. 3, pp. 272–276.
  31. Kablov E.N. Innovative developments of FSUE «VIAM» SSC of RF on realization of «Strategic directions of the development of materials and technologies of their processing for the period until 2030». Aviacionnye materialy i tehnologii, 2015, no. 1 (34), pp. 3–33. DOI: 10.18577/2071-9140-2015-0-1-3-33.
  32. Kablov E.N. Aerospace materials science. Vse materialy. Entsiklopedicheskiy spravochnik, 2008, no. 3, pp. 2–14.
  33. Kablov E.N. Chemistry in aviation materials science. Rossiyskiy khimicheskiy zhurnal, 2010, vol. LIV, no. 1, pp. 3–4.
  34. Kablov E.N., Semenova L.V., Petrova G.N., Larionov S.A., Perfilova D.N. Polymer composite materials on a thermoplastic matrix. Izvestiya vysshikh uchebnykh zavedeniy. Ser.: Chemistry and chemical technology, 2016, vol. 59, no. 10, pp. 61–71.