Aleksandrov D.A., Gorlov D.S. The research of erosion resistance and residual stresses in layered ion-plasma coatings // Proceedings of VIAM. 2022. No. 12 (118). Ст. 08. URL: https://www.viam-works.ru. DOI: 10.18577/2307-6046-2022-0-12-87-95.

The research of erosion resistance and residual stresses in layered ion-plasma coatings

Aleksandrov D.A., Gorlov D.S.
Abstract

Presents the results of studies of various variants of layered erosion-resistant coatings based on titanium and zirconium nitrides, chromium carbide. Metallographic studies, studies of residual stresses, phase composition, tests for erosion resistance, endurance of samples with coatings were carried out. The dependence of erosion resistance, phase composition and stress-strain state of coatings on the energy parameters of the application process has been established. The influence of functional sublayers on the stress-strain state of the layered ion-plasma coating and its erosion resistance has been established.

Keywords
erosion resistance, residual stresses, ion-plasma coatings, titanium nitride, chromium carbide
Reference list
  1. Kablov E.N., Kashapov O.S., Pavlova T.V., Nochovnaya N.A. Development of a pilot industrial technology for the manufacture of semi-finished products from pseudo-alpha-titanium alloy VT41. Titan, 2016, no. 2 (52), pp. 33–42.
  2. Kablov E.N., Kashapov O.S., Medvedev P.N., Pavlova T.V. Study of a α + β-titanium alloy based on a system of Ti–Al–Sn–Zr–Si–β-stabilizing alloying elements. Aviacionnye materialy i tehnologii, 2020, no. 1 (58), pp. 30–37. DOI: 10.18577/2071-9140-2020-0-1-30-37.
  3. Peskova A.V., Sukhov D.I., Mazalov P.B. Exami-nation of the formation of the titanium alloy VT6 structure obtained by additive manufacturing. Aviacionnye materialy i tehnologii, 2020, no. 1 (58), pp. 38–44. DOI: 10.18577/2071-9140-2020-0-1-38-44.
  4. Alexandrov D.A., Gorlov D.S., Budinovskii S.A. Application of a complex of ion-plasma technologies to protect the compressor blades of a helicopter gas-turbine engine from erosion wear and fretting. Trudy VIAM, 2021, no. 2 (96), paper no. 08. Available at: http://www.viam-works.ru (accessed: August 08, 2022). DOI: 10.18577/2307-6046-2021-0-2-71-80.
  5. Kablov E.N., Muboyadzhyan S.A. Erosion-resistant coatings for gas turbine engine compressor blades. Russian metallurgy (Metally), 2017, vol. 2017, no. 6, pp. 494–504.
  6. Muboyadzhyan S.A. Erosion-resistant coatings for GTE compressor blades. Metally, 2009, no. 3, pp. 3–20.
  7. Yakusheva N.A. High-strength constructional steels for landing gears of perspective products of aircraft equipment. Aviacionnye materialy i tehnologii, 2020, no. 2 (59), pp. 3–9. DOI: 10.18577/2071-9140-2020-0-2-3-9.
  8. Gromov V.I., Yakusheva N.A., Vostrikov A.V., Cherkashneva N.N. High strength structural steels for gas-turbine engine shafts (review). Aviation materials and technology, 2021. no. 1 (62). paper no. 01. Available at: http://www.journal.viam.ru (accessed: August 08, 2022). DOI: 10.18577/2713-0193-2021-0-1-3-12.
  9. Grzesik W., Malecka J., Kwasny W. Identification of oxidation process of TiAlN coatings versus heat resistant aerospace alloys based on diffusion couples and tool wear tests. CIRP Annals – Manufacturing Technology, 2020, no. 69, pp. 41–44. DOI: 10.1016/j.cirp.2020.04.024.
  10. Zhang M., Cheng Y., Xin L. et al. Cyclic oxidation behaviour of Ti/TiAlN composite multilayer coatings deposited on titanium alloy. Corrosion Science, 2020, no. 166, pp. 108476–108486. DOI: 10.1016/j.corsci.2020.108476.
  11. Vereschaka A.A., Grigoriev S.N. Study of cracking mechanisms in multi-layered composite nano-structured coatings. Wear, 2017, no. 378–379, pp. 43–57. DOI: 10.1016/j.wear.2017.01.101.
  12. Xu Y.X., Riedl H., Holec D. et al. Thermal stability and oxidation resistance of sputtered Ti–Al–Cr–N hard coatings. Surface & Coatings Technology, 2017, no. 324, pp. 48–56. DOI: 10.1016/j.surfcoat.2017.05.053.
  13. Asanuma H., Polcik P., Kolozsvari S. et al. Cerium doping of Ti–Al–N coatings for excellent thermal stability and oxidation resistance. Surface & Coatings Technology, 2017, no. 326, pp. 165–172. DOI: 10.1016/j.surfcoat.2017.07.037.
  14. Sui X., Li G., Zhou H. et al. Evolution behavior of oxide scales of TiAlCrN coatings at high temperature. Surface & Coatings Technology, 2019, no. 360, pp. 133–139. DOI: 10.1016/j.surfcoat.2019.01.016.
  15. Tillmann W., Grisales D., Stangier D. et al. Residual stresses and tribomechanical behaviour of TiAlN and TiAlCN monolayer and multilayer coatings by DCMS and HiPIMS. Surface & Coatings Technology, 2021, no. 406, pp. 126664–126675. DOI: 10.1016/j.surfcoat.2020.126664.
  16. Pilemalm R., Sjögren A. High pressure and high temperature behaviour of TiAlN coatings deposited on c-BN based substrates. Processing and Application of Ceramics, 2020 no. 14, vol. 3, pp. 210–217. DOI: 10.2298/PAC2003210P.
  17. Özkan D., Erarslan Y., Sulukan E. et al. Tribological behavior of TiAlN, AlTiN, and AlCrN coatings at boundary lubricating condition. Tribology Letters, 2018, no. 66, pp. 152–167. DOI: 10.1007/s11249-018-1111-1.
  18. Lin J., Zhang X., Ge F. et al. Thick CrN/AlN superlattice coatings deposited by hot filament assisted HiPIMS for solid particle erosion and high temperature wear resistance. Surface & Coatings Technology, 2019, no. 377, pp. 124922–124933. DOI: 10.1016/j.surfcoat.2019.124922.