Dvoretskov R.M., Karachevtsev F.N., Petrov P.S. Comparisons of the nickel alloys VZh172 and VZhL21 reference materials using the X-ray fluorescence analysis method // Proceedings of VIAM. 2022. No. 11 (117). Ст. 11. URL: https://www.viam-works.ru. DOI: 10.18577/2307-6046-2022-0-11-119-133.

Comparisons of the nickel alloys VZh172 and VZhL21 reference materials using the X-ray fluorescence analysis method

Dvoretskov R.M., Karachevtsev F.N., Petrov P.S.
Abstract

This work is devoted to the issues of comparison of domestic and foreign standard samples (certified reference materials) of nickel alloys of various grades. Using the method of x-ray fluorescence spectrometry on sets of State standard samples of alloys VZh172 and VZhL21 containing elements such as Al, Co, Cr, Mo, Ti, W, Zr, Fe, Mn, calibration dependences of the mass fraction of elements on the intensity of the signal – the characteristicx-ray radiation. Using statistical techniques, an assessment was made of the possibility of joint use of sets in the construction of general calibration characteristics for the simultaneous determination of Al, Co, Cr, Mo, Nb, Ta, Ti, W, Zr, Fe, Mn in nickel alloys of similar composition.

Keywords
heat-resistant nickel alloys, x-ray fluorescence spectrometry, x-ray fluorescence analysis, comparison certified reference materials, calibration, chemical analysis
Reference list
  1. Otto M. Modern methods of analytical chemistry: in 2 vols. M.: Technosphere, 2003, vol. I, 416 p.
  2. Karpov Yu.A., Baranovskaya V.B. Analytical control – an integral part of the diagnosis of materials. Zavodskaya laboratoriya. Diagnostika materialov, 2017, vol. 83, no. 1, pp. 5–12.
  3. Karpov Yu.A., Baranovskaya V.B. Problems of standardization of chemical analysis methods in metallurgy. Zavodskaya laboratoriya. Diagnostika materialov, 2019, vol. 85, no. 1-2, pp. 5–14.
  4. Kablov E.N. Quality control of materials – a guarantee of the safety of the operation of aviation equipment. Aviacionnnye materialy i tehnologii, 2001, no. 1, pp. 3–8.
  5. Karpov Yu.A., Baranovskaya V.B. The role and possibilities of analytical control in metallurgy. Tsvetnye metally, 2016, no. 8 (884), pp. 63–67. DOI: 10.17580/TSM 2016.08.09.
  6. Chernikova I.I., Kostrikina T.V., Tyumneva K.V., Ermolaeva T.N. The use of standard samples of domain, steelmaker, converter slag and welding flows in the development of a methodology for analyzing slag-forming mixtures using the atomic-emission spectrometry with inductively connected plasma. Standartnyye obraztsy, 2017, no. 3–4, pp. 29–40. DOI: 10.20915/2077-1177-2017-13-3-4-29-40.
  7. Kablov E.N., Cabina E.B., Morozov G.A., Muravskaya N.P. Assessment of compliance of new materials using high -level CO and MI. Kompetentnost, 2017, no. 2 (143), pp. 40–46.
  8. Lomberg B.S., Ovsepjan S.V., Bakradze M.M., Letnikov M.N., Mazalov I.S. The application of new wrought nickel alloys for advanced gas turbine engines. Aviacionnye materialy i tehnologii, 2017, no. S, pp. 116–129. DOI: 10.18577/2071-9140-2017-0-S-116-129.
  9. Kablov E.N., Sidorov V.V., Kablov D.E., Min P.G. The metallurgical fundamentals for high quality maintenance of single crystal heat-resistant nickel alloys. Aviacionnye materialy i tehnologii, 2017, no. S, pp. 55–71. DOI: 10.18577/2071-9140-2017-0-S-55-71.
  10. Muravskaya N.P., Ivanov A.V., Ermakova Y.I., Zyablikova I.N. The testing methodology for standard samples using the state primary standard GET 196–2011. II Int. Sc. Conf. “Standard samples in measurements and technologies”: a collection of works. Ekaterinburg: Ural Scientific-Iser. Institute of Metrology, 2015, pp. 46.
  11. Lutsenko A.N., Letov A.F., Karachevtsev F.N. Problematic issues of the development of standard samples of composition and the properties of aviation materials. Standartnye obraztsy, 2016, no. 4, pp. 31–41.
  12. Eroshkin S.G., Orlov G.V. Research of material inhomogeneity of reference samples made of wrought Ni-based superalloy VZH175-ID. Trudy VIAM, 2015, no. 8, paper no. 11. Available at: http://viam-works.ru (accessed: June 15, 2022). DOI: 10.18577/2307-6046-2015-0-8-11-11.
  13. The Federal Information Fund for Ensuring the Uniformity of Measurements. Available at: http://fundmetrology.ru (accessed: June 22, 2022).
  14. Orlov G.V., Titov V.I. X-ray-fluorescent and optical-emission methods of analysis of aviation alloys. Metallurgiya mashinostroeniya, 2018, no. 3, pp. 31–33.
  15. Afonin V.P., Komyak N.I., Nikolaev V.P., Plotnikov R.I. X-ray-fluorescence analysis. Novosibirsk: Nauka, 1991, 173 p.
  16. Stepanovsky V.V. Standard cast iron samples and steel for spectral analysis developed by the Institute of Standard Samples CJSC. Zavodskaya laboratoriya. Diagnostika materialov, 2017, vol. 83, no. 1, part II, pp. 70–77.
  17. Saprygin A.V., Golik V.M., Makarov A.A., Dzhavaev B.G., Kudryavtsev V.N. Closure of standard samples of the isotopic composition of uranium production NBL (USA) and UECC. Standartnye obraztsy, 2007, no. 2, pp. 39–48.
  18. Nalobin D.P., Osintseva E.V. Methods of comparing standard samples of the composition of substances and materials. Standartnye obraztsy, 2006, no. 1 (3), pp. 36–44.
  19. Stepanovsky V.V., Guzeev L.I. Mixing of domestic and foreign standard samples on the SA-2000. Analitika i kontrol, 2000, vol. 4, no. 3, pp. 293–297.
  20. Maryina G.E. Analytical control of ferroalloys by radiofluorescent spectrometry: thesis, Cand. Sc. (Tech.). Moscow, 2012, pp. 33–40.
  21. Dudik S.L., Kalinin B.D., Rudnev A.V., Sergeev Yu.I. Analysis of steels and alloys on x-ray spectrometers of the Spectroscan Max series. Zavodskaya laboratoriya. Diagnostika materialov, 2014, vol. 80, no. 1, pp. 19–26.
  22. Kalinin B.D., Plotnikov R.I. X-ray-fluorescent determination of alloying and impurity elements in homogeneous materials in the absence of adequate calibration samples. Analitika i kontrol, 2010, vol. 14, no. 4, pp. 236–242.
  23. RMG 56–2002 GSI. Sets of standard samples of the composition of substances and materials. Methods of mutual comparison. Moscow: Publishing House of Standards, 2004, 10 p.
  24. MI 3257–2009 GSI. Standard materials (substances). Methods of mutual comparison. Ekaterinburg: UNIIM, 2009, 36 p.
  25. Dvoretskov R.M., Slavin А.V., Karachevtsev F.N., Zagvozdkina Т.N. Comparisons of the nickel alloys VZh172 and VZhL21 reference materials kits using the AES ICP method. Trudy VIAM, 2021, no. 11 (105), paper no. 12. Available at: http://www.viam-works.ru (accessed: June 22, 2022). DOI: 10.18577/2307-6046-2021-0-11-120-132.
  26. Kablov E.N. Innovative developments of FSUE «VIAM» SSC of RF on realization of «Strategic directions of the development of materials and technologies of their processing for the period until 2030». Aviacionnye materialy i tehnologii, 2015, no. 1 (34), pp. 3–33. DOI: 10.18577/2071-9140-2015-0-1-3-33.
  27. Kablov E.N. Aviation materials science in the 21st century. Prospects and tasks. Aviation materials. Selected works of VIAM 1932–2002. Moscow: MISIS–VIAM, 2002, pp. 23–47.
  28. Kablov E.N. Trends and guidelines of innovative development of Russia: collections scientific-inform. materials. 3rd ed. Moscow: VIAM, 2015, 720 p.
  29. Letov A.F., Karachevtsev F.N., Zagvozdkina T.N. Development the set of methods measurements of the chemical composition of nickel-based alloys. Trudy VIAM, 2018, no. 8 (68), paper no. 09. Available at: http://www.viam-works.ru (accessed: June 15, 2022). DOI: 10.18577/2307-6046-2018-0-8-89-97.
  30. Osintseva E.V. Separation of standard samples: experiment planning and processing measurement results. Standartnye obraztsy, 2016, no. 4, pp. 3–14. DOI: 10.20915/2077-1177-2016-0-4-3-14.
  31. Derffel K. Statistics in analytical chemistry. Moscow: Mir, 1994, 268 p.
  32. Garmash A.V., Sorokina N.M. Metrological foundations of analytical chemistry. Moscow: Lomonosov Moscow State University, 2012, 47 p.